Influence of cooling rate during the heat treatment process on the precipitates and ductility behavior of inconel 718 superalloy fabricated by selective laser melting

被引:6
|
作者
Yang, Peixin [1 ,2 ]
Su, Haijun [1 ,2 ]
Guo, Yinuo [1 ,2 ]
Zhou, Haotian [2 ]
Xia, Le [2 ]
Shen, Zhonglin [2 ]
Wang, Meng [2 ]
Zhang, Zhuo [2 ]
Guo, Min [2 ]
机构
[1] Northwestern Polytech Univ Shenzhen, Res & Dev Inst, Shenzhen 518057, Peoples R China
[2] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
基金
中国国家自然科学基金;
关键词
IN718; superalloy; Selective laser melting (SLM); Heat treatment (HT); Cooling rates; Microstructure; Ductility behavior; DELTA-PHASE PRECIPITATION; MECHANICAL-PROPERTIES; SCANNING STRATEGY; MICROSTRUCTURE;
D O I
10.1016/j.msea.2024.146603
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
IN718 superalloy by elective laser melting (SLM) has shown great application prospects in the aerospace engine key parts. Different phases are precipitated during the SLM forming process. Although the Laves phase could be dissolved in dendrites by heat treatment, the specific evolution of the second phase particles is still unclear. In this work, the influences of solution and aging heat treatment, as well as cooling rate on the precipitates and ductility behavior of IN718 superalloy fabricated by SLM were systematically investigated. The medium temperature (980 degrees C) solution treatment regimes included three different colling rates and the control group only underwent aging treatment were studied. The results indicated that high temperature solid solution treatment effectively improved compositional segregation and significantly enhanced homogeneity of microstructure. The reduce of cooling rate at 980 degrees C was beneficial to the extension time and increased the number of delta phase precipitation. An appropriate number of delta phase improves the notch sensitivity and nails grain boundaries. In addition, the complex dislocations and second phase particles retards the migration of slip dislocations during ductility deformation process, which enhances the strength of SLM-ed IN718. The yield strength of specimens increases from 680 MPa to 1205 MPa. The microhardness is greatly improved as compared with as-deposited IN718, and the highest microhardness reaches 485 HV. The results provide a technical support and reference for formulating the heat treatment schedule of IN718 prepared by SLM.
引用
收藏
页数:15
相关论文
共 50 条
  • [41] Stress relaxation of inconel 718 superalloy manufactured by selective laser melting (SLM)
    Alikarami, Sh
    Nakhodchi, S.
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2025, 214
  • [42] Microstructural evolution and phase transformation of Inconel 718 alloys fabricated by selective laser melting under different heat treatment
    Liu, Peng
    Hu, Jiaying
    Sun, Siyu
    Feng, Keyun
    Zhang, Yuanbin
    Cao, Meiqing
    JOURNAL OF MANUFACTURING PROCESSES, 2019, 39 : 226 - 232
  • [43] Effects of Solution Treatment on Microstructure and Hardness of Inconel 718 Alloy Fabricated by Selective Laser Melting
    Guo, Yuhao
    Zhao, Xueping
    Bai, Pucun
    Cao, Yu
    Hou, Xiaohu
    Liu, Fei
    Zhongguo Biaomian Gongcheng/China Surface Engineering, 2021, 34 (02): : 114 - 121
  • [44] Effects of Solution Treatment on Microstructure and Hardness of Inconel 718 Alloy Fabricated by Selective Laser Melting
    Guo Yuhao
    Zhao Xueping
    Bai Pucun
    Cao Yu
    Hou Xiaohu
    Liu Fei
    CHINA SURFACE ENGINEERING, 2021, 34 (02) : 114 - 121
  • [45] Heat treatment of Inconel 718 produced by selective laser melting: Microstructure and mechanical properties
    Huang, Wenpu
    Yang, Jingjing
    Yang, Huihui
    Jing, Guanyi
    Wang, Zemin
    Zeng, Xiaoyan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 750 : 98 - 107
  • [46] Deformation behavior of selective laser-melted Inconel 718 superalloy
    Zhang, Shuya
    Guo, Chunwen
    Lin, Xin
    Zhao, Hongliang
    Yang, Haiou
    Huang, Weidong
    MATERIALS CHARACTERIZATION, 2024, 216
  • [47] Friction and wear behaviour of Inconel 718 alloy fabricated by selective laser melting after heat treatments
    Zhao, Zhanyong
    Qu, Hongqiao
    Bai, Peikang
    Li, Jing
    Wu, Liyun
    Huo, Pengcheng
    PHILOSOPHICAL MAGAZINE LETTERS, 2018, 98 (12) : 547 - 555
  • [48] Temperature and strain-rate dependence of the elevated temperature ductility of Inconel 718 prepared by selective laser melting
    McLouth, Tait D.
    Witkin, David B.
    Lohser, Julian R.
    Sitzman, Scott D.
    Adams, Paul M.
    Lingley, Zachary R.
    Bean, Glenn E.
    Yang, Jenn-Ming
    Zaldivar, Rafael J.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 824
  • [49] Micro-porosity and Tensile Property of High Relative Density Inconel 718 Superalloy Fabricated by Selective Laser Melting
    Liu, Fencheng
    Hu, Wenwei
    Jia, Jiongyu
    Liu, Fenggang
    Xu, Yang
    Wang, Zhitai
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2021, 50 (10): : 3684 - 3692
  • [50] Micro-porosity and Tensile Property of High Relative Density Inconel 718 Superalloy Fabricated by Selective Laser Melting
    Liu Fencheng
    Hu Wenwei
    Jia Jiongyu
    Liu Fenggang
    Xu Yang
    Wang Zhitai
    RARE METAL MATERIALS AND ENGINEERING, 2021, 50 (10) : 3684 - 3692