An Investigation into the Microstructures and Mechanical Properties of a TIG Welding Joint in Ti-4Al-2V Titanium Alloy

被引:1
|
作者
Chen, Yao [1 ]
Liu, Xiao [1 ]
Zhang, Zhendi [1 ]
Wang, Kaiqing [1 ]
Zhang, Shanglin [1 ]
Qian, Bingnan [1 ,2 ,3 ]
Wu, Jun [1 ]
Wang, Li [1 ]
机构
[1] Nucl Power Inst China, Natl Key Lab Nucl Reactor Technol, Chengdu 610041, Peoples R China
[2] Southern Univ Sci & Technol, Shenzhen Key Lab Intelligent Robot & Flexible Mfg, Shenzhen 518055, Peoples R China
[3] Southern Univ Sci & Technol, Dept Mech & Energy Engn, Shenzhen 518055, Peoples R China
关键词
Ti-4Al-2V titanium alloy; TIG welding; microstructure; nanoindentation; mechanical properties of microzones; TI-6AL-4V; EVOLUTION; BEHAVIOR; HARDNESS; ZONES;
D O I
10.3390/met14050596
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The Ti-4Al-2V (wt. %) titanium alloy has garnered widespread applications across diverse fields due to its exceptional strength-to-weight ratio, high toughness, specific strength, and corrosion resistance. The welding of Ti-4Al-2V titanium alloy components is often necessary in manufacturing processes, where the reliability of a welded joint critically influences the overall service life of these components. Consequently, a comprehensive understanding of the welded joint's microstructure and mechanical properties is imperative. In this study, Ti-4Al-2V titanium alloy was welded using multi-layer and multi-pass TIG welding techniques, and a detailed examination was conducted to analyze the microstructure and grain morphology of each microzone of the welded joint. The results revealed the presence of an initial alpha phase and a secondary lamellar alpha phase in the heat affected zone (HAZ). Meanwhile, the fusion zone (FZ) primarily comprised a coarse secondary alpha phase and a small amount of an acicular martensitic alpha' phase. Both the recrystallization zone and the superheated zone exhibited a distinct preferred orientation, with grains smaller than 10 mu m accounting for 65.9% and 55.1%, respectively. To assess the mechanical properties of the various microzones and the typical microstructure within the welded joint, nanoindentation tests were performed. The results indicated that the recrystallization zone possessed a higher nanohardness (3.753 GPa) than the incomplete recrystallization zone (3.563 GPa) and the superheated zone (3.48 GPa). Among all the microzones, the FZ exhibited the lowest average nanohardness (3.058 GPa). Notably, the basket-weave microstructure demonstrated the highest average nanohardness, reaching 3.93 GPa. This was followed by the fine-grain microstructure, which possessed a slightly lower nanohardness. The Widmanst & auml;tten microstructure, on the other hand, exhibited the lowest nanohardness among the three microstructures within the HAZ. Therefore, the basket-weave microstructure stands out as the most desirable microstructure to achieve in the welded joint. In summary, this study provides a comprehensive characterization and analysis of the microstructure and properties of Ti-4Al-2V titanium alloy TIG welds, aiming to contribute to the optimization of the TIG welding process for Ti-4Al-2V titanium alloy.
引用
收藏
页数:12
相关论文
共 50 条
  • [21] Lattice parameters of Ti-4Al-2V alloy with thermal oxidation
    Omidbakhsh, Faraz
    Ebrahimi, Ali Reza
    RARE METALS, 2016, 35 (02) : 149 - 153
  • [22] Investigation on mechanical properties of laser welded joints for Ti-6Al-4V titanium alloy
    Zhao, X.
    Zhang, J.
    Song, X.
    Guo, W.
    MATERIALS SCIENCE AND TECHNOLOGY, 2013, 29 (12) : 1405 - 1413
  • [23] Correlation between welding parameters and microstructures in TIG, plasma and laser welded Ti-6Al-4V alloy
    Sun, Z
    Pan, D
    Zhang, W
    TRENDS IN WELDING RESEARCH, PROCEEDINGS, 2003, : 760 - 767
  • [24] Structure and Properties of a Permanent Joint of Ti-6Al-4V Titanium Alloy Formed by Friction Stir Welding
    Chumaevskii, A., V
    Amirov, A., I
    Moskvichev, E. N.
    Ivanov, A. N.
    Kolubaev, E. A.
    RUSSIAN PHYSICS JOURNAL, 2022, 65 (05) : 765 - 770
  • [25] Structure and Properties of a Permanent Joint of Ti-6Al-4V Titanium Alloy Formed by Friction Stir Welding
    A. V. Chumaevskii
    A. I. Amirov
    E. N. Moskvichev
    A. N. Ivanov
    E. A. Kolubaev
    Russian Physics Journal, 2022, 65 : 765 - 770
  • [26] Microstructures and Mechanical Properties of Friction Welded Ti-6Al-4V Alloy
    Kim, Gyeong-Woo
    Song, Kuk-Hyun
    Jeong, Se-Min
    MATERIALS TRANSACTIONS, 2022, 63 (10) : 1323 - 1331
  • [27] Study on Microstructure and Mechanical Properties of Ti6Al4V Titanium Alloy Joint with Ultrasonic Consolidation
    Zhu, Zhengqiang
    Li, Mingfeng
    Su, Zhanzhan
    Zhang, Deqin
    Zhang, Yifu
    TRANSACTIONS ON INTELLIGENT WELDING MANUFACTURING, VOL I, NO. 1 2017, 2018, 1 (01): : 120 - 129
  • [28] Microstructure and mechanical properties of thick titanium alloy joint in narrow-gap TIG welding
    Lü, Shixiong
    Cui, Qinglong
    Huang, Yongxian
    Zheng, Chuanqi
    Wang, Yang
    Hanjie Xuebao/Transactions of the China Welding Institution, 2012, 33 (08): : 81 - 84
  • [29] INVESTIGATION AND OPTIMIZATION OF LASER WELDING OF TI-6AL-4V TITANIUM ALLOY PLATES
    Caiazzo, Fabrizia
    Alfieri, Vittorio
    Corrado, Gaetano
    Cardaropoli, Francesco
    Sergi, Vincenzo
    PROCEEDINGS OF THE ASME 8TH INTERNATIONAL MANUFACTURING SCIENCE AND ENGINEERING CONFERENCE - 2013, VOL 1, 2013,
  • [30] Investigation and Optimization of Laser Welding of Ti-6Al-4 V Titanium Alloy Plates
    Caiazzo, Fabrizia
    Alfieri, Vittorio
    Corrado, Gaetano
    Cardaropoli, Francesco
    Sergi, Vincenzo
    JOURNAL OF MANUFACTURING SCIENCE AND ENGINEERING-TRANSACTIONS OF THE ASME, 2013, 135 (06):