Effect of Hf addition on structural transformation and aging stability of Cu-15Ni-8Sn alloy

被引:1
|
作者
Zhang, Junjia [1 ]
Zheng, Jisen [1 ]
Chen, Xin [1 ]
Liao, Qiyu [1 ]
Wang, Ze [1 ]
Yin, Bingbing [1 ]
Dong, Yong [2 ]
Zou, Cunlei [3 ]
Fu, Ying [4 ]
机构
[1] Northeastern Univ, Sch Mat Sci & Engn, Key Lab Lightweight Struct Mat Liaoning Prov, Shenyang 110819, Peoples R China
[2] Guangdong Univ Technol, Sch Mat & Energy, Guangzhou 510006, Peoples R China
[3] Dalian Jiaotong Univ, Sch Mat Sci & Engn, Dalian 116028, Peoples R China
[4] Songshan Lake Mat Lab, Dongguan 523808, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2024年 / 899卷
基金
中国国家自然科学基金;
关键词
Cu-15Ni-8Sn alloy; Microstructural evolution; Aging stability; Softening resistance; DISCONTINUOUS PRECIPITATION; CELLULAR PRECIPITATION; MECHANICAL-PROPERTIES; MICROSTRUCTURES; ELEMENTS; DEPENDENCE; BEHAVIOR; KINETICS; GROWTH; CERIUM;
D O I
10.1016/j.msea.2024.146434
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The Cu-15Ni-8Sn-xHf (wt.%, x = 0-0.6) alloys were prepared by vacuum melting, and the effect of Hf on the micro -structure of as -cast, as -solution -treated and as -aged alloys was systematically investigated, as well as the alloy aging stability. The Hf addition provided a significant role on refining the solidification structure and reducing the micro -segregation degree, and it also made gamma- D0 3 phases more likely to form in needlelike-shape rather than lamellar -shape. With the presence of more Hf atoms, their existence form was accordingly changed from solid solute atoms to nano -scale precipitation phases and then to micron -scale segregation phase. A small content of Hf (0.1 wt%) could effectively improve the aging stability by inhibiting the growth of gamma- D0 3 . Once its content reached or exceeded 0.3 wt%, the harmful discontinuous precipitation was completely inhibited, and the common lamellar -shape gamma- D0 3 locating around the grain boundary was no longer formed. Even the alloy failed at higher temperatures, it could only be carried out through the continuous precipitation method, namely the generation of needlelike-shape gamma- D0 3 uniformly in the matrix. The appropriate Hf addition was capable of extending the alloy aging window, and the hardness of Cu-15Ni-8Sn-0.3Hf alloy could still exceed 360 HV even after 48 h aging.
引用
收藏
页数:13
相关论文
共 50 条
  • [21] Microstructures of spinodal phases in Cu-15Ni-8Sn alloy
    Wang, YH
    Wang, MP
    Hong, B
    JOURNAL OF UNIVERSITY OF SCIENCE AND TECHNOLOGY BEIJING, 2005, 12 (03): : 243 - 247
  • [22] Re-aging behavior of Cu-15Ni-8Sn alloy pretreated by dynamic strain aging
    Peng, Guangwei
    Gan, Xueping
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 752 : 18 - 23
  • [23] Inhibition of discontinuous precipitation and enhanced properties of Cu-15Ni-8Sn alloy with Fe addition
    Guo, Chengjun
    Wan, Jia
    Chen, Jinshui
    Xiao, Xiangpeng
    Huang, Hao
    Liu, Jinping
    Yang, Bin
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 795
  • [24] Effects of P addition on spinodal decomposition and discontinuous precipitation in Cu-15Ni-8Sn alloy
    Guo, Chengjun
    Shi, Yufan
    Chen, Jinshui
    Xiao, Xiangpeng
    Liu, Baixiong
    Liu, Jinpin
    Yang, Bin
    MATERIALS CHARACTERIZATION, 2021, 171
  • [25] Effect mechanism of Nb addition on grain refinement and inhibition of discontinuous precipitation of Cu-15Ni-8Sn alloy
    Yang, Wenhao
    Zhou, Yanjun
    Yang, Ran
    Yang, Shaodan
    Zhou, Fei
    Song, Kexing
    Feng, Jiang
    Jiang, Hao
    Zhang, Xuebin
    Du, Juan
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 32 : 3966 - 3979
  • [26] High strength and excellent softening resistance Cu-15Ni-8Sn alloy by Ti addition
    Chen, Liangguo
    Liang, Yuanxin
    Luo, Boyi
    Ding, Biao
    Shen, Zhe
    Zhang, Shunran
    Lu, Haibiao
    Zheng, Tianxiang
    Li, Qiang
    Zhou, Bangfei
    Liu, Chunmei
    Ren, Weili
    Zhong, Yunbo
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 30 : 4552 - 4563
  • [27] Comparison of discontinuous precipitation behavior of Cu-15Ni-8Sn alloy with and without Co addition
    Guo, Chengjun
    Qi, Zhaoming
    Xu, Huaben
    Shi, Yufan
    Xiao, Xiangpeng
    An, Guihuan
    Yang, Bin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 930
  • [28] Solidification Characteristics and Segregation Behavior of Cu-15Ni-8Sn Alloy
    Guo, Zhongkai
    Jie, Jinchuan
    Liu, Shichao
    Liu, Jiaming
    Yue, Shipeng
    Zhang, Yubo
    Li, Tingju
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2020, 51 (03): : 1229 - 1241
  • [29] Solidification Characteristics and Segregation Behavior of Cu-15Ni-8Sn Alloy
    Zhongkai Guo
    Jinchuan Jie
    Shichao Liu
    Jiaming Liu
    Shipeng Yue
    Yubo Zhang
    Tingju Li
    Metallurgical and Materials Transactions A, 2020, 51 : 1229 - 1241
  • [30] Effect of defect strengthening on the mechanical properties of a novel Cu-15Ni-8Sn alloy
    Zhang, Junjia
    Wang, Ze
    Miao, Shuran
    Zhang, Yajing
    Fu, Ying
    Dong, Yong
    Liu, Shichao
    Jie, Jinchuan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 868