The anti-oxidation behavior of the Ti3SiC2/Cu composites at high temperatures

被引:0
|
作者
Zhang, Rui [1 ,2 ]
Zhang, Huiming [1 ]
Liu, Fuyan [3 ]
Ma, Shuai [4 ]
机构
[1] Chengdu Univ, Sch Mech Engn, Chengdu 610106, Peoples R China
[2] Chinese Acad Sci, Lanzhou Inst Chem Phys, State Key Lab Solid Lubricat, Lanzhou, Peoples R China
[3] Changzhou Inst Technol, Sch Chem Engn & Mat, Changzhou 213032, Peoples R China
[4] Xinjiang Univ, Sch Mech Engn, Urumqi, Peoples R China
关键词
oxidation resistance; SPS; Ti3SiC2/Cu composites; OXIDATION BEHAVIOR; RESISTANCE;
D O I
10.1111/ijac.14869
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The Ti3SiC2/Cu composites were synthesized by spark plasma sintering (SPS) at 950 degrees C, 1000 degrees C, and 1050 degrees C, and the as-formed composites were oxidized at 700 degrees C, 800 degrees C, and 900 degrees C. The effects of the sintering temperature and the oxidation temperature on the anti-oxidation of the composites at high temperatures were explored. The samples were characterized by X-ray diffraction, optical microscopy, scanning electron microscopy, energy dispersive spectroscopy, and X-ray photoelectron spectroscope. The results indicated that the sintering temperature significantly improved the oxidation resistance of the composites. With the increase of the sintering temperature, the weight gain of the oxidation of the composites decreased and the optimum sintering temperature was 1050 degrees C. At an identical sintering temperature, with the increase of the oxidation temperature, the weight gain of the oxidation of the composites first decreased and then it increased. Thus, when the oxidation temperature was 800 degrees C, the composites exhibited an excellent oxidation resistance (oxidation weight gain: .0042 x 10(-5) g/mm(2)). The anti-oxidation behavior of the composites benefited by the formation of an oxide layer. The oxide layer was composed by TiO2, CuO, and amorphous SiO2.
引用
收藏
页数:9
相关论文
共 50 条
  • [41] Ti3SiC2/TiC composites prepared by PDS
    S. Konoplyuk
    T. Abe
    T. Uchimoto
    T. Takagi
    Journal of Materials Science, 2005, 40 : 3409 - 3413
  • [42] Microstructural and mechanical properties of Ti3SiC2 composites
    Huang, Jow-Lay
    Lu, Horng-Hwa
    Key Engineering Materials, 2009, 403 : 189 - 192
  • [43] Ti3SiC2/TiC composites prepared by PDS
    Konoplyuk, S
    Abe, T
    Uchimoto, T
    Takagi, T
    JOURNAL OF MATERIALS SCIENCE, 2005, 40 (13) : 3409 - 3413
  • [44] Fabrication and properties of Al/Ti3SiC2 composites
    Ai, MX
    Zhai, HX
    Zhou, Y
    Huang, ZY
    Zhang, ZL
    Guan, ML
    Li, SB
    RARE METAL MATERIALS AND ENGINEERING, 2005, 34 : 397 - 400
  • [45] Wettability of Ti3SiC2 by Ag–Cu and Ag–Cu–Ti melts
    O. Dezellus
    R. Voytovych
    A. P. H. Li
    G. Constantin
    F. Bosselet
    J. C. Viala
    Journal of Materials Science, 2010, 45 : 2080 - 2084
  • [46] Preparation and properties of TaC/Ti3SiC2 composites
    Yin, Hongfeng, 1600, Beijing University of Aeronautics and Astronautics (BUAA) (31):
  • [47] Ti3SiC2 as a bonding phase in diamond composites
    Jaworska, L
    Szutkowska, M
    Morgiel, J
    Stobierski, L
    Lis, J
    JOURNAL OF MATERIALS SCIENCE LETTERS, 2001, 20 (19) : 1783 - 1786
  • [48] Microstructural and Mechanical Properties of Ti3SiC2 Composites
    Huang, Jow-Lay
    Lu, Horng-Hwa
    SIAIONS AND NON-OXIDES, 2009, 403 : 189 - +
  • [49] Microstructure and Oxidation of (La,Sr)CrO3-Added Ti3SiC2 Composites
    Lee, Dong Bok
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2015, 15 (11) : 8381 - 8387
  • [50] Contribution of plastic deformation of Ti3SiC2 to the crack deflection in the Al2O3/Ti3SiC2 composites
    Chin, Yuan-Liang
    Tuan, Wei-Hsing
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (7-8): : 3270 - 3274