Impacts of frost heave susceptibility and temperature-changing conditions on freeze-thaw deterioration of welded tuffs

被引:0
|
作者
Gang, Mingwei [1 ]
Nonaka, Satoshi [2 ]
Utashiro, Keisuke [3 ]
Kodama, Jun-ichi [1 ]
Nakamura, Dai [4 ]
Fujii, Yoshiaki [1 ]
Fukuda, Daisuke [1 ]
Wang, Shuren [5 ]
机构
[1] Hokkaido Univ, Grad Sch Engn, Sapporo 0608628, Japan
[2] JFE Engn Co Ltd, Reconstruct Div, Tokyo 2308611, Japan
[3] Japan Racing Assoc, Tokyo Racecourse, Tokyo 1860024, Japan
[4] Kitami Inst Technol, Fac Engn, Kitami 0908507, Japan
[5] Henan Polytech Univ, Sch Civil Engn, Jiaozuo 454003, Peoples R China
关键词
Frost and non-frost heave rocks; Cooling-heating conditions; Freeze-thaw cycle; Damage model; Deterioration; Expansive strain; MECHANICAL-PROPERTIES; ROCK; CYCLES; STRENGTH; DEGRADATION; GRANITE; PERMEABILITY; PROPAGATION; DAMAGE; MODEL;
D O I
10.1016/j.coldregions.2024.104270
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Damage development in rocks by freeze-thaw cycles, a phenomenon that is typical to cold regions, is known to reduce the strength and durability of structures. In this study, a series of freeze-thaw tests were performed on frost and non-frost heave rocks to examine the impact of frost heave susceptibility and temperature-changing conditions on rock behaviors. The freeze-thaw life and uniaxial compressive strength (UCS) of rocks subjected to freeze-thaw cycles were estimated using a model that was based on fatigue damage mechanisms. Furthermore, we proposed a method for estimating the freeze-thaw life of rocks, using expansive strain as an important factor. The results indicated that the Shikotsu welded tuff (a non-frost heave rock) exhibited higher durability than the Noboribetsu welded tuff (a frost heave rock); this may be because the Shikotsu welded tuff had a larger pore radius and more unsaturated pores. The one-dimensional (1D) cooling-heating conditions induced significantly less damage than the three-dimensional (3D) conditions, owing to the continuous migration of free water into the unfrozen zone. The damage model estimated that for the Noboribetsu welded tuff, the freeze-thaw life in the 1D conditions was approximately eight times longer than that in the 3D conditions. Notably, with respect to the Shikotsu welded tuff, a critical freeze-thaw period induced significant expansion, resulting in damage development in the tuff. The freeze-thaw life of each rock sample was estimated based on the magnitude of the volumetric expansive strain. This study contributes to the rational assessment of the stability and durability of rock structures in cold regions.
引用
收藏
页数:11
相关论文
共 47 条
  • [31] Bank erosion under the impacts of fluvial erosion, frost heaving/ freeze-thaw process of rivers in seasonal frozen regions
    Yang, Jun
    Jia, Dongdong
    Zhai, Biyao
    Chen, Xiaona
    Wang, Jinyang
    HELIYON, 2024, 10 (17)
  • [32] The effect of meso-structure on temperature distribution in shale subject to freeze-thaw conditions
    Liu, H.
    Yang, G. S.
    BOUNDARIES OF ROCK MECHANICS: RECENT ADVANCES AND CHALLENGES FOR THE 21ST CENTURY, 2008, : 109 - 113
  • [33] The Compound Impacts of Changing Temperature and Snow Cover on Freeze and Thaw Patterns across Quebec
    Hatami, Shadi
    Nazemi, Ali
    GEO-EXTREME 2021: INFRASTRUCTURE RESILIENCE, BIG DATA, AND RISK, 2021, 330 : 368 - 376
  • [34] High-temperature and freeze-thaw aged biochar impacts on sulfonamide sorption and mobility in soil
    Tang, Wei
    Jing, Fanqi
    Laurent, Zanli Bi Lepohi Guy
    Liu, Yuyan
    Chen, Jiawei
    CHEMOSPHERE, 2021, 276
  • [35] Deterioration of volcanic tuffs from rock dwellings in Brhlovce (Slovakia) induced by freeze-thaw cycling studied by non-destructive tests and μCT visualization
    Mala, M.
    Greif, V.
    Ondrasik, M.
    BULLETIN OF ENGINEERING GEOLOGY AND THE ENVIRONMENT, 2024, 83 (05)
  • [36] Analysis on crack propagation of CRTS III slab ballastless track under temperature loads and freeze-thaw deterioration
    Chen, Wei
    Li, Siqi
    Wang, Weidong
    Pan, Zili
    Lou, Ping
    Li, Dongbai
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2024, 129
  • [37] Frost-Heaving Behavior and Enhancement Approaches of Cement-Based Grout Materials under Freeze-Thaw Conditions
    Wei, Yongfeng
    Dou, Hui
    Gao, Jiangtao
    Su, Run
    Ma, Shengjun
    COATINGS, 2023, 13 (11)
  • [38] Durability of FRP composite bridge deck materials under freeze-thaw and low temperature conditions
    Wu, Hwai-Chung
    Fu, Gongkang
    Gibson, Ronald F.
    Yan, An
    Warnemuende, Kraig
    Anumandla, Vijay
    JOURNAL OF BRIDGE ENGINEERING, 2006, 11 (04) : 443 - 451
  • [39] The freeze-thaw metallogenic model of regenerated gold placers under cold low temperature conditions
    ZHANG Baolin~1
    2. Changchun Institute of Geography
    Chinese Science Bulletin, 1999, (S2) : 11 - 13
  • [40] Microstructure deterioration of sandstone under freeze-thaw cycles using CT technology: The effects of different water immersion conditions
    Qiu, Bei
    Fan, Lifeng
    Du, Xiuli
    JOURNAL OF ROCK MECHANICS AND GEOTECHNICAL ENGINEERING, 2025, 17 (03) : 1599 - 1611