Hot corrosion behavior of selective laser melted TiC/GT D222 nickel-based composite in 75% Na2SO4 and 25% K2SO4 molten salt medium at 900°C

被引:0
|
作者
Lv, Yuting [1 ]
Ouyang, Xing [1 ]
Liu, Yaojie [1 ]
Tian, Ying [1 ]
Wang, Rui [2 ]
Wei, Guijiang [3 ,4 ]
机构
[1] Shandong Univ Sci & Technol, Coll Mech & Elect Engn, Qingdao, Peoples R China
[2] Shanghai Jiao Tong Univ, Shanghai, Peoples R China
[3] Youjiang Med Univ Nationalities, Affiliated Hosp, Guangxi, Peoples R China
[4] Youjiang Med Univ Nationalities, Ctr Med Lab Sci, Affiliated Hosp, Baise, Peoples R China
关键词
Hot corrosion; TiC/GTD222; composite; Selective laser melting (SLM); Mixed sulfates (Na2SO4 + K2SO4); NI-BASED SUPERALLOY; MECHANICAL-PROPERTIES; OXIDATION BEHAVIOR; DEGREES-C; MICROSTRUCTURE;
D O I
10.1108/ACMM-06-2024-3031
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Purpose This paper aims to investigate the differences in hot corrosion behavior of the GTD222 superalloy and TiC/GTD222 composite in a mixed salt of 75% Na2SO4 and 25% K2SO4 at 900 degrees C. Design/methodology/approach The GTD222 superalloy and TiC/GTD222 nickel-based composite were prepared using selective laser melting (SLM). Subsequently, the hot corrosion behavior of the two alloys was systematically investigated in a salt mixture consisting of 75% Na2SO4 and 25% K2SO4 (Wt.%) at 900 degrees C. Findings The TiC/GTD222 composite exhibited better hot corrosion resistance compared to the GTD222 superalloy. First, the addition of alloying elements led to the formation of a protective oxide film on the TiC/GTD222 composites 20 h before hot corrosion. Second, TiC/GTD222 composite corrosion surface has a higher Ti content, after 100 h of hot corrosion, the composite corrosion surface Ti content of 10.8% is more than two times the GTD222 alloy 4% Ti. The Ti and Cr oxides are tightly bonded, effectively resisting the erosion of corrosive elements. Originality/value The hot corrosion behavior of GTD222 superalloy and TiC/GTD222 composites prepared by SLM in a mixed salt of 75% Na2SO4 and 25% K2SO4 was studied for the first time. This study provides insights into the design of high-temperature alloys resistant to hot corrosion.
引用
收藏
页码:686 / 696
页数:11
相关论文
共 50 条
  • [21] Hot Corrosion of Co-based Alloys with 25%NaCl+75%Na2SO4 Coating at 1173 K
    Fu, Guangyan
    Guo, Xingxing
    Liu, Qun
    Zhao, Xin
    Su, Yong
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2013, 32 (03) : 317 - 321
  • [22] Hot Corrosion Behavior of Inconel 625 in Na2SO4 and V2O5 Molten Salt System
    Li, Liang
    Li, Lanfeng
    Zhang, Guofeng
    Xue, Hongdi
    Cui, Maomao
    Wang, Wenxu
    Liu, Dexue
    METALS, 2023, 13 (06)
  • [23] Effect of Co on oxidation and hot corrosion behavior of two nickel-based superalloys under Na2SO4-NaCl at 900 °C
    Meng, Jun-sheng
    Chen, Ming-xuan
    Shi, Xiao-ping
    Ma, Qiang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2021, 31 (08) : 2402 - 2414
  • [24] HOT CORROSION OF NICKEL IN NA2SO4-CASO4-PBO SALT MIXTURES AT 900-DEGREES-C
    SHATYNSKI, SR
    ARBAB, M
    JOURNAL OF METALS, 1980, 32 (12): : 5 - 5
  • [25] THE EFFECT OF K2SO4 ADDITIVE IN NA2SO4 DEPOSITS ON LOW-TEMPERATURE HOT CORROSION OF IRON ALUMINUM-ALLOYS
    SHI, LQ
    ZHANG, YS
    SHIH, ST
    OXIDATION OF METALS, 1992, 38 (5-6): : 385 - 405
  • [26] Hot corrosion behavior of ni-base alloys coated with salt film of 75%Na2SO4+25%NaCl at 900℃
    Shenyang University of Chemical Technology, Shenyang
    110142, China
    Xiyou Jinshu Cailiao Yu Gongcheng, 5 (1112-1115):
  • [27] NABO2(KBO2)-NA2SO4(K2SO4)-H2O SYSTEMS AT 25-DEGREES-C
    SKVORTSOV, VG
    AKIMOV, VM
    PETROVA, OV
    BELOVA, VF
    EZHOV, AI
    ZHURNAL NEORGANICHESKOI KHIMII, 1995, 40 (04): : 683 - 686
  • [28] Hot corrosion behaviors of a Cr13Ni5Si2-based metal silicide alloy in Na2SO4+25 wt.% K2SO4 and Na2SO4+25 wt.% NaCl molten salts
    Yuan, L.
    Wang, H. M.
    INTERMETALLICS, 2010, 18 (03) : 324 - 329
  • [29] Hot Corrosion of Cobalt-Based Alloy with (Na, K)2SO4 Coating At 900 °C
    Fu, Guangyan
    Zhao, Xin
    Liu, Qun
    Su, Yong
    ADVANCED ENGINEERING MATERIALS, PTS 1-3, 2011, 194-196 : 1305 - 1308
  • [30] Study of hot corrosion resistance of electroless nickel coating with different content of phosphorous in molten salt deposit Na2SO4–NaCl at 650°C
    Ghaderi M.
    Rezagholizadeh M.
    Nasiri-Vatan H.
    Ebrahimi-Kahrizsangi R.
    Surface Engineering and Applied Electrochemistry, 2015, 51 (04) : 367 - 373