Indentation Behavior Assessment of As-Built, Solution, and Artificial Aged Heat-Treated Selective Laser Melting Specimens of AlSi10Mg

被引:0
|
作者
Kamil, Abubakr Shahnawaz [1 ]
Muzamil, Muhammad [1 ]
Akhtar, Maaz [2 ]
Alsaleh, Naser [2 ]
Khan, Rashid [2 ]
Samiuddin, Muhammad [3 ]
Siddiqui, Ali Khursheed [2 ]
Yang, Junzhou [4 ]
Djuansjah, Joy [2 ]
机构
[1] NED Univ Engn & Technol, Dept Mech Engn, Karachi 75270, Pakistan
[2] Imam Mohammad Ibn Saud Islamic Univ, Coll Engn, Mech & Ind Engn Dept, Riyadh 11432, Saudi Arabia
[3] NED Univ Engn & Technol, Dept Met Engn, Karachi 75270, Pakistan
[4] Xian Univ Architecture & Technol, Sch Met Engn, Xian 710075, Peoples R China
关键词
SLM; AlSi10Mg; solution treatment; artificial aging; indentation; Finite Element Analysis; Rockwell Indentation; hardness; PARTS;
D O I
10.3390/cryst14070610
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
This study was conducted to determine the indentation behavior of thin AlSi10Mg specimens manufactured using Selective Laser Melting (SLM) in the as-built condition along with two post-treatments, namely solution heat treatment and artificial aging. Four different thicknesses of 1.0 mm, 1.5 mm, 2 mm, and 2.5 mm of SLM specimens, with the different post-treatments, underwent standardized Rockwell hardness tests using a spherical indenter to determine their hardness values and assess the impression using a stereo microscope and scanning electron microscope (SEM). The as-built specimens showed a trend of smaller indentation depths with increasing specimen thickness, and finally creased with 0.1547 mm depth at 2.5 mm. However, the post-treatments altered the behavior of the specimens to a certain degree, giving larger experimental indentation depths of 0.2204 mm, 0.1962 mm, and 0.1798 mm at 1.0 mm, 1.5 mm, and 2.5 mm thickness, respectively, after solution heat treatment. Artificial aging showed a general decrease in indentation depth with increasing specimen thickness in contrast to solution treatment, and resulted in depths of 0.1888 mm and 0.1596 mm at 1.0 mm and 2.5 mm thickness. Furthermore, a material numerical model was made using stress-strain data on ANSYS Workbench to develop a predictive model for the indentation behavior of the specimens in contrast to experimentation. Under multi-linear isotropic hardening, the Finite Element Analysis (FEA) simulation produced indentation geometry with an average accuracy of 95.4% for the artificial aging series.
引用
收藏
页数:24
相关论文
共 50 条
  • [31] Effect of Heat Treatment on Microstructure and Properties of Selective Laser Melting AlSi10Mg Alloy
    Jian, Haigen
    Yang, Man
    Fang, Wu
    Pai, Junjun
    Yang, Xiaomei
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, : 3267 - 3280
  • [32] Laser Weldability of AlSi10Mg Alloy Produced by Selective Laser Melting: Microstructure and Mechanical Behavior
    Carlo Alberto Biffi
    Jacopo Fiocchi
    Ausonio Tuissi
    Journal of Materials Engineering and Performance, 2019, 28 : 6714 - 6719
  • [33] Laser Weldability of AlSi10Mg Alloy Produced by Selective Laser Melting: Microstructure and Mechanical Behavior
    Biffi, Carlo Alberto
    Fiocchi, Jacopo
    Tuissi, Ausonio
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (11) : 6714 - 6719
  • [34] Thermal behavior in single track during selective laser melting of AlSi10Mg powder
    Wei, Pei
    Wei, Zhengying
    Chen, Zhen
    He, Yuyang
    Du, Jun
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2017, 123 (09):
  • [35] Thermal behavior in single track during selective laser melting of AlSi10Mg powder
    Pei Wei
    Zhengying Wei
    Zhen Chen
    Yuyang He
    Jun Du
    Applied Physics A, 2017, 123
  • [36] A study on cavitation erosion behavior of AlSi10Mg fabricated by selective laser melting (SLM)
    Zou, J.
    Zhu, Y.
    Pan, M.
    Xie, T.
    Chen, X.
    Yang, H.
    WEAR, 2017, 376 : 496 - 506
  • [37] Surface quality and fatigue behavior of L-PBF AlSi10Mg in as-built condition
    Konecna, Radomila
    Uriati, Federico
    Nicoletto, Gianni
    Tibor, Varmus
    SECOND EUROPEAN CONFERENCE ON THE STRUCTURAL INTEGRITY OF ADDITIVELY MANUFACTURED MATERIALS, 2021, 34 : 135 - 140
  • [38] Evolution of internal pores within AlSi10Mg manufactured by laser powder bed fusion under tension: As-built and heat treated conditions
    Hastie, James C.
    Koelblin, Joachim
    Kartal, Mehmet E.
    Attallah, Moataz M.
    Martinez, Rafael
    MATERIALS & DESIGN, 2021, 204
  • [39] Direction and location dependency of selective laser melted AlSi10Mg specimens
    Hitzler, Leonhard
    Janousch, Christoph
    Schanz, Jochen
    Merkel, Markus
    Heine, Burkhard
    Mack, Florian
    Hall, Wayne
    Oechsner, Andreas
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2017, 243 : 48 - 61
  • [40] Effect of Prewelding Solution Heat Treatment on Pore Defect in Laser Welding of AlSi10Mg Alloy Prepared by Selective Laser Melting
    Chen Weihao
    Liu Fencheng
    Niu Pengliang
    You Qifan
    Liu Fenggang
    Wang Zhitai
    RARE METAL MATERIALS AND ENGINEERING, 2024, 53 (04) : 1111 - 1119