High temperature oxidation behavior of liquid phases sintered SiC ceramics with ZrB 2 addition

被引:1
|
作者
Shen, Xu [1 ,3 ,4 ]
Zhang, Yu [1 ,3 ,4 ]
Ma, Qin [1 ,3 ,4 ]
Mu, Shuang [1 ,3 ,4 ]
Dong, Shaoming [1 ,2 ,3 ]
Yang, Jinshan [1 ,3 ]
机构
[1] Chinese Acad Sci, Shanghai Inst Ceram, State Key Lab High Performance Ceram & Superfine M, Shanghai 200050, Peoples R China
[2] Univ Chinese Acad Sci, Ctr Mat Sci & Optoelect Engn, Beijing 100049, Peoples R China
[3] Chinese Acad Sci, Shanghai Inst Ceram, Struct Ceram & Composites Engn Res Ctr, Shanghai 200050, Peoples R China
[4] Univ Chinese Acad Sci, Beijing 100049, Peoples R China
基金
国家重点研发计划; 中国国家自然科学基金;
关键词
SiC ceramics; ZrB2; Liquid phase sintered; Oxidation behavior; Microstructure; SIC/SIC COMPOSITES; MECHANICAL-PROPERTIES; SILICON-CARBIDE; MATRIX COMPOSITES; MICROSTRUCTURE; RESISTANCE; PYROLYSIS; GLASSES; Y2O3; INTERFACE;
D O I
10.1016/j.ceramint.2024.05.171
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The oxidation property of liquid-phase sintered silicon carbide (LPS-SiC) ceramics with ZrB 2 addition was studied after oxidation test in air at 1400 degrees C. The results indicate that the addition of ZrB 2 decreased the degree of polymerization (DOP) of the silicate networks in the oxide layer, suppressing the additional oxidation caused by residual bubbles in the oxide layer of LPS-SiC, which bypassed the layer and directly corroded the material internally. After 100 h of oxidation, the additional oxidation depth was found to be 125 mu m in the sample without ZrB 2 and 0 mu m in those containing 10 wt% ZrB 2 . Simultaneously, the decrease in DOP facilitates the migration of crystalline phases. The generated ZrSiO 4 can migrate and aggregate at the interface between the surface oxide layer and the SiC/ZrB 2 matrix, forming a continuous ZrSiO 4 barrier. This impedes the diffusion of the oxidant and enhances the oxidation resistance. However, an insufficient ZrB 2 content leads to a discontinuous ZrSiO 4 layer, thereby weakening its protective effect. Simultaneously, a decrease in DOP increases the rate of oxygen diffusion, resulting in an increase in the oxidation layer thickness. This study contributes to a better understanding of the failure mechanisms of LPS-SiC in oxidizing environments and provide a reference for the design of oxidationresistant LPS-SiC materials.
引用
收藏
页码:29142 / 29152
页数:11
相关论文
共 50 条
  • [21] Oxidation Behavior of ZrB2-YAG-Al2O3 Ceramics at High Temperature
    Song, Jie-Guang
    MATERIALS AND MANUFACTURING PROCESSES, 2010, 25 (08) : 724 - 729
  • [22] Mechanical and oxidation behavior of spark plasma sintered ZrB 2-ZrC-SiC composites
    Istanbul Technical University, Department of Metallurgical and Materials Engineering, 34469 Maslak Istanbul, Turkey
    J Ceram Soc Jpn, 1400 (143-149):
  • [23] Mechanical and oxidation behavior of spark plasma sintered ZrB2-ZrC-SiC composites
    Akin, Ipek
    Goller, Gultekin
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2012, 120 (1400) : 143 - 149
  • [24] Oxidation Behavior of a SPS Sintered ZrB2-SiC-MoSi2 Ceramic at 1500 °C
    Li, Qi
    Cao, Lamei
    Yi, Xiaosu
    INTERNATIONAL SYMPOSIUM ON MATERIALS APPLICATION AND ENGINEERING (SMAE 2016), 2016, 67
  • [25] Effect of graphite addition on the spark-plasma sinterability of ZrB2 and ZrB2-SiC ultra-high-temperature ceramics
    Zamora, Victor
    Nygren, Mats
    Guiberteau, Fernando
    Ortiz, Angel L.
    CERAMICS INTERNATIONAL, 2014, 40 (07) : 11457 - 11464
  • [26] Ultra High Temperature Oxidation Resistance and Strength of ZrB2-SiC Ceramics in Reduced Pressure Plasma
    Oguri, Kazuyuki
    Sekigawa, Takahiro
    Kamita, Tohru
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2011, 75 (05) : 291 - 296
  • [27] Liquid sintered SiC ceramics
    Kuei Suan Jen Hsueh Pao, 2 (191-197):
  • [28] High-temperature oxidation of AlN-ZrB2 ceramics
    Inst for Problems of Materials, Science, Kiev, Ukraine
    Key Eng Mat, Pt 3 (1625-1628):
  • [29] Combustion synthesis of high-temperature ZrB2-SiC ceramics
    Iatsyuk, I. V.
    Pogozhev, Yu. S.
    Levashov, E. A.
    Novikov, A. V.
    Kochetov, N. A.
    Kovalev, D. Yu.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2018, 38 (07) : 2792 - 2801
  • [30] Aqueous gelcasting of ZrB2-SiC ultra high temperature ceramics
    He, Rujie
    Zhang, Xinghong
    Hu, Ping
    Liu, Chen
    Han, Wenbo
    CERAMICS INTERNATIONAL, 2012, 38 (07) : 5411 - 5418