Study on the corrosion mechanism of Zr-1Sn- x Fe-0.2Cr-0.02Ni alloy in 500 ° C super-heated steam with oxygen

被引:0
|
作者
Xu, Shitong [1 ]
Xiao, Xiangyi [1 ]
Huang, Jiansong [1 ]
Li, Zhikang [1 ]
Yao, Meiyi [1 ]
Hu, Lijuan [1 ]
Xie, Yaoping [1 ]
Zhou, Bangxin [1 ]
机构
[1] Shanghai Univ, Sch Mat Sci & Engn, Shanghai 200444, Peoples R China
基金
中国国家自然科学基金;
关键词
A. Zirconium alloys; B; TEM; XPS; C. High temperature corrosion; DISSOLVED-OXYGEN; ZIRCONIUM; OXIDATION; RESISTANCE; BEHAVIOR; ZIRCALOY;
D O I
10.1016/j.corsci.2024.112121
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Zr-1Sn- x Fe-0.2Cr-0.02Ni ( x =0.3, 0.45, wt%) alloys were exposed in 500 degrees C super-heated steam with oxygen to investigate the effect of oxygen concentrations in the corrosion environment and Fe contents in the alloys on the corrosion behavior. Results showed that increasing the Fe contents from 0.3 % to 0.45 % and the oxygen concentrations from deaeration to 1000 ppb can both accelerate the corrosion of the alloys, and the mechanism was explored from the perspective of Fe and oxygen affecting the oxidation of alloying elements and the microstructure evolution of the oxide film.
引用
收藏
页数:14
相关论文
共 29 条
  • [21] Corrosion Resistance of Zr-0.7Sn-1Nb-0.03Fe-xCu-xGe (x=0, 0.05, 0.2) Alloys in Superheated Steam at 400 °C/10.3 MPa
    Tu Liming
    Zhang Jinlong
    Xu Qidi
    Yao Meiyi
    Zhou Bangxin
    RARE METAL MATERIALS AND ENGINEERING, 2015, 44 (06) : 1391 - 1396
  • [22] Corrosion resistance of Zr-0.7Sn-1Nb-0.03Fe-xCu-xGe (x=0, 0.05, 0.2) alloys in superheated steam at 400℃/10.3 MPa
    Tu, Liming
    Zhang, Jinlong
    Xu, Qidi
    Yao, Meiyi
    Zhou, Bangxin
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2015, 44 (06): : 1391 - 1396
  • [23] STUDY ON THE CORROSION RESISTANCE OF Zr-1Nb-0.7Sn-0.03Fe-xGe ALLOY IN LITHIATED WATER AT 360 °C
    Zhang Jinlong
    Xie Xingfei
    Yao Meiyi
    Zhou Bangxin
    Peng Jianchao
    Liang Xue
    ACTA METALLURGICA SINICA, 2013, 49 (04) : 443 - 450
  • [24] Comparative studies of the long-term corrosion behavior of Zr-Sn-Fe-Cr-Ni alloys in pure water at 360 °C/18.6 MPa with high and low dissolved oxygen content
    Lei, Aijia
    Dai, Xun
    Du, Yufeng
    Liao, Jingjing
    Deng, Ruiju
    Xu, Jiangtao
    Huang, Xuefei
    JOURNAL OF NUCLEAR MATERIALS, 2025, 603
  • [25] Influence of Solution Annealing Temperature on the Microstructure, Mechanical Properties, and Corrosion Resistance of a Lean Duplex Stainless Steel Fe-0.02C-20Cr-6Mn-1Ni-0.2N-0.35Si
    Sun, Jie
    Wu, Chunbo
    Han, Ying
    Liu, Zhenghong
    Sun, Jiapeng
    Zu, Guoqing
    Zhu, Weiwei
    Ran, Xu
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024,
  • [26] The study of stress application and corrosion cracking on Ni-16 Cr-9 Fe (Alloy 600) C-ring samples by polychromatic X-ray microdiffraction
    Chao, Jing
    Fuller, Marina L. Suominen
    McIntyre, N. Stewart
    Carcea, Anatolie G.
    Newman, Roger C.
    Kunz, Martin
    Tamura, Nobumichi
    ACTA MATERIALIA, 2012, 60 (03) : 781 - 792
  • [27] Study of the system Zr1-xTix(Cr0.5M0.4 V-0.1)(2)-H-2(0<=x<=0.2, M=Fe, Co, Ni).
    Bououdina, M
    Menier, P
    Soubeyroux, JL
    Fruchart, D
    JOURNAL OF ALLOYS AND COMPOUNDS, 1997, 253 : 302 - 307
  • [28] Study of the system Zr1-xTix(Cr0.5M0.4V0.1)2 - H2 (0&le x &le0.2, M=Fe, Co, Ni)
    Bououdina, M.
    Menier, P.
    Soubeyroux, J.L.
    Fruchart, D.
    Journal of Alloys and Compounds, 1997, 253-254 (1-2): : 302 - 307
  • [29] Study on the corrosion-wear behavior of Ni67.57Cr15.59Fe2.83C0.6Si3.98B3.47O0.045Mo2.97Co2.94 nickel alloy coating prepared by high velocity oxygen fuel spraying
    Ho, Kuo-Chang
    Sheu, Hung-Hua
    Chang, Jun-Kai
    Lin, Hwai-En
    Lee, Ya-Wei
    Hsiao, Po-Sen
    Lee, Hung-Bin
    Li, Wen-Ken