Investigation and evaluation of high-temperature lead-bismuth eutectic (LBE) corrosion resistance and compression performance of the FeCrAl-based coatings

被引:0
|
作者
Zhang, Wei [1 ]
Qiu, Xi [2 ]
Zhou, Mingyang [2 ]
Yang, Jijun [1 ]
机构
[1] Sichuan Univ, Inst Nucl Sci & Technol, Minist Educ, Key Lab Radiat Phys & Technol, Chengdu 610064, Peoples R China
[2] Nucl Power Inst China, Sci & Technol Reactor Syst Design Technol Lab, Chengdu 610213, Peoples R China
基金
中国国家自然科学基金;
关键词
FeCrAl coating; LBE corrosion; mechanical properties; F/M cladding tube; INTERFACIAL SHEAR-STRENGTH; ALUMINA SCALE GROWTH; 2 REACTIVE ELEMENTS; OXIDATION PERFORMANCE; ALLOY; STEEL; T91; COMPOSITE; STRESS;
D O I
10.1088/2053-1591/ad6820
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The high-temperature lead-bismuth eutectic (LBE) corrosion resistance and ring compression performance of the Fe15Cr11Al2Si, Fe15Cr11Al0.5Y, and Fe15Cr11Al2Si0.5Y coatings were investigated. Even if the corrosion test temperature reaches 800 degrees C, all these coatings can effectively protect the steel cladding tube. After the corrosion test temperature exceeded 660 degrees C, an obvious Al-rich oxide layer was formed on the surface of the coating, and Al element enrichment occurred at the interface between the coating and the substrate. After the corrosion test at 800 degrees C, holes appeared in the thick interface layer of the Fe15Cr11Al2Si0.5Y coating. The Fe15Cr11Al2Si coating cracked after the ring compression test with a deformation rate of 3%, and the coating peeled off after the deformation rate reached 5%. When the deformation rate reached 5%, there was still no cracking in the Fe15Cr11Al0.5Y coating. When the deformation rate reached 30%, the coating cracked, but the cracked coating was still tightly bonded with the substrate. The Fe15Cr11Al2Si0.5Y coating has the worst compression performance, even if the deformation rate is 1%, the coating still peels off obviously. The underlying mechanism for the evolution of corrosion resistance and compression performance was discussed.
引用
收藏
页数:17
相关论文
共 43 条
  • [21] Early stages of dissolution corrosion in 316L and DIN 1.4970 austenitic stainless steels with and without anticorrosion coatings in static liquid lead-bismuth eutectic (LBE) at 500 °C
    Charalampopoulou, Evangelia
    Lambrinou, Konstantina
    Van der Donck, Tom
    Paladino, Boris
    Di Fonzo, Fabio
    Azina, Clio
    Eklund, Per
    Mraz, Stanislav
    Schneider, Jochen M.
    Schryvers, Dominique
    Delville, Remi
    MATERIALS CHARACTERIZATION, 2021, 178
  • [22] Microstructure, mechanical and oxygen-deficient lead-bismuth eutectic corrosion properties of FeCrAlTiMo high-entropy alloy coatings for fuel claddings
    Yang, Jian
    Zhang, Feifei
    Zhai, Lihong
    Qu, Guofeng
    Yang, Jijun
    INTERMETALLICS, 2024, 175
  • [23] Revealing different corrosion behaviors of Cr-containing refractory high-entropy alloy coatings in static liquid lead-bismuth eutectic
    Deng, Jiuguo
    Zhang, Wei
    Qiu, Xi
    Zhou, Mingyang
    Zhou, Yi
    Liu, Ning
    Yang, Jijun
    MATERIALS & DESIGN, 2024, 244
  • [24] Improved lead-bismuth eutectic corrosion resistance and mechanical properties of reactive gas pulse sputtered AlCrFeMoTi/(AlCrFeMoTi)N composite multilayered high-entropy alloy coatings
    Yang, Jian
    Lyu, Liangliang
    Qiu, Xi
    Zhou, Mingyang
    Zhou, Yi
    Li, Quan
    Chen, Qingsong
    Liu, Hao
    Zhong, Yilong
    Deng, Jiuguo
    Zhang, Wei
    Zhu, Changda
    Liu, Ning
    Yang, Jijun
    JOURNAL OF NUCLEAR MATERIALS, 2022, 572
  • [25] Low-temperature oxy-nitriding of 316 L austenitic stainless steel for improved corrosion resistance in liquid lead-bismuth eutectic
    Chen, Guang
    Wang, Jun
    Zhang, Hongtao
    Li, Longyi
    Fan, Hongyuan
    SCRIPTA MATERIALIA, 2021, 202
  • [26] Early corrosion behavior of low carbon 9Cr-ODS steel in high temperature oxygen-saturated lead-bismuth eutectic
    Yang, Chongdou
    Xu, Yuwen
    Yun, Di
    Zhao, Bingyao
    Liu, Wenguan
    Gao, Rui
    Xie, Shijing
    Qiu, Jie
    CORROSION SCIENCE, 2024, 236
  • [27] Effect of Substrate Bias Voltage on the High-Temperature Corrosion Resistance and Cutting Performance of CrAlN Coatings
    Jie, Song
    Tian, Haiping
    Li, Junzhou
    Zhang, Pengjiao
    An, Sun
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024,
  • [28] EVALUATION OF HIGH-TEMPERATURE CORROSION-RESISTANCE OF AL DIFFUSION COATINGS BY AC IMPEDANCE METHOD
    WU, C
    NISHIKATA, A
    TSURU, T
    TAKEI, A
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1992, 56 (10) : 1161 - 1167
  • [29] Numerical simulation of energy-mass transport in high-pressure liquid CO2 injected into high-temperature liquid lead-bismuth eutectic pool
    Yuan, Junjie
    Liu, Li
    Bao, Ruiqi
    Luo, Haotian
    Jia, Zheng
    Chen, Shuo
    Gu, Hanyang
    APPLIED THERMAL ENGINEERING, 2025, 267
  • [30] Insight into the structure and protective performance of Mo/FeCrAl bilayer coatings on Zry-4 substrates in hydrothermal corrosion and high-temperature steam environment
    Zhu, Pengzhou
    Wang, Junjun
    Huang, Weijiu
    Ruan, Haibo
    Ning, Yi
    Zhang, Tengfei
    Xu, Meng
    Liao, Haiyan
    Su, Yongyao
    SURFACE & COATINGS TECHNOLOGY, 2025, 497