Temperature rise in photopolymerized adhesively-bonded resin composite: A thermography study

被引:4
|
作者
Algamaiah, Hamad [1 ]
Yang, Jiawei [2 ,3 ]
Alayed, Abdulaziz [1 ,5 ]
Alshabib, Abdulrahman [1 ]
Alshehri, Abdullah [4 ]
Watts, David C. [5 ,6 ,7 ,8 ]
机构
[1] King Saud Univ, Coll Dent, Dept Restorat Dent Sci, POB 60169, Riyadh 11545, Saudi Arabia
[2] Shanghai Jiao Tong Univ, Shanghai Peoples Hosp 9, Coll Stomatol, Sch Med,Dept prosthodont, Shanghai, Peoples R China
[3] Shanghai Jiao Tong Univ, Natl Clin Res Ctr Oral Dis, Coll Stomatol, Sch Med, Shanghai, Peoples R China
[4] Prince Sattam bin Abdulaziz Univ, Coll Dent, Dept Conservat Dent Sci, Alkharj 11942, Saudi Arabia
[5] Univ Manchester, Sch Med Sci, Div Dent, Biomat Sci, Manchester, England
[6] Univ Manchester, Photon Sci Inst, Manchester, England
[7] Univ Manchester, Sch Med Sci, Coupland 3 Bldg,Oxford Rd, Manchester M13 9PL, England
[8] Photon Sci Inst, Coupland 3 Bldg,Oxford Rd, Manchester M13 9PL, England
关键词
Thermal imaging; Thermographic analysis; Bonding agent; Universal adhesive; Resin composite; Bulk-fill resin composites; High-irradiance; URPBF; Dentin; AFCT; RAFT; BULK-FILL COMPOSITES; POLYMERIZATION SHRINKAGE; CONVERSION; LIGHT; KINETICS; COMPONENTS; EXPOSURE; EXOTHERM; DENTIN; MODES;
D O I
10.1016/j.dental.2023.12.006
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: To assess visually and quantitatively the contributions of the adhesive layer photopolymerization and the subsequent resin composite increment to spatio-temporal maps of temperature at five different cavity locations, subjected to two irradiance curing protocols: standard and ultra-high. Methods: Caries-free molars were used to obtain 40, 2 mm thick dentin slices, randomly assigned to groups (n = 5). These slices were incorporated within 3D-printed model cavites, 4 mm deep, restored with Adhese (R) Universal bonding agent and 2 mm thick Tetric (R) Powerfill resin composite, and photocured sequentially, as follows: G1: control-empty cavity; G2: adhesive layer; G3 composite layer with no adhesive; and G4 composite layer with adhesive. The main four groups were subdivided based on two curing protocols, exposed either to standard 10 s (1.2 W/cm(2)) or Ultra high 3 s (3 W/cm(2)) irradiance modes using a Bluephase PowerCure LCU. Temperature maps were obtained, via a thermal imaging camera, and numerically analyzed at 5 locations. The data were analyzed using two-way ANOVA followed by multiple one-way ANOVA, independent t-tests and Tukey post-hoc tests (alpha = 0.05). T-max, Delta T, T-int (integrated area under the curve) and time-to-reach-maximum-temperature were evaluated. Results: Two-way ANOVA showed that there was no significant interaction between light-curing time and location on the measured parameters (p > 0.05), except for the time-to-reach-maximum-temperature (p < 0.05). Curing the adhesive layer alone with the 10 s protocol resulted in a significantly increased pulpal roof temperature compared to 3 s cure (p < 0.05). Independent T-tests between G3 and G4, between 3 s and 10 s, confirmed that the adhesive agent caused no significant increases (p > 0.05) on the measured parameters. The ultra-high light-curing protocol significantly increased Delta T in composite compared to 10 s curing (p < 0.05). Significance: When the adhesive layer was photocured alone in a cavity, with a 2 mm thick dentin floor, the exothermal release of energy resulted in higher temperatures with a 10 s curing protocol, compared to a 3 s high irradiance. But when subsequently photocuring a 2 mm layer of composite, the resultant temperatures generated at pulpal roof location from the two curing protocols were similar and therefore there was no increased hazard to the dental pulp from the immediately prior adhesive photopolymerization, cured via the ultra-high irradiation protocol.
引用
收藏
页码:458 / 465
页数:8
相关论文
共 50 条
  • [31] The fracture behaviour of adhesively-bonded composite joints: Effects of rate of test and mode of loading
    Blackman, B. R. K.
    Kinloch, A. J.
    Rodriguez-Sanchez, F. S.
    Teo, W. S.
    INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 2012, 49 (13) : 1434 - 1452
  • [32] Damage analysis of composite-aluminium adhesively-bonded single-lap joints
    Ribeiro, T. E. A.
    Campilho, R. D. S. G.
    da Silva, L. F. M.
    Goglio, L.
    COMPOSITE STRUCTURES, 2016, 136 : 25 - 33
  • [33] The effects of pre-bond moisture on the fracture behaviour of adhesively-bonded composite joints
    Blackman, B. R. K.
    Johnsen, B. B.
    Kinloch, A. J.
    Teo, W. S.
    JOURNAL OF ADHESION, 2008, 84 (03): : 256 - 276
  • [34] Geometrical parameter study of adhesively-bonded T-joints by cohesive models
    Lopes, J. P. M.
    Campilho, R. G. S. G.
    Rocha, R. J. B.
    Silva, F. J. G.
    4TH INTERNATIONAL CONFERENCE ON STRUCTURAL INTEGRITY (ICSI 2021), 2022, 37 : 714 - 721
  • [35] A study of the impact properties of adhesively-bonded aluminum alloy based on impact velocity
    Teng Gao
    Anthony J. Kinloch
    Bamber R. K. Blackman
    F. S. Rodriguez Sanchez
    Sang-kyo Lee
    Chongdu Cho
    Hye-jin Bang
    Seong Sik Cheon
    Jae Ung Cho
    Journal of Mechanical Science and Technology, 2015, 29 : 493 - 499
  • [36] Study of the crack deviation angle in adhesive ruptures of ceramic adhesively-bonded assemblies
    Levallois, F
    El Abdi, R
    Baziard, Y
    Petit, JA
    JOURNAL OF ADHESION, 1997, 60 (1-4): : 1 - 14
  • [37] A study of the impact properties of adhesively-bonded aluminum alloy based on impact velocity
    Gao, Teng
    Kinloch, Anthony J.
    Blackman, Bamber R. K.
    Sanchez, F. S. Rodriguez
    Lee, Sang-kyo
    Cho, Chongdu
    Bang, Hye-jin
    Cheon, Seong Sik
    Cho, Jae Ung
    JOURNAL OF MECHANICAL SCIENCE AND TECHNOLOGY, 2015, 29 (02) : 493 - 499
  • [38] Adhesively-bonded joints in metallic alloys, polymers and composite materials: Mechanical and environmental durability performance
    A. Baldan
    Journal of Materials Science, 2004, 39 : 4729 - 4797
  • [39] Strength of adhesively-bonded tubular single lap carbon/epoxy composite-steel joints
    Kim, YG
    Oh, JH
    Lee, DG
    JOURNAL OF COMPOSITE MATERIALS, 1999, 33 (20) : 1897 - 1917
  • [40] Adhesion failure propagation in adhesively-bonded single-lap laminated FRP composite joints
    Panigrahi, S.K.
    Pradhan, B.
    Journal of Adhesion Science and Technology, 2007, 21 (5-6): : 379 - 398