The effects of temperature and hygrothermal aging on the properties of CF/PA6 composite and its compression failure mechanisms

被引:2
|
作者
Yu, Mingming [1 ]
Xiao, Rongbin [1 ]
Xie, Wang [1 ]
Liu, Xueqiang [2 ]
Ge, Lili [1 ]
Fang, Lin [1 ]
Ren, Musu [1 ]
Sun, Jinliang [1 ]
机构
[1] Shanghai Univ, Res Ctr Composite Mat, Shanghai 200444, Peoples R China
[2] Res Ctr Mat, Inst Syst Engn, Beijing, Peoples R China
关键词
CF/PA6; composites; elevated temperature; failure mechanisms; hygrothermal; residual compression strength; IMPACT BEHAVIOR; HUMIDITY; TENSILE; MOISTURE; DAMAGE;
D O I
10.1002/pc.28506
中图分类号
TB33 [复合材料];
学科分类号
摘要
Carbon fiber reinforced polyamide composites have outstanding properties, but their applications are significantly affected by the service environment. This work evaluates the effects of temperature (25, 80, 140, and 200 degrees C) and hygrothermal conditions on the mechanical properties of CF/PA6 composite containing delamination damage, and studies its damage behaviors and failure mechanisms. After hygrothermal aging, recrystallization of PA6 improves the heat resistance of CF/PA6 composites, but water absorption reduces the interfacial strength of composites, resulting in the decrease of modulus and compressive strength (24% and 42%, respectively). With the increase in temperature, the compressive strength of CF/PA6 composites gradually decreases (from 132 MPa at 25 degrees C to 24 MPa at 200 degrees C), and the failure mode transitions from fiber fractures, interlayer shear fractures, delamination to kinking. In addition, the compressive failure process of CF/PA6 composites is divided into three stages: buckling, delamination bulging and kinking failure. Highlights Hygrothermal aging reduces the fiber/resin interface performance.<br /> Fiber fracture, interlayer shear and delamination convert to kinking failure.<br /> The failure process is divided into buckling, delamination and kinking
引用
收藏
页码:10775 / 10787
页数:13
相关论文
共 50 条
  • [31] Simulation of Temperature Field in Selective Laser Sintering on PA6/Cu Composite Powders
    Zhang, Jian
    Li, Deying
    Qiu, Bin
    Zhao, Longzhi
    ADVANCED MATERIALS RESEARCH, 2011, 213 : 519 - 523
  • [32] Influence of hygrothermal aging on dimensional stability of thin injection-molded short glass fiber reinforced PA6 materials
    Illing, Thomas
    Schossig, Marcus
    Bieroegel, Christian
    Grellmann, Wolfgang
    JOURNAL OF APPLIED POLYMER SCIENCE, 2015, 132 (28)
  • [33] Friction and wear mechanisms of a thermoplastic composite GF/PA6 subjected to different thermal histories
    Cartledge, HCY
    Baillie, C
    Mai, YW
    WEAR, 1996, 194 (1-2) : 178 - 184
  • [34] Copper nanowire/PA6 composites prepared by in situ polymerization and its properties
    Xu, Qijie
    Li, Xiaohong
    Zhang, Shengmao
    Hao, Yanping
    Zhang, Zhijun
    JOURNAL OF POLYMER RESEARCH, 2013, 20 (10)
  • [35] Fracture mechanisms and failure analysis of PA6/NBR/graphene nanocomposites by essential work of fracture
    Nakhaei, Mohammad Reza
    Naderi, Ghasem
    Ghoreishy, Mir Hamid Reza
    IRANIAN POLYMER JOURNAL, 2021, 30 (09) : 975 - 987
  • [36] Fracture mechanisms and failure analysis of PA6/NBR/graphene nanocomposites by essential work of fracture
    Mohammad Reza Nakhaei
    Ghasem Naderi
    Mir Hamid Reza Ghoreishy
    Iranian Polymer Journal, 2021, 30 : 975 - 987
  • [37] Oligomer composition and content in regenerated PA6 fiber and its effect on properties
    Wang, Yongjun
    Guo, Yintao
    Zhong, Shuimi
    Lin, Qisong
    Gao, Feng
    Chen, Wenxing
    Lu, Wangyang
    JOURNAL OF APPLIED POLYMER SCIENCE, 2024, 141 (13)
  • [38] Copper nanowire/PA6 composites prepared by in situ polymerization and its properties
    Qijie Xu
    Xiaohong Li
    Shengmao Zhang
    Yanping Hao
    Zhijun Zhang
    Journal of Polymer Research, 2013, 20
  • [39] Effects of hygrothermal aging on bending properties of PBO fiber/epoxy resin composite
    Wang, Yi-Long
    Liu, Xiao-Yun
    Zhuang, Qi-Xin
    Han, Zhe-Wen
    Liu, Xiao-Yun, 1600, Journal of Solid Rocket Technology (37): : 704 - 710
  • [40] Effect on the mechanic properties and failure morphology of the modified PA6/keviar fiber composites
    College of Chemistry and Chemical Engineering, Fuzhou University, Fuzhou 350002, China
    Gaofenzi Cailiao Kexue Yu Gongcheng, 2006, 1 (151-153+157):