Effects of processing parameters on fabrication defects, microstructure and mechanical properties of additive manufactured Mg–Nd–Zn–Zr alloy by selective laser melting process

被引:0
|
作者
Wenyu Xu [1 ]
Penghuai Fu [1 ,2 ]
Nanqing Wang [1 ]
Lei Yang [1 ]
Liming Peng [1 ]
Juan Chen [1 ]
Wenjiang Ding [1 ]
机构
[1] National Engineering Research Center of Light Alloy Net Forming and State Key Laboratory of Metal Matrix Composite, School of Materials Science and Engineering, Shanghai Jiao Tong University
[2] Shanghai Light Alloy Net Forming National Engineering Research Center Co,
关键词
D O I
暂无
中图分类号
TG146.22 []; TG665 [光能加工设备及其加工];
学科分类号
摘要
Mg–3Nd–0.2Zn–0.4Zr(NZ30K, wt.%) alloy is a new kind of high-performance metallic biomaterial. The combination of the NZ30K Magnesium(Mg) alloy and selective laser melting(SLM) process seems to be an ideal solution to produce porous Mg degradable implants.However, the microstructure evolution and mechanical properties of the SLMed NZ30K Mg alloy were not yet studied systematically.Therefore, the fabrication defects, microstructure, and mechanical properties of the SLMed NZ30K alloy under different processing parameters were investigated. The results show that there are two types of fabrication defects in the SLMed NZ30K alloy, gas pores and unfused defects.With the increase of the laser energy density, the porosity sharply decreases to the minimum first and then slightly increases. The minimum porosity is 0.49 ± 0.18%. While the microstructure varies from the large grains with lamellar structure inside under low laser energy density,to the large grains with lamellar structure inside & the equiaxed grains & the columnar grains under middle laser energy density, and further to the fine equiaxed grains & the columnar grains under high laser energy density. The lamellar structure in the large grain is a newly observed microstructure for the NZ30K Mg alloy. Higher laser energy density leads to finer grains, which enhance all the yield strength(YS), ultimate tensile strength(UTS) and elongation, and the best comprehensive mechanical properties obtained are YS of 266 ± 2.1 MPa,UTS of 296 ± 5.2 MPa, with an elongation of 4.9 ± 0.68%. The SLMed NZ30K Mg alloy with a bimodal-grained structure consisting of fine equiaxed grains and coarser columnar grains has better elongation and a yield drop phenomenon.
引用
收藏
页码:2249 / 2266
页数:18
相关论文
共 50 条
  • [31] Hot deformation microstructure and mechanical properties of Mg-Zn-Nd-Cd-Zr alloy
    Liu, Xianlan
    Liu, Chuming
    Zhang, Wenyu
    Li, Huizhong
    Zeng, Sumin
    ADVANCED MATERIALS AND PROCESSES, PTS 1-3, 2011, 311-313 : 690 - +
  • [32] Effect of Nd on the microstructure and mechanical properties of Mg–3Zn-0.5Zr alloy
    Zhang, J.H.
    Nie, K.B.
    Deng, K.K.
    Han, X.Z.
    Wang, Z.D.
    Materials Science and Engineering: A, 2022, 838
  • [33] Microstructure and mechanical properties of extruded Mg-Zn-Nd-Y-Zr-Ca alloy
    Li, Q
    Wang, QD
    Zeng, XQ
    Ding, WJ
    Tang, QB
    Huang, SD
    MAGNESIUM - SCIENCE, TECHNOLOGY AND APPLICATIONS, 2005, 488-489 : 385 - 388
  • [34] Effect of Nd on the microstructure and mechanical properties of Mg-3Zn-0.5Zr alloy
    Zhang, J. H.
    Nie, K. B.
    Deng, K. K.
    Han, X. Z.
    Wang, Z. D.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 838
  • [35] Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting
    Croteau, Joseph R.
    Griffiths, Seth
    Rossell, Marta D.
    Leinenbach, Christian
    Kenel, Christoph
    Jansen, Vincent
    Seidman, David N.
    Dunand, David C.
    Vo, Nhon Q.
    ACTA MATERIALIA, 2018, 153 : 35 - 44
  • [36] Microstructure and mechanical properties of pure copper manufactured by selective laser melting
    Yan, Xingchen
    Chang, Cheng
    Dong, Dongdong
    Gao, Shuohong
    Ma, Wenyou
    Liu, Min
    Liao, Hanlin
    Yin, Shuo
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 789
  • [37] Effects of process parameters on microstructure properties of WE43 magnesium alloy by selective laser melting
    Shi, Yangyang
    Guo, Kai
    Shi, Hao
    Huang, Xiaoming
    Yang, Bin
    Sun, Jie
    MATERIALS TODAY COMMUNICATIONS, 2024, 39
  • [38] Effect of direct aging on the microstructure and tensile properties of AlSi10Mg alloy manufactured by selective laser melting process
    Park, Tae-Hyun
    Baek, Min-Seok
    Hyer, Holden
    Sohn, Yongho
    Lee, Kee-Ahn
    Lee, Kee-Ahn (keeahn@inha.ac.kr), 1600, Elsevier Inc. (176):
  • [39] Effect of direct aging on the microstructure and tensile properties of AlSi10Mg alloy manufactured by selective laser melting process
    Park, Tae-Hyun
    Baek, Min-Seok
    Hyer, Holden
    Sohn, Yongho
    Lee, Kee-Ahn
    MATERIALS CHARACTERIZATION, 2021, 176
  • [40] Research on the formation process of selective laser melting Mg-Y-Sm-Zn-Zr alloy
    Wang, Wenli
    He, Lun
    Yang, Xin
    Wang, Dan
    MATERIALS SCIENCE AND TECHNOLOGY, 2021, 37 (02) : 174 - 181