Usually a post-weld heat treatment is performed on weld repairs for heavy section low alloy 2.25Cr-1 Mo steel power plant components. This procedure relieves the stresses in the weldment and results in improvements in both the room and high temperature properties. A significant saving, in both time and cost, could be realized if the post-weld heat treatment could be safely eliminated by an in situ heat treatment or non-post-weld heat treatment. In the present work, two different multi-pass and multi-layer welding procedures were employed and the resulting welds were subjected to a simulated in situ heat treatment of 538-degrees-C for up to 4000 h. The first procedure followed the relatively standard weaving method of pressure pipe welding, while the second involved a low heat input ratio temper-bead technique. A refined grain structure, within the HAZ was observed for both welding procedures. After exposure, at the simulated operating temperature of 538-degrees-C, there was an initial rapid reduction in hardness and an increase in toughness. Carbide development had a major influence on the mechanical properties. The conventional welding procedure resulted in a higher degree of tempering than the temper-bead weld procedure.
引用
收藏
页码:345 / 358
页数:14
相关论文
共 50 条
  • [41] CREEP LIFE ESTIMATION OF 2.25CR-1MO STEEL WELD-JOINTS BY A PARAMETRIC METHOD
    AHILA, S
    IYER, SR
    RADHAKRISHNAN, VM
    INDIAN JOURNAL OF ENGINEERING AND MATERIALS SCIENCES, 1994, 1 (01) : 48 - 52
  • [42] Effect of cold working deformation on the internal friction of 2.25Cr-1Mo steel
    Liu, Xinbao
    Shiwa, Mitsuharu
    Sawada, Kota
    Yamawaki, Hisashi
    Watanabe, Makoto
    Yin, Fuxing
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (24-25): : 6741 - 6744
  • [43] SERRATED FLOW BEHAVIOR OF 2.25CR-1MO STEEL BASE-METAL, WELDMENTS AND SIMULATED HEAT-AFFECTED ZONE STRUCTURES
    LAHA, K
    CHANDRAVATHI, KS
    RAO, KBS
    MANNAN, SL
    ZEITSCHRIFT FUR METALLKUNDE, 1994, 85 (12): : 839 - 844
  • [44] HOT CORROSION OF 2.25CR-1MO BOILER TUBE STEEL AND ITS WELDMENTS .2. CORROSION MECHANISM
    AHILA, S
    IYER, SR
    RADHAKRISHNAN, VM
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 1994, 47 (2-3): : 183 - 191
  • [45] Carbide development in the heat affected zone of tempered and post-weld heat treated 2,25Cr-1Mo steel weldments
    Peddle, BE
    Pickles, CA
    CANADIAN METALLURGICAL QUARTERLY, 2001, 40 (01) : 105 - 125
  • [46] EFFECT OF IMPURITY LEVEL AND NORMALIZING CONDITION ON CREEP RUPTURE BEHAVIOR OF 2.25CR-1MO STEEL THICK WELD JOINT
    Tezuka, Hideshi
    Kato, Hideto
    JOINT EPRI - 123HIMAT INTERNATIONAL CONFERENCE ON ADVANCES IN HIGH-TEMPERATURE MATERIALS, 2019, 2019, : 162 - 173
  • [47] THE NUCLEATION OF HIGH-TEMPERATURE BRITTLE INTERGRANULAR FRACTURE IN 2.25CR-1MO STEEL
    HIPPSLEY, CA
    LEWANDOWSKI, JJ
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1988, 19 (12): : 3005 - 3011
  • [48] HOT CORROSION OF 2.25CR-1MO BOILER TUBE STEEL AND ITS WELDMENTS .1. THERMOGRAVIMETRIC AND METALLURGICAL STUDY
    AHILA, S
    IYER, SR
    RADHAKRISHNAN, VM
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 1994, 47 (2-3): : 169 - 182
  • [49] RESTORATION OF ELEVATED-TEMPERATURE TENSILE-STRENGTH IN 2.25CR-1MO STEEL
    WADA, T
    BISS, VA
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1983, 14 (05): : 845 - 855
  • [50] Low temperature fracture toughness of embrittled 2.25Cr-1Mo pressure vessel steel
    Islam, A
    Knott, JF
    Bowen, P
    ADVANCES IN MECHANICAL BEHAVIOUR, PLASTICITY AND DAMAGE, VOLS 1 AND 2, PROCEEDINGS, 2000, : 1415 - 1420