STRUCTURAL FEATURES OF GROWTH OF SHORT CRACKS IN A HIGH-STRENGTH STEEL

被引:0
|
作者
KISHKINA, SI
MANAEVA, KG
GUK, NV
机构
[1] All-Union Institute of Aviation Materials, Moscow
来源
SOVIET MATERIALS SCIENCE | 1992年 / 27卷 / 05期
关键词
D O I
10.1007/BF00726458
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the fatigue fracture surfaces of the high-strength steel the zone of failure borders with the structure-sensitive zone (SSZ), whose microrelief depends on the microstructure of the steel (diameter of the primary grain, the size of the martensite packet and its orientation). Outside the limits of the SSZ there is a regular fatigue relief-secondary cracks and striations with the same orientation. The SSZ dimensions determine the boundary between the short and long cracks. The short cracks in the examined steels are 2-2.5 mm long. At high stresses this boundary is displaced to even shorter cracks and may be smaller than a millimeter. When using the Δl/ΔN (l) coordinates, the dependences for describing crack growth in the SSZ and in the zone with the regular fatigue relief differ. In the SSZ the crack growth rate decreases with an increase of the crack length to 200-300 μm; further growth of the crack is described with sufficient accuracy by the logarithmic dependence. In the zone with the regular fatigue relief the growth rate of the short crack is an exponential function of its length and, consequently, the stress intensity factor. © 1992 Plenum Publishing Corporation.
引用
收藏
页码:471 / 476
页数:6
相关论文
共 50 条
  • [41] Levelling of high-strength steel
    Fimi S.p.A., Vigano , Italy
    Metall Plant Technol Int, 2012, 4 (78-81):
  • [42] PLANING HIGH-STRENGTH STEEL
    CHERNENKO, AF
    SOVIET ENGINEERING RESEARCH, 1984, 4 (11): : 36 - 37
  • [43] RULES OF DEVELOPMENT OF FATIGUE CRACKS IN HIGH-STRENGTH STEEL IN 2-FREQUENCY LOADING
    TRUFYAKOV, VI
    MIKHEEV, PP
    KNYSH, VV
    KUZMENKO, AZ
    KARZOV, GP
    LUSHKOV, EN
    SOVIET MATERIALS SCIENCE, 1987, 23 (02): : 170 - 172
  • [44] Occurrence of cold cracks in welding of high-strength S960 QL steel
    Garašié, Ivica
    Ćorié, Anto
    Kožuh, Zoran
    Samardžié, Ivan
    Tehnicki Vjesnik, 2010, 17 (03): : 327 - 335
  • [45] HYDROGEN OXYGEN AND SUBCRITICAL CRACK GROWTH IN A HIGH-STRENGTH STEEL
    HANCOCK, GG
    JOHNSON, HH
    TRANSACTIONS OF THE METALLURGICAL SOCIETY OF AIME, 1966, 236 (04): : 513 - &
  • [46] OCCURRENCE OF COLD CRACKS IN WELDING OF HIGH-STRENGTH S960 QL STEEL
    Garasic, Ivica
    Coric, Anto
    Kozuh, Zoran
    Samardzic, Ivan
    TEHNICKI VJESNIK-TECHNICAL GAZETTE, 2010, 17 (03): : 327 - 335
  • [47] Method of calculating the shear strength of steel reinforced high-strength concrete short columns
    Jiang, Dong-Hong
    Wang, Lian-Guang
    Liu, Zhi-Yang
    Sun, Yi-Zeng
    Liaoning Gongcheng Jishu Daxue Xuebao (Ziran Kexue Ban)/Journal of Liaoning Technical University (Natural Science Edition), 2002, 21 (02):
  • [48] Numerical study of high-strength spiral stirrup confined high-strength concrete filled high-strength square steel tubular short columns under axial compression
    Yang, Zhijian
    Sun, Lisuo
    Liu, Mo
    STRUCTURES, 2025, 72
  • [49] Steel - structural material of the Modern Era - from cast iron to high-strength, weldable structural steel
    Werner, Frank
    Zimmermann, Gerd
    STAHLBAU, 2019, 88 (10) : 1024 - 1033
  • [50] Structural Transformation of the Surface of a High-Strength Steel after Hydroabrasive Action
    Tereshchenko, N. A.
    Tabatchikova, T. I.
    Yakovleva, I. L.
    Gudnev, N. Z.
    JOURNAL OF SURFACE INVESTIGATION, 2019, 13 (06): : 1336 - 1342