- [22] HOT CORROSION OF 2.25CR-1MO BOILER TUBE STEEL AND ITS WELDMENTS .1. THERMOGRAVIMETRIC AND METALLURGICAL STUDY TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 1994, 47 (2-3): : 169 - 182
- [24] Corrosion fatigue crack growth in clad low-alloy steels .1. Water flow rate effects in high-sulfur plate steel JOURNAL OF PRESSURE VESSEL TECHNOLOGY-TRANSACTIONS OF THE ASME, 1997, 119 (03): : 255 - 263
- [25] EFFECTS OF IMPURITY SEGREGATION ON SUSTAINED LOAD CRACKING OF 2-1/4 CR-1MO STEELS .1. CRACK INITIATION ACTA METALLURGICA, 1987, 35 (03): : 593 - 608
- [26] Development of Sulfuric and Hydrochloric Acid Dew-Point Corrosion-Resistant Steels: 1. Effect of Alloying Elements on the Corrosion Resistance of Low-Alloy Steels KOREAN JOURNAL OF METALS AND MATERIALS, 2014, 52 (11): : 837 - 855
- [27] TEMPER EMBRITTLEMENT OF LOW-ALLOY NI-CR STEELS .1. SUSCEPTIBILITY TO TEMPER EMBRITTLEMENT AND THE INFLUENCE OF INTERMEDIATE TEMPERING TREATMENTS ACTA METALLURGICA, 1980, 28 (03): : 335 - 356
- [28] Effects of local-brittle-zone (LBZ) microstructures on crack initiation and propagation in three Mo-added high-strength low-alloy (HSLA) steels MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 760 : 125 - 133