RAPID CRACK-PROPAGATION IN SMALL-DIAMETER THERMOPLASTIC PIPE

被引:0
|
作者
LEEVERS, PS
FREEMAN, PN
ARTHUR, MM
机构
关键词
D O I
暂无
中图分类号
TB33 [复合材料];
学科分类号
摘要
The S4 (small scale steady state) test, measuring resistance to fast-running fracture, is to become a specifying standard for PE gas pipe. To extend understanding of the method, and to assess its broader usefulness in polymer testing. S4 tests were carried out on commercial 50 mm diameter pipe of 3-6 mm nominal thickness to compare MDPE with ten other polymers used in process pipework. Results were normalised, on a hoop stress basis, to a mean radius to thickness ratio of 5 (SDR 11), and must also be factored up to estimate any service critical pressure. On this basis, MDPE, with a 0 degrees C S4 critical pressure of 2.8 bar, was matched by PVDF and slightly bettered by PB. ABS performed very well, exceeding 20 bar. PP homopolymer, PA6 and PTFE also out-performed MDPE, but PC, modified PVC and PP random copolymer failed to survive 2 bar. The critical pressure of POM was too low to measure.
引用
收藏
页码:113 / 121
页数:9
相关论文
共 50 条
  • [21] RAPID CRACK-PROPAGATION IN A HIGH-STRENGTH STEEL
    HAHN, GT
    HOAGLAND, RG
    ROSENFIELD, AR
    SEJNOHA, R
    METALLURGICAL TRANSACTIONS, 1974, 5 (02): : 475 - 482
  • [22] AN ALTERNATIVE METHOD TO STUDY RAPID CRACK-PROPAGATION IN PE
    GENUSSOV, RMS
    WILLIAMS, JG
    INSTITUTE OF PHYSICS CONFERENCE SERIES, 1989, (102): : 149 - 156
  • [23] Nonaxiality of small-diameter pipe inner surface inspection sensor
    College of Mechanical Engineering, University of Shanghai for Science and Technology, Shanghai 200093, China
    不详
    Guangdianzi Jiguang, 2006, 4 (410-414):
  • [24] ULTRASONIC INSPECTION OF SMALL-DIAMETER RIBBED-BORE PIPE
    BURMISTROV, VV
    KONONOVA, OM
    TRESHCHALIN, MA
    SOVIET JOURNAL OF NONDESTRUCTIVE TESTING-USSR, 1978, 14 (02): : 182 - 184
  • [25] RESISTANCE OF PIPE GRADE POLYETHYLENES TO HIGH-SPEED CRACK-PROPAGATION
    LEEVERS, PS
    WILLIAMS, JG
    JOURNAL DE PHYSIQUE, 1988, 49 (C-3): : 231 - 236
  • [26] CRACK-PROPAGATION IN KCL
    FREIMAN, SW
    BECHER, PF
    AMERICAN CERAMIC SOCIETY BULLETIN, 1974, 53 (04): : 319 - 319
  • [27] CRACK-PROPAGATION IN POLYCARBONATE
    GLOVER, AP
    JOHNSON, FA
    RADON, JC
    POLYMER ENGINEERING AND SCIENCE, 1974, 14 (06): : 420 - 428
  • [28] CRACK-PROPAGATION IN PZT
    KOEPKE, BG
    JOHNSON, RG
    AMERICAN CERAMIC SOCIETY BULLETIN, 1976, 55 (04): : 418 - 419
  • [29] INTERFACIAL CRACK-PROPAGATION
    MULVILLE, DR
    VAISHNAV, RN
    JOURNAL OF ADHESION, 1975, 7 (03): : 215 - 233
  • [30] CRACK-PROPAGATION IN CERAMICS
    FREIMAN, SW
    MULVILLE, DR
    MAST, PW
    REPORT OF NRL PROGRESS, 1972, (FEB): : 36 - &