NEGATIVE EXCESS VOLUME OF MIXING IN POLYBUTADIENE POLYISOPRENE BLENDS

被引:11
|
作者
KAWAHARA, S [1 ]
SATO, K [1 ]
AKIYAMA, S [1 ]
机构
[1] TOKYO UNIV AGR & TECHNOL, FAC GEN EDUC,CHEM LAB,3-5-8 FUCHU SHI,SAIWAI CHO, FUCHU, TOKYO 183, JAPAN
关键词
MISCIBILITY; EXCESS VOLUME OF MIXING; POLYBUTADIENE; POLYISOPRENE; SOLID STATE PROTON NMR; STRUCTURE EFFECT ON MISCIBILITY;
D O I
10.1002/polb.1994.090320103
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The temperature dependence of specific volume was measured for miscible polybutadiene/polyisoprene blends by dilatometry. The negative excess volume of mixing below the lower critical solution temperature was studied in terms of the Flory equation-of-state. In order to achieve a best-fit of the calculated excess volume to the experimental excess volume, Flory's interaction parameter X12 was estimated to be negative for the blend. Thus, a stereo structural effect for mixing would be predicted, since only van der Waals dispersion forces are expected between blend components. Considering that one way to observe the stereo-structural effect is to study conformational changes during mixing, solid-state proton NMR measurements were conducted. Evidence of a conformational change was obtained for the blend. The occurrence of a structural effect was also suggested. (C) 1994 John Wiley & Sons, Inc.
引用
收藏
页码:15 / 20
页数:6
相关论文
共 50 条