RAPID-DETERMINATION OF DIVALENT TIN IN ALKALINE TIN-PLATING SOLUTION BY DIRECT POTENTIOMETRY

被引:0
|
作者
LEUNG, A [1 ]
CHEN, G [1 ]
HUANG, D [1 ]
机构
[1] S CHINA UNIV TECHNOL,ANALYT CHEM LAB,GUANGZHOU 510640,PEOPLES R CHINA
来源
PLATING AND SURFACE FINISHING | 1995年 / 82卷 / 06期
关键词
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
A novel method for determination of Sn(II) in alkaline tin plating solutions by potentiometry has been developed, Potassium ferricyanide is added to form an equilibrium of both Sn(OH)(6)(-2)/HSnO2- and Fe(CN)(6)(-3)/ Fe(CN)(6)(-4) in the solution, The quantity of Sn(II) in the solution is obtained by measuring the potential of Fe(CN)(6)(-3)/Fe(CN)(6)(-4), which is rapid, with a stable reading within three to six min, The potential difference becomes as great as 50 mV when the content of Sn(II) is 0.02 g/L and 0.20 g/L, respectively, The average success rate for the determination of Sn(II) in alkaline tin plating solutions by this method is 95.2 percent, with a relative standard deviation of 1.2 percent.
引用
收藏
页码:88 / 90
页数:3
相关论文
共 50 条
  • [31] Study of tin cementation in alkaline solution
    Liu, Y
    Piron, DL
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1998, 145 (01) : 186 - 190
  • [32] DETERMINATION OF THICKNESS OF TIN LAYER AND UNDERLAYER IN TIN PLATING OF COPPER AND STEEL BASES
    LUBYOVA, Z
    FELLNER, P
    SILNY, A
    MATIASOVSKY, K
    SURFACE TECHNOLOGY, 1977, 5 (06): : 479 - 485
  • [33] SPECTROPHOTOMETRIC DETERMINATION OF TIN IN PLATING BATH SOLUTIONS
    DZHURAEV, RR
    KARAMINOVA, GV
    VORONINA, IB
    KOTOV, AV
    JOURNAL OF ANALYTICAL CHEMISTRY OF THE USSR, 1991, 46 (11): : 1649 - 1650
  • [34] COLORIMETRIC DETERMINATION OF BISMUTH IN TIN PLATING BATHS
    PORYVAEV.GN
    INDUSTRIAL LABORATORY, 1970, 36 (09): : 1338 - &
  • [35] Study on the control system of vertical tin-plating process for semi-flexible coaxial cable
    Wang, Xu
    Yang, Lijun
    Sun, Guizheng
    Liu, Wei
    Cheng, Fangjie
    ADVANCED MATERIALS AND PROCESS TECHNOLOGY, PTS 1-3, 2012, 217-219 : 1336 - +
  • [36] Control of Pinhole Defects Formation in Semi-flexible Coaxial Cable by Vertical Tin-Plating Process
    程方杰
    肖鑫
    孙贵铮
    杨立军
    张凤玉
    Transactions of Tianjin University, 2011, 17 (05) : 320 - 323
  • [37] Rapid Oxidative Dissolution of Metallic Tin in Alkaline Solution Containing Iodate Ions
    Taninouchi, Yu-ki
    Uda, Tetsuya
    JOURNAL OF SUSTAINABLE METALLURGY, 2021, 7 (04) : 1762 - 1771
  • [38] Rapid Oxidative Dissolution of Metallic Tin in Alkaline Solution Containing Iodate Ions
    Yu-ki Taninouchi
    Tetsuya Uda
    Journal of Sustainable Metallurgy, 2021, 7 : 1762 - 1771
  • [39] RAPID-DETERMINATION OF ALKALINE-PHOSPHATASE REACTIVATION
    KLEYN, DH
    HO, CL
    JOURNAL OF THE ASSOCIATION OF OFFICIAL ANALYTICAL CHEMISTS, 1977, 60 (06): : 1389 - 1391
  • [40] Determination of tin and Nickel Content in Pyrophosphate Tin-nickel Alloy Plating Bath
    Geng Qiuju
    Wei Xue
    FUNDAMENTAL OF CHEMICAL ENGINEERING, PTS 1-3, 2011, 233-235 : 214 - +