DEFORMATION-MECHANISM MAP FOR TI-6 WT-PERCENT AL-ALLOY

被引:9
|
作者
JANGHORBAN, K
ESMAEILI, S
机构
[1] Department of Materials Science and Engineering, Shiraz University, Shiraz
关键词
D O I
10.1007/BF01124686
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A micro-computer program was developed to plot deformation mechanism maps for metals and substitutional solid solutions such as Ti-6 wt% Al. The package written in Turbo Basic is versatile and can be run to print out maps, using the related stored data files. In modelling the maps, the rate equations governing different deformation mechanisms were employed to find the dominant mechanisms and strain rate contours. In particular, the map for Ti-6 wt% Al was generated and it was found that the power law creep dominated over a wider range of stresses and temperatures than that of pure titanium. It is concluded that the strengthening effect of aluminium has shifted the iso-strain rate contours to higher stresses and temperatures.
引用
收藏
页码:3362 / 3365
页数:4
相关论文
共 50 条
  • [41] A DIFFERENTIAL SCANNING CALORIMETRIC INVESTIGATION OF PRECIPITATION KINETICS IN THE AL-1.53 WT-PERCENT CU-0.79 WT-PERCENT MG ALLOY
    JENA, AK
    GUPTA, AK
    CHATURVEDI, MC
    ACTA METALLURGICA, 1989, 37 (03): : 885 - 895
  • [42] Thermal effects of continuous laser treatment on Ti-6 Al(wt%)-4V(wt%) titanium alloy
    Velasquez, J. D. Puerta
    Lavisse, L.
    Kneip, J. C.
    Andrzejewski, H.
    Chevrier, P.
    Bolle, B.
    Tidu, A.
    Mattei, S.
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 7, PTS 1 AND 2, 2008, 595-598 : 1033 - 1038
  • [43] THE RELATIONSHIP BETWEEN DEFORMATION, CAVITATION, AND FRACTURE FOR SUPERPLASTIC FLOW IN AN AL-4 WT-PERCENT GE ALLOY
    KUZNETSOVA, RI
    ZHUKOV, NN
    POIDA, VP
    PHYSICS OF METALS, 1985, 5 (03): : 544 - 552
  • [44] DETECTION OF THE SPINODAL POINT IN AN AL-ZN 40 WT-PERCENT ALLOY
    ABIS, S
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1990, 9 (01) : 119 - 121
  • [45] AUTOCATALYTIC CONTINUOUS PRECIPITATION IN AN AL-8 WT-PERCENT MG ALLOY
    HAMANA, D
    NEBTI, S
    BOUTEFNOUCHET, A
    CHEKROUD, S
    ZEITSCHRIFT FUR METALLKUNDE, 1993, 84 (01): : 33 - 39
  • [46] PRE-PRECIPITATION IN AL-0.1 WT-PERCENT CR ALLOY
    GARG, NK
    SINGH, N
    RAMACHANDRAN, TR
    JOURNAL OF MATERIALS SCIENCE, 1978, 13 (05) : 1136 - 1138
  • [47] DISCONTINUOUS COARSENING OF LAMELLAR CELLULAR PRECIPITATE IN AN AUSTENITIC FE-30 WT-PERCENT NI-6 WT-PERCENT TI ALLOY .2. GROWTH-KINETICS
    FOURNELLE, RA
    ACTA METALLURGICA, 1979, 27 (07): : 1147 - 1155
  • [48] THE INFLUENCE OF STRAIN RATE ON THE FLOW-STRESS OF ZN-1.1 WT-PERCENT AL-ALLOY DEFORMED AT ROOM-TEMPERATURE
    LUKAC, P
    MALEK, P
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 1981, 63 (02): : K167 - K169
  • [49] INFLUENCE OF DEFORMATION ON THE BETA-]ALPHA+BETA-TRANSFORMATION KINETICS OF TI-6WT-PERCENT AL-4WT-PERCENT V ALLOY
    LOIER, C
    THAUVIN, G
    HAZOTTE, A
    SIMON, A
    JOURNAL OF THE LESS-COMMON METALS, 1985, 108 (02): : 295 - 312
  • [50] AN ELECTRON MICROSCOPY STUDY OF STRUCTURE OF QUENCHED TI-6 PERCENT MO ALLOY
    OKA, M
    TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS, 1967, 8 (04): : 215 - &