Tin Whiskers Formation on an Electronic Product: A Case Study

被引:2
|
作者
Asrar, Nausha [1 ]
Vancauwenberghe, Oliver [2 ]
Prangere, Sebastien [2 ]
机构
[1] Sugar Land Technol Ctr Schlumberger, Sugar Land, TX 77478 USA
[2] Schlumberger MEMS TC, F-78990 Elancourt, France
关键词
Tin whiskers; Thermal cycling; Intermetallics; Lead-freesolder;
D O I
10.1007/s11668-007-9028-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
During qualification testing, a printed circuit board (PCB) of an electronic device for a drilling tool failed. The circuit board was exposed to a 120 h aging cycle at 180 degrees C followed by 10 thermal cycles between -40 and 180 degrees C before a failure was noticed. During inspection numerous white whiskers were observed over a lead-free solder surface. Scanning electron microscopy (SEM) and energy-dispersive X-ray spectrometry (EDS) were used for microscopic examination and material characterization of the whiskers, end-cap metallization, and the solder materials. The tin whisker formation was attributed to the compressive stress in the tin solder material, which was caused by diffusion of the end cap metallization, formation of intermetallics, and thermal cycling of the soldered components. Recommendations are given to mitigate/control whisker formation on the lead-free solder materials.
引用
收藏
页码:179 / 182
页数:4
相关论文
共 50 条
  • [1] Study of morphologies for tin whiskers
    Hao, Hu
    Li, Guang-Dong
    Shi, Yao-Wu
    Xia, Zhi-Dong
    Lei, Yong-Ping
    Guo, Fu
    Li, Xiao-Yan
    Cailiao Kexue yu Gongyi/Material Science and Technology, 2010, 18 (01): : 111 - 115
  • [2] Microscopy Study of Tin Whiskers
    Champaign, Robert F.
    Ogden, Robert R.
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2010, 10 (06) : 444 - 449
  • [3] Formation and Growth of Tin Whiskers on Aluminum-Tin Alloys
    Murakami, Koji
    Hino, Makoto
    Mitooka, Yutaka
    Kanadani, Teruto
    MATERIALS TRANSACTIONS, 2012, 53 (01) : 209 - 216
  • [4] Modeling and Experimental Study of Tin Whiskers for 3D Electronic Packaging
    Wang Z.
    Zhang F.
    Shanghai Jiaotong Daxue Xuebao/Journal of Shanghai Jiaotong University, 2021, 55 (11): : 1445 - 1452
  • [5] The formation of whiskers on electroplated tin containing copper
    Moon, KW
    Williams, ME
    Johnson, CE
    Stafford, GR
    Handwerker, CA
    Boettinger, WJ
    PRICM 4: FORTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, VOLS I AND II, 2001, : 1115 - 1118
  • [6] INVESTIGATIONS OF FORMATION OF WHISKERS FROM VAPOUR DEPOSITED TIN
    POLITYCKI, A
    KEHRER, HP
    ZEITSCHRIFT FUR METALLKUNDE, 1969, 60 (01): : 17 - +
  • [7] TEM and SEM Analysis for Formation Mechanism of Tin Whiskers
    Kuwano, Noriyuki
    Horikami, Sadanori
    Maeda, Masanori
    Sosiati, Harini
    ADVANCEMENT OF MATERIALS AND NANOTECHNOLOGY II, 2012, 545 : 16 - +
  • [8] ON TIN WHISKERS
    FRANK, FC
    PHILOSOPHICAL MAGAZINE, 1953, 44 (355): : 854 - 860
  • [9] Study of the characteristics and growth of tin whiskers in orbit
    Ichimaru, Shinichiro
    Nakagawa, Tsuyoshi
    Nemoto, Norio
    Suganuma, Katsuaki
    Tatsumi, Hiroaki
    Nishikawa, Hiroshi
    MICROELECTRONICS RELIABILITY, 2024, 162
  • [10] Formation of tin whiskers and spheres on anodic aluminum oxide template
    Say, Wen C.
    Chen, Chien Chon
    Japanese Journal of Applied Physics, Part 1: Regular Papers and Short Notes and Review Papers, 2007, 46 (11): : 7577 - 7580