摘要
The effect of Li content (up to 4%), Cu content (up to 5%), and Mn content (up to 1.4%) on the hot cracking susceptibility of Al alloys containing Li was investigated. The usual tests, principally the measurement of crack length in ring castings, were used To evaluate the hot cracking susceptibility of the alloys. The values of linear shrinkage and elongation to failure in the brittle temperature range in the solid-liquid condition were compared. An increase in Li and Cu content ill the AI-Cu-Li system results in a decrease in the hot cracking susceptibility corresponding to a rise in the elongation to failure in the brittle range in the solid-liquid condition. The addition of Mn increases the hot cracking susceptibility associated with a decease in elongation to failure in this temperature range. (C) 1995 The Institute of Materials.
引用
收藏
页码:926 / 932
页数:7
相关论文
共 50 条
  • [1] Hot cracking susceptibility of Al-Cu-Li and Al-Cu-Li-Mn alloys
    Department of Physical Metallurgy of Non-Ferrous Metals, Moscow Steel and Alloys Instltute, Moscow, Russia
    不详
    Mater. Sci. Technol., 9 (926-932):
  • [2] Hydrogen trapping and embrittlement susceptibility in Al-Cu-Li alloys
    Wang, Xiaoya
    Li, Guoai
    He, Qiyao
    Xiao, Enhui
    Jiang, Jiantang
    Shao, Wenzhu
    Zhen, Liang
    CORROSION SCIENCE, 2024, 226
  • [3] Hydrogen trapping and embrittlement susceptibility in Al-Cu-Li alloys
    Wang, Xiaoya
    Li, Guoai
    He, Qiyao
    Xiao, Enhui
    Jiang, Jiantang
    Shao, Wenzhu
    Zhen, Liang
    Corrosion Science, 2024, 226
  • [4] Weldability of commercial Al-Cu-Li alloys
    Lippold, JC
    Lin, W
    ALUMINIUM ALLOYS: THEIR PHYSICAL AND MECHANICAL PROPERTIES, PTS 1-3, 1996, 217 : 1685 - 1690
  • [5] Hot cracking behaviour of an autogenously laser welded Al-Cu-Li alloy
    Enz, J.
    Carrarin, C.
    Riekehr, S.
    Ventzke, V.
    Kashaev, N.
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2018, 95 (1-4): : 299 - 310
  • [6] Hot cracking behaviour of an autogenously laser welded Al-Cu-Li alloy
    J. Enz
    C. Carrarin
    S. Riekehr
    V. Ventzke
    N. Kashaev
    The International Journal of Advanced Manufacturing Technology, 2018, 95 : 299 - 310
  • [7] Quantitative Phase Analysis of Al-Mg-Li and Al-Cu-Li Alloys
    Betsofen, Sergey
    Chizhikov, Mihail
    ALUMINIUM ALLOYS 2014 - ICAA14, 2014, 794-796 : 915 - 920
  • [8] Dynamic microstructural evolution of Al-Cu-Li alloys during hot deformation
    Tang, Ya
    Xiao, Daihong
    Huang, Lanping
    You, Renxuan
    Zhao, Xinyue
    Lin, Nan
    Ma, Yunzhu
    Liu, Wensheng
    MATERIALS CHARACTERIZATION, 2022, 191
  • [9] Dynamic microstructural evolution of Al-Cu-Li alloys during hot deformation
    Tang, Ya
    Xiao, Daihong
    Huang, Lanping
    You, Renxuan
    Zhao, Xinyue
    Lin, Nan
    Ma, Yunzhu
    Liu, Wensheng
    MATERIALS CHARACTERIZATION, 2022, 191
  • [10] EFFECT OF MICROSTRUCTURE ON THE FATIGUE CRACK-PROPAGATION BEHAVIOR OF AL-LI-MN AND AL-CU-LI ALLOYS
    COYNE, EJ
    STARKE, EA
    JOURNAL OF METALS, 1979, 31 (12): : 69 - 69