Mechanochemical synthesis and sintering behaviour of magnesium aluminate spinel

被引:0
|
作者
K. J. D. Mackenzie
J. Temuujin
Ts. Jadambaa
M. E. Smith
P. Angerer
机构
[1] University of Oxford,Department of Materials
[2] Mongolian Academy of Sciences,Institute of Chemistry and Chemical Technology
[3] Mongolian Technical University,Department of Chemical Technology
[4] University of Warwick,Department of Physics
[5] Institute of Materials,German Aerospace Center
来源
关键词
Gibbsite; MgAl2O4; Hydrotalcite; Brucite; Magnesium Aluminate;
D O I
暂无
中图分类号
学科分类号
摘要
X-ray amorphous precursor phases for the synthesis of spinel (MgAl2O4) have been prepared by grinding mixtures of gibbsite (Al(OH)3) with brucite (Mg(OH)2) or hydromagnesite (4MgCO3·Mg(OH)2·4H2O). The mechanochemical treatment does not remove any water or carbonate, but converts some of the gibbsite octahedral Al sites into tetrahedral sites and other sites with a 27Al MAS NMR resonance at about 38 ppm. The brucite-derived precursor forms spinel on heating at ≤850°C, by contrast with unground mixtures which show little spinel formation even at 1250°C. The hydromagnesite-derived precursor transforms at about 850°C into a mixture of spinel and hydrotalcite (Mg6Al2(OH)16CO3·4H2O), the latter decomposing to spinel and MgO by 1050°C. Spinel derived from the hydromagnesite-containing precursor shows superior pressureless sintering properties at 1400–1600°C, producing a body of 97% theoretical bulk density at 1600°C. Under the same conditions, the brucite-derived spinel sintered to 72% theoretical density and showed a morphology consisting of widely disparate grain sizes.
引用
收藏
页码:5529 / 5535
页数:6
相关论文
共 50 条
  • [1] Mechanochemical synthesis and sintering behaviour of magnesium aluminate spinel
    Mackenzie, KJD
    Temuujin, J
    Jadambaa, T
    Smith, ME
    Angerer, P
    JOURNAL OF MATERIALS SCIENCE, 2000, 35 (22) : 5529 - 5535
  • [2] Mechanochemical synthesis of magnesium aluminate spinel powder at room temperature
    Domanski, D
    Urretavizcaya, G
    Castro, FJ
    Gennari, FC
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2004, 87 (11) : 2020 - 2024
  • [3] Mechanochemical synthesis of magnesium aluminate spinel in oxide-hydroxide systems
    Plesingerová, B
    Stevulová, N
    Luxová, M
    Boldizárová, E
    JOURNAL OF MATERIALS SYNTHESIS AND PROCESSING, 2000, 8 (5-6) : 287 - 293
  • [4] A new sintering aid for magnesium aluminate spinel
    Ganesh, I
    Bhattacharjee, S
    Saha, BP
    Johnson, R
    Mahajan, YR
    CERAMICS INTERNATIONAL, 2001, 27 (07) : 773 - 779
  • [5] Sintering and grain growth behaviour of magnesium aluminate spinel: Effect of lithium hydroxide addition
    Talimian, Ali
    El-Maghraby, H. F.
    Michalkova, Monika
    Galusek, Dusan
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2021, 41 (11) : 5634 - 5643
  • [6] Reaction sintering of alumina rich magnesium aluminate spinel
    Ghosh, A
    Sarkar, R
    SILICATES INDUSTRIELS, 2003, 68 (9-10): : 125 - 128
  • [7] Synthesis and Sintering Behavior of Ultrafine (<10 nm) Magnesium Aluminate Spinel Nanoparticles
    Rufner, Jorgen
    Anderson, David
    van Benthem, Klaus
    Castro, Ricardo H. R.
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2013, 96 (07) : 2077 - 2085
  • [8] Reaction sintering of alumina-rich magnesium aluminate spinel
    Ghosh, A
    Sarkar, R
    AMERICAN CERAMIC SOCIETY BULLETIN, 2003, 82 (12): : 9501 - 9506
  • [9] Deterioration in the final-stage sintering of magnesium aluminate spinel
    Ting, CJ
    Lu, HY
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2000, 83 (07) : 1592 - 1598
  • [10] Defect reactions and the controlling mechanism in the sintering of magnesium aluminate spinel
    Ting, CJ
    Lu, HY
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1999, 82 (04) : 841 - 848