Medium-temperature pressure leaching of copper concentrates — Part IV: Application at Morenci, Arizona

被引:0
|
作者
J. O. Marsden
J. C. Wilmot
R. J. Smith
机构
[1] Freeport-McMoRan Copper & Gold Inc.,
[2] Concentrate Leach Plant,undefined
[3] Freeport-McMoRan Copper & Gold Inc.,undefined
来源
关键词
Copper; Pressure leaching;
D O I
暂无
中图分类号
学科分类号
摘要
Parts I and II in this series of papers presented the chemistry of medium-temperature pressure leaching of copper sulfide concentrates and reviewed the metallurgical development of a process to effectively recover copper using medium-temperature pressure leaching and direct electrowinning (DEW). Part III reviewed the large-scale demonstration of the MT-DEW-SX process at Bagdad, Arizona. Key features of the process were the use of superfine grinding of the concentrate (to a P98 of 12 to 15 µm and a P80 of 6 to 7 µm), pressure leaching at 160°C with 1,380 kPa (200 psig) oxygen overpressure, DEW to produce LME Grade A cathode, recycling some of the lean electrolyte to the pressure leaching step, and treatment of a lean electrolyte bleed by solution extraction (SX). Recycling of lean electrolyte provided all of the acid required to effectively dissolve copper and convert approximately 65% to 70% of the sulfide sulfur to elemental sulfur, resulting in an acid-autogenous process for pressure leaching. This paper (Part IV) discusses the development and design of a full-scale commercial application for the Morenci operation in Arizona.
引用
收藏
页码:226 / 236
页数:10
相关论文
共 50 条