Effect of the chemical structure of aromatic polyimides on their thermal aging, relaxation behavior and mechanical properties

被引:1
|
作者
Giuseppe Ragosta
Mario Abbate
Pellegrino Musto
Gennaro Scarinzi
机构
[1] National Research Council of Italy,Institute of Chemistry and Technology of Polymers
来源
关键词
Polyimide; Aging Time; Thermal Aging; Relaxation Property; Aromatic Polyimide;
D O I
暂无
中图分类号
学科分类号
摘要
This article examines the effects of structural changes and thermal aging treatments on the relaxation processes and mechanical properties of three polyimides differing for their molecular structure i.e. PMDA-ODA, 6FDA-ODA, and 6FDA-6FpDA. These polyimides were obtained by thermal imidization of their polyamic acid precursors, which were synthesized from the respective dianhydrides [pyromellitic anhydride (PMDA), hexahydrofluoroisopropylidene diphthalic anhydride (6FDA)], and diamines [4,4′-diaminodiphenyl ether (ODA), 4,4′-(hexafluoroisopropylidene) dianiline (6FpDA)]. After the curing process, the polyimides were thermally aged at a fixed temperature for various times Dynamic mechanical measurements performed in a multi-frequency mode, were used to determine the glass-rubber and sub-glass transitions, as well as the activation energy of the β transition. It was found that the Tg decreased in the order PMDA-ODA > 6FDA-6FpDA > 6FDA-ODA as a result of an increased chain rigidity and molecular packing induced by charge transfer interactions during the thermal imidization process. The β sub-glass transition showed two relaxation processes identified as β′ and β′′. The β′ process was attributed to the local motion of the diamine constituents while the β′′ process was caused by the local motion of the dianhydride moiety. The cooperativity of these molecular motions was also assessed via the Starkweather method. The thermal aging enhanced the state of aggregation of polyimide chains and thus the Tg and the sub-glass transition properties. This effect was particularly marked for the PMDA-ODA polyimide. Also the mechanical properties were significantly affected by chemical structure and aging treatments. For non-aged samples the more influenced parameter was the elongation at break, which decreased in the order PMDA-ODA > 6FDA-ODA > 6FDA-6FpDA. The aging enhanced the elastic modulus and the tensile strength and reduced the elongation at break.
引用
收藏
页码:2637 / 2647
页数:10
相关论文
共 50 条
  • [1] Effect of the chemical structure of aromatic polyimides on their thermal aging, relaxation behavior and mechanical properties
    Ragosta, Giuseppe
    Abbate, Mario
    Musto, Pellegrino
    Scarinzi, Gennaro
    JOURNAL OF MATERIALS SCIENCE, 2012, 47 (06) : 2637 - 2647
  • [2] RELAXATION MECHANICAL-PROPERTIES OF AROMATIC POLYIMIDES OF VARIOUS STRUCTURE
    BESSONOV, MI
    KUZNETSO.NP
    ADROVA, NA
    FLORINSK.FS
    VYSOKOMOLEKULYARNYE SOEDINENIYA SERIYA A, 1974, 16 (09): : 2093 - 2100
  • [3] MECHANISM OF THERMAL DEGRADATION OF AROMATIC POLYIMIDES OF VARIES CHEMICAL STRUCTURE
    KRASNOV, EP
    AKSENOVA, VP
    KHARKOV, SN
    BARANOVA, SA
    VYSOKOMOLEKULYARNYE SOEDINENIYA SECTION A, 1970, 12 (04): : 873 - &
  • [4] INFLUENCE OF CHEMICAL-STRUCTURE OF AROMATIC POLYIMIDES (POLYARIMIDES) ON THEIR PROPERTIES
    ADROVA, NA
    ZHUKOVA, TI
    KOTON, MM
    LAIUS, LA
    SAZANOV, YN
    FLORINSKII, FS
    JOURNAL OF APPLIED CHEMISTRY OF THE USSR, 1974, 47 (08): : 1847 - 1849
  • [5] ABOUT STRUCTURE AND BEHAVIOR OF AROMATIC POLYIMIDES
    VINOGRADOVA, SV
    SLONIMSKII, GL
    VYGODSKII, YS
    ASKADSKI.AA
    MZHELSKI.AI
    CHUROCHK.NA
    KORSHAK, VV
    VYSOKOMOLEKULYARNYE SOEDINENIYA SECTION A, 1969, 11 (12): : 2725 - +
  • [6] Effect of the chemical structure of aromatic-cycloaliphatic copolyimide films on their surface morphology, relaxation behavior and dielectric properties
    Chisca, Stefan
    Musteata, Valentina Elena
    Stoica, Iuliana
    Sava, Ion
    Bruma, Maria
    JOURNAL OF POLYMER RESEARCH, 2013, 20 (03)
  • [7] Effect of the chemical structure of aromatic-cycloaliphatic copolyimide films on their surface morphology, relaxation behavior and dielectric properties
    Stefan Chisca
    Valentina Elena Musteata
    Iuliana Stoica
    Ion Sava
    Maria Bruma
    Journal of Polymer Research, 2013, 20
  • [9] INFLUENCE OF CHEMICAL-STRUCTURE ON PROPERTIES OF AROMATIC POLYIMIDES OBTAINED BY THE CHEMICAL CYCLIZATION METHOD
    LIKHACHEV, DY
    ARZHAKOV, MS
    CHVALUN, SN
    SINEVICH, YA
    ZUBOV, YA
    KARDASH, IY
    PRAVEDNIKOV, AN
    VYSOKOMOLEKULYARNYE SOEDINENIYA SERIYA B, 1985, 27 (10): : 723 - 728
  • [10] The structure and properties of aromatic polyimides - Comment
    Vygodskii, YS
    VYSOKOMOLEKULYARNYE SOEDINENIYA SERIYA A & SERIYA B, 1999, 41 (12): : 2047 - 2047