An experimental investigation of the velocity of sound in molten lead and bismuth and in their reciprocal eutectic alloy at high temperatures

被引:0
|
作者
P. S. Popel’
D. A. Yagodin
A. G. Mozgovoi
M. A. Pokrasin
机构
[1] Ural State Pedagogical University,Joint Institute for High Temperatures
[2] Russian Academy of Sciences,Baikov Institute of Metallurgy and Materials Studies
[3] Russian Academy of Sciences,undefined
来源
High Temperature | 2010年 / 48卷
关键词
Bismuth; Sound Velocity; Confidence Error; Liquid Lead; Lead Bismuth Eutectic;
D O I
暂无
中图分类号
学科分类号
摘要
The pulse-phase method is used for measuring the velocity of sound in liquid lead and bismuth and in lead-bismuth eutectic in the range from the melting temperature to 1380 K. The purity of investigated metals is 9.99% by mass or better. The confidence error of experimental results does not exceed 0.3%. The experimental data are compared with those available from the literature.
引用
收藏
页码:181 / 187
页数:6
相关论文
共 50 条
  • [1] An experimental investigation of the velocity of sound in molten lead and bismuth and in their reciprocal eutectic alloy at high temperatures
    Popel', P. S.
    Yagodin, D. A.
    Mozgovoi, A. G.
    Pokrasin, M. A.
    HIGH TEMPERATURE, 2010, 48 (02) : 181 - 187
  • [2] Experimental Investigation of the Density of Molten Lead–Bismuth Eutectic
    B. B. Alchagirov
    T. M. Shamparov
    A. G. Mozgovoi
    High Temperature, 2003, 41 : 210 - 215
  • [3] Experimental investigation of the density of molten lead-bismuth eutectic
    Alchagirov, BB
    Shamparov, TM
    Mozgovoi, AG
    HIGH TEMPERATURE, 2003, 41 (02) : 210 - 215
  • [4] Experimental investigation on the characteristics of molten lead–bismuth non-eutectic alloy fragmentation in water
    Shao-Jie Tan
    Yu-Bao Zhong
    Hui Cheng
    Song-Bai Cheng
    Nuclear Science and Techniques, 2022, 33
  • [5] Experimental investigation on the characteristics of molten lead–bismuth non-eutectic alloy fragmentation in water
    Shao-Jie Tan
    Yu-Bao Zhong
    Hui Cheng
    Song-Bai Cheng
    NuclearScienceandTechniques, 2022, 33 (09) : 61 - 81
  • [6] Experimental investigation on the characteristics of molten lead-bismuth non-eutectic alloy fragmentation in water
    Tan, Shao-Jie
    Zhong, Yu-Bao
    Cheng, Hui
    Cheng, Song-Bai
    NUCLEAR SCIENCE AND TECHNIQUES, 2022, 33 (09)
  • [7] The solubility of helium and argon in liquid lead, bismuth, and their eutectic alloy at high temperatures
    Shpil'rain, E. E.
    Skovorod'ko, S. N.
    Mozgovoi, A. G.
    HIGH TEMPERATURE, 2007, 45 (01) : 127 - 130
  • [8] The solubility of helium and argon in liquid lead, bismuth, and their eutectic alloy at high temperatures
    E. E. Shpil’rain
    S. N. Skovorod’ko
    A. G. Mozgovoi
    High Temperature, 2007, 45 : 127 - 130
  • [9] Systematic experimental investigation on the characteristics of molten lead-bismuth eutectic fragmentation in water
    Cheng, Hui
    Chen, Xiaolin
    Ye, Yiji
    Cheng, Songbai
    NUCLEAR ENGINEERING AND DESIGN, 2021, 371
  • [10] FeCrMoWCBY metallic glass with high corrosion resistance in molten lead-bismuth eutectic alloy
    Wei, X. S.
    Jin, J. L.
    Jiang, Z. Z.
    Liang, D. D.
    Shen, J.
    CORROSION SCIENCE, 2021, 190