Mechanisms of cast structure and stressed state formation in Hadfield steel

被引:0
|
作者
Dmitri Gorlenko
Konstantin Vdovin
Nikolay Feoktistov
机构
[1] Nosov Magnitogorsk State Technical University,
来源
China Foundry | 2016年 / 13卷
关键词
Hadfield steel; crystallization; austenite; excessive phase; stress; TG142.33; A;
D O I
暂无
中图分类号
学科分类号
摘要
The paper describes the investigation of mechanisms of cast structure formation in Hadfield steel depending on the changes in the cooling rate of a casting in the following two temperature ranges: crystallization temperature (1,200-1,390 °С) and the temperature of excessive phase separation (560-790 °С). Changes in the cooling rate of the crystallization temperature range from 1.1 to 25.0 °С•s-1 result in the reduction of the average size of austenite grains from 266 to 131 μm. At the same time, the magnitude of developing shrinkage stresses changes from +195 to 0 MPa. When the cooling rate is higher than 16 °С•s-1, no shrinkage stresses are formed in the casting. Changes in the cooling rate of the casting in the temperature range of the excessive phase separation influence the number of phases, their morphology and chemical composition, the values of phase stresses, and the possibility of martensitic transformation. Changing in the cooling rate from 0.24 to 5.46 °С•s-1 results in the decrease of the amount of the excessive phase from 14.8% to 2.1%, which is composed of eutectic and carbides depending on the cooling rate, their quantitative ratio and morphology change. Such changes in the microstructure are reflected on the changes of value of developing phase stresses. When the cooling rate is 0.24 °С•s-1, it is +100 MPa, while the increase of the cooling rate to 1.4 °С•s-1 results in the decrease of tensile stresses to 0 MPa and their qualitative stresses change to compressive ones. Further increase of the cooling rate results in the increase of the value of compressive stresses. When the cooling rate is 5.5 °С•s-1, their value reaches -92 MPa. Martensite forming in the structure of Hadfield steel is possible if the cooling rate of the casting in the range of excessive phase separation is less than 0.25 °С•s-1.
引用
收藏
页码:433 / 442
页数:9
相关论文
共 50 条
  • [1] Mechanisms of cast structure and stressed state formation in Hadfield steel
    Gorlenko, Dmitri
    Vdovin, Konstantin
    Feoktistov, Nikolay
    CHINA FOUNDRY, 2016, 13 (06) : 433 - 442
  • [2] Mechanisms of cast structure and stressed state formation in Hadfield steel
    Dmitri Gorlenko
    Konstantin Vdovin
    Nikolay Feoktistov
    China Foundry, 2016, 13 (06) : 433 - 442
  • [3] MECHANISMS OF INFLUENCE OF PHOSPHORUS ON MECHANICAL-PROPERTIES OF CAST HADFIELD STEEL
    SULIK, D
    KAMARAS, L
    KOVOVE MATERIALY-METALLIC MATERIALS, 1990, 28 (06): : 717 - 726
  • [4] Structure formation and properties of NbC-Hadfield steel cermets
    Ya. A. Kryl’
    P. M. Prysyazhnyuk
    Journal of Superhard Materials, 2013, 35 : 292 - 297
  • [5] Structure formation and properties of NbC-Hadfield steel cermets
    Kryl, Ya. A.
    Prysyazhnyuk, P. M.
    JOURNAL OF SUPERHARD MATERIALS, 2013, 35 (05) : 292 - 297
  • [6] Comparison of Abrasive Wear Resistance of Hardox Steel and Hadfield Cast Steel
    Zemlik, Martyna
    Konat, Lukasz
    Lesny, Kacper
    Jamroziak, Krzysztof
    APPLIED SCIENCES-BASEL, 2024, 14 (23):
  • [7] THE FINE-STRUCTURE OF HADFIELD STEEL
    GULYAEV, AA
    TYAPKIN, YD
    GOLIKOV, VA
    ZHARINOVA, VS
    METAL SCIENCE AND HEAT TREATMENT, 1985, 27 (5-6) : 411 - 415
  • [9] FINE STRUCTURE OF HADFIELD STEEL.
    Gulyaev, A.A.
    Tyapkin, Yu.D.
    Golikov, V.A.
    Zharinova, V.S.
    Metal Science and Heat Treatment (English Translation of Metallovedenie i Termicheskaya Obrabotka Metallov), 1985, 27 (5-6): : 411 - 415
  • [10] MACHINING HADFIELD CAST STEEL HEATED BY ELECTRIC-ARC
    GRZESIK, T
    MECHANIK MIESIECZNIK NAUKOWO-TECHNICZNY, 1984, 57 (07): : 355 - 357