Effect of CrxCy–NiCr coating on the hydrogen embrittlement of 17-4 PH stainless steel using the smooth bar tensile test

被引:1
|
作者
Sicong Shen
Xiaolong Song
Qizhen Li
Xinfeng Li
Ruihua Zhu
Gongxian Yang
机构
[1] Xi’an Jiaotong University,State Key Laboratory for Mechanical Behavior of Materials
[2] Washington State University,School of Mechanical and Materials Engineering
[3] Dongfang Turbine Co.,State Key Laboratory for Long
[4] Ltd.,Life High Temperature Materials
来源
关键词
D O I
暂无
中图分类号
学科分类号
摘要
A CrxCy–NiCr cermet coating was fabricated using the supersonic plasma spray technique, and its effect on the hydrogen embrittlement of 17-4 PH stainless steel was studied through electrochemical hydrogen charging and slow strain rate tensile testing. The index of hydrogen embrittlement susceptibility was calculated, and the results show that the CrxCy–NiCr coating plays a significant role in preventing hydrogen embrittlement cracking. The hydrogen content analysis demonstrates that the CrxCy–NiCr coating enhances the resistance to hydrogen embrittlement by acting as a hydrogen diffusion barrier. This effect is mainly due to the CrxCy ceramics in the cermet coating having a very low hydrogen diffusion rate. In addition, the strength and ductility of the specimen without the coating decrease gradually with increasing hydrogen charging current density. According to the tensile testing results and the fracture surface analysis, the hydrogen embrittlement phenomenon is explained by a mixed mechanism involving hydrogen-enhanced local plasticity and hydrogen-enhanced decohesion.
引用
收藏
页码:7356 / 7368
页数:12
相关论文
共 50 条
  • [1] Effect of CrxCy-NiCr coating on the hydrogen embrittlement of 17-4 PH stainless steel using the smooth bar tensile test
    Shen, Sicong
    Song, Xiaolong
    Li, Qizhen
    Li, Xinfeng
    Zhu, Ruihua
    Yang, Gongxian
    JOURNAL OF MATERIALS SCIENCE, 2019, 54 (09) : 7356 - 7368
  • [2] Effect of solution-treated temperature on hydrogen embrittlement of 17-4 PH stainless steel
    Shen, Sicong
    Li, Xinfeng
    Zhang, Peng
    Nan, Yanli
    Yang, Gongxian
    Song, Xiaolong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 703 : 413 - 421
  • [3] Hydrogen embrittlement induced fracture of 17-4 PH stainless steel valve stem
    Jiang, Tao
    Zhong, Jiru
    Zhang, Xiaocheng
    Wang, Wulin
    Guan, Kaishu
    ENGINEERING FAILURE ANALYSIS, 2020, 113
  • [4] The role of delta ferrite in hydrogen embrittlement fracture of 17-4 PH stainless steel
    Fan, Y. H.
    Zhao, H. L.
    Weng, K. R.
    Ma, C.
    Yang, H. X.
    Dong, X. L.
    Guo, C. W.
    Li, Y. G.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2022, 47 (79) : 33883 - 33890
  • [5] Hydrogen susceptibility of 17-4 PH stainless steel
    Chiang, WC
    Pu, CC
    Yu, BL
    Wu, JK
    MATERIALS LETTERS, 2003, 57 (16-17) : 2485 - 2488
  • [6] The effect of low hydrogen content on hydrogen embrittlement of additively manufactured 17-4 stainless steel
    Ben-Hamu, Guy
    Metalnikov, Polina
    Eliezer, Dan
    PROGRESS IN ADDITIVE MANUFACTURING, 2024, 9 (05) : 1319 - 1330
  • [7] Onto the role of copper precipitates and reverted austenite on hydrogen embrittlement in 17-4 PH stainless steel
    Schutz, P.
    Latu-Romain, L.
    Martin, F.
    Auzoux, Q.
    Adem, J.
    Wouters, Y.
    Ravat, B.
    Menut, D.
    MATERIALS CHARACTERIZATION, 2023, 202
  • [8] Embrittlement of laser surface-annealed 17-4 PH stainless steel
    Tsay, LW
    Yang, TY
    Young, MC
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 311 (1-2): : 64 - 73
  • [9] A comparative study of microstructure and hydrogen embrittlement of selective laser melted and wrought 17-4 PH stainless steel
    Alnajjar, Michella
    Christien, Frederic
    Bosch, Cedric
    Wolski, Krzysztof
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 785
  • [10] ENVIRONMENTAL EMBRITTLEMENT OF 17-4 PH MARTENSITIC STAINLESS-STEEL AND ITS PREVENTION
    OZAKI, T
    ISHIKAWA, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1989, 75 (04): : 673 - 680