Fatigue and fracture properties of thin metallic foils

被引:0
|
作者
A. Hadrboletz
B. Weiss
G. Khatibi
机构
[1] University of Vienna,Institute of Materialphysics
来源
International Journal of Fracture | 2001年 / 107卷
关键词
Dislocation structure; fatigue crack growth; fatigue threshold metallic foils; fracture topography; size effect special; fatigue testing device.;
D O I
暂无
中图分类号
学科分类号
摘要
Metallic thin foils are essential structural parts in microsystems,which may be subjected to fatigue loading caused by thermal fluctuations and mechanical vibrations influencing their reliability in numerous engineering applications. It is well known that the fatigue properties of bulk material cannot be adopted for small scaled structures. For a better understanding of the `size-effect' in the present investigation fatigue crack growth near threshold in the high cycle fatigue regime and associated fracture processes were studied. Free- standing rolled and electrodeposited Cu-, Mo- and Al foils of thickness from 20 μm to 250 μm in different conditions have been tested in a special experimental set up operating at R=−1 and a testing frequency of 20 kHz. At a given constant strain value the fatigue crack growth behaviour has been recorded accompanied by intermittent observation of the change of the dislocation structure in the vicinity of the growing crack by use of the electron channeling contrast imaging (ECCI)-technique in a scanning electron microscope (SEM). In a load shedding technique fatigue threshold stress intensity factor values have been derived and compared with data of bulk material. Typical crack growth features were detected depending on thickness and grain sizes of the foils. Various criteria (compliance, extent of plastic zones and plastic strain gradients) were selected for the explanation of this anomalous behaviour. Additionally fractomicrographs of uniaxial strained and fatigued foils have been studied to obtain further insight of the effect of dimensional constraint.
引用
收藏
页码:307 / 327
页数:20
相关论文
共 50 条
  • [1] Fatigue and fracture properties of thin metallic foils
    Hadrboletz, A
    Weiss, B
    Khatibi, G
    INTERNATIONAL JOURNAL OF FRACTURE, 2001, 107 (04) : 307 - 327
  • [2] Fatigue and fracture properties of thin metallic foils
    Hadrboletz, A
    Weiss, B
    Khatibi, G
    INTERNATIONAL JOURNAL OF FRACTURE, 2001, 109 (01) : 69 - 89
  • [3] Fatigue and fracture properties of thin metallic foils
    A. Hadrboletz
    B. Weiss
    G. Khatibi
    International Journal of Fracture, 2001, 109 : 69 - 89
  • [4] The ⟫size effect⟪ on the fatigue -: and fracture properties of thin metallic foils and wires
    Hadrboletz, A
    Weiss, B
    Khatibi, G
    MICRO MATERIALS, PROCEEDINGS, 2000, : 558 - 559
  • [5] The 'size effect' on the stress-strain, fatigue and fracture properties of thin metallic foils
    Klein, M
    Hadrboletz, A
    Weiss, B
    Khatibi, G
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 319 : 924 - 928
  • [6] Fatigue threshold behavior of thin metallic foils
    Hadrboletz, A
    Kathibi, G
    Weiss, B
    Stickler, R
    ECF 12: FRACTURE FROM DEFECTS, VOLS. I-III, 1998, : 247 - 252
  • [7] Fatigue crack growth behaviour of thin metallic foils
    Hadrboletz, A
    Kathibi, G
    Weiss, B
    Stickler, R
    FATIGUE '99: PROCEEDINGS OF THE SEVENTH INTERNATIONAL FATIGUE CONGRESS, VOLS 1-4, 1999, : 1865 - 1870
  • [8] Fatigue Properties and Morphology of Fatigue Fracture of Bulk Metallic Glass
    Zhao, X. Y.
    Chen, Z. H.
    Wang, H. P.
    Zhan, J.
    METAL SCIENCE AND HEAT TREATMENT, 2016, 58 (7-8) : 487 - 492
  • [9] Fatigue Properties and Morphology of Fatigue Fracture of Bulk Metallic Glass
    X. Y. Zhao
    Z. H. Chen
    H. P. Wang
    J. Zhan
    Metal Science and Heat Treatment, 2016, 58 : 487 - 492
  • [10] Fatigue properties of titanium alloy thin foils for MEMS applications
    Zhang, Bin
    Lei, Li-Ming
    Yang, Jia
    Guo, Xin-Hu
    Zhang, Guang-Ping
    MATERIALS LETTERS, 2012, 89 : 302 - 304