Evaluation of the Residual Strength of a Polyester/E-Glass Composite Tray After Exposure to High Temperatures Due to a Nearby Fire Event

被引:0
|
作者
B. J. Lopes
G. A. S. da Silva
J. R. M. d’Almeida
机构
[1] Pontifícia Universidade Católica do Rio de Janeiro,Chemical and Materials Engineering Department
来源
Fire Technology | 2018年 / 54卷
关键词
Polyester/; -Glass composite; Mechanical properties; Thermal degradation; Non-destructive test;
D O I
暂无
中图分类号
学科分类号
摘要
The mechanical behavior of pultruded polyester/E-Glass trays was evaluated as a function of high temperature exposure time at 250°C. This temperature was chosen based on the composite’s thermal behavior, which was determined by thermogravimetric analysis and differential scanning calorimetry. The mechanical behavior of the composite was determined before and after exposure to high temperature by using a three-point bending test and a non-destructive sonic test. The average value of the fracture load increased in the first 90 min of exposure to temperature, and only after longer exposure times, upwards of 120 min, the failure load decreased. This behavior was attributed to a post-curing effect on the composite’s polymeric matrix. However, toughness sharply decreased as a consequence of the exposure to temperature, and large amounts of smoke were generated, even after exposures as short as 30 min. The value of the damping ratio evaluated by the sonic test, decreased during the first 60 min of exposure and then increased, showing a possible competition between post-curing and thermal degradation as a function of exposure time. From a macroscopic point of view, it can be observed that the failure of fiber/matrix interfaces may be the main damage mechanism.
引用
收藏
页码:853 / 865
页数:12
相关论文
共 49 条
  • [1] Evaluation of the Residual Strength of a Polyester/E-Glass Composite Tray After Exposure to High Temperatures Due to a Nearby Fire Event
    Lopes, B. J.
    da Silva, G. A. S.
    d'Almeida, J. R. M.
    FIRE TECHNOLOGY, 2018, 54 (04) : 853 - 865
  • [2] Plane behavior of an E-glass/polyester composite at high strain rates
    Kammerer, C
    Neme, A
    COMPOSITES SCIENCE AND TECHNOLOGY, 1998, 58 (05) : 717 - 725
  • [3] Post-fire fatigue performance of E-glass/polyester CSM composite laminates
    Staedtke, H.
    Prusty, B. G.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2007, 30 (08) : 723 - 733
  • [4] Residual Strength for Concrete after Exposure to High Temperatures
    Li Xiaoyong
    Bu Fanjie
    INNOVATIVE COMPUTING AND INFORMATION, PT II, 2011, 232 : 382 - 390
  • [5] STRENGTH LOSS IN E-GLASS FIBERS AFTER EXPOSURE TO ORGANIC-ACIDS
    JONES, RL
    CHANDLER, HD
    JOURNAL OF MATERIALS SCIENCE, 1985, 20 (09) : 3325 - 3328
  • [6] Understanding physical changes and strength loss of E-glass fibres following exposure to elevated temperatures
    Jenkins, P. G.
    MATERIALS SCIENCE AND TECHNOLOGY, 2017, 33 (03) : 255 - 264
  • [7] STRENGTH LOSS IN E-GLASS FIBERS AFTER EXPOSURE TO HYDROCHLORIC, HYDROBROMIC AND HYDRIODIC ACIDS
    JONES, RL
    CHANDLER, HD
    JOURNAL OF MATERIALS SCIENCE, 1985, 20 (09) : 3320 - 3324
  • [8] Residual mechanical properties of high strength steels after exposure to fire
    Li, Hai-Ting
    Young, Ben
    JOURNAL OF CONSTRUCTIONAL STEEL RESEARCH, 2018, 148 : 562 - 571
  • [9] Numerical and Experimental Studies of High Strain Rate Mechanical Behavior of E-Glass/Polyester Composite Laminates
    Tunusoglu, Gozde
    Tasdemirci, Alper
    Guden, Mustafa
    Hall, I. W.
    PROCEEDINGS OF THE ASME 10TH BIENNIAL CONFERENCE ON ENGINEERING SYSTEMS DESIGN AND ANALYSIS, 2010, VOL 2, 2010, : 61 - 68
  • [10] The strength of glass fibre reinforcement after exposure to elevated composite processing temperatures
    Thomason, J. L.
    Kao, C. C.
    Ure, J.
    Yang, L.
    JOURNAL OF MATERIALS SCIENCE, 2014, 49 (01) : 153 - 162