Formation Mechanisms and Leachability of Hexavalent Chromium in Cr2O3-Containing Refractory Castables of Electric Arc Furnace Cover

被引:0
|
作者
Yingjiang Wu
Shengqiang Song
Zhengliang Xue
Mithun Nath
机构
[1] Wuhan University of Science and Technology,The State Key Laboratory of Refractories and Metallurgy
[2] Wuhan University of Science and Technology,Key Laboratory for Ferrous Metallurgy and Resources Utilization of Ministry of Education
[3] Hubei Provincial Engineering Technology Research Center of Metallurgical Secondary Resources,undefined
关键词
D O I
暂无
中图分类号
学科分类号
摘要
Cr (III)-containing refractories are widely used as electric-arc furnace cover because of their excellent corrosion resistance properties. However, the formation of hexavalent chromium [Cr(VI)] remains a matter of concern during the service and subsequent disposal of the spent refractories. Moreover, the Cr(VI) formation mechanism and total amount of Cr(VI) generated are not clearly understood. In this study, samples from different parts of a spent electric arc furnace cover were collected from a local integrated steel plant. The phase composition, microstructure, formation and leachability of Cr(VI) were investigated using X-ray photoelectron spectroscopy, X-ray diffraction, scanning electron microscopy with energy dispersive X-ray spectroscopy, and TRGS 613 leaching test (Technische Regeln für Gefahrstoffe-TRGS 613-October 2002)/multiple leaching tests. A Cr(VI)-containing phase namely CaCrO4 existed in the sample at a medium temperature range, while another Cr(VI)-containing phase namely hauyne (Ca4Al6CrO16) and a Cr(III)-containing phase (Al2O3–Cr2O3 solid solution) formed in the high temperature region. Concentrations of Cr(VI) in the leachates (as in the TRGS 613 procedure) exceeded the European permissible limit. During the leaching tests in an acid condition, Cr(VI) was reduced by Fe2+, which was primarily derived from the dissolution of FeO in the samples, while more Cr(VI) leached out with distilled water. Formation of an Al2O3–Cr2O3 solid solution can inhibit Cr(VI) generation.
引用
收藏
页码:808 / 815
页数:7
相关论文
共 50 条
  • [1] Formation Mechanisms and Leachability of Hexavalent Chromium in Cr2O3-Containing Refractory Castables of Electric Arc Furnace Cover
    Wu, Yingjiang
    Song, Shengqiang
    Xue, Zhengliang
    Nath, Mithun
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2019, 50 (02): : 808 - 815
  • [2] Correction to: Formation Mechanisms and Leachability of Hexavalent Chromium in Cr2O3-Containing Refractory Castables of Electric Arc Furnace Cover
    Yingjiang Wu
    Shengqiang Song
    Zhengliang Xue
    Mithun Nath
    Metallurgical and Materials Transactions B, 2019, 50 : 1528 - 1528
  • [3] Formation Mechanisms and Leachability of Hexavalent Chromium in Cr2O3-Containing Refractory Castables of Electric Arc Furnace Cover (vol 50, pg 808, 2019)
    Wu, Yingjiang
    Song, Shengqiang
    Xue, Zhengliang
    Nath, Mithun
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2019, 50 (03): : 1528 - 1528
  • [4] Effect of cooling conditions on the leachability of chromium in Cr2O3-containing steelmaking slag
    Yu, Y.
    Wang, D.
    Li, J.
    Li, M.
    Xue, Z.
    JOURNAL OF THE SOUTHERN AFRICAN INSTITUTE OF MINING AND METALLURGY, 2018, 118 (05) : 539 - 543
  • [5] Formation and leachability of hexavalent chromium in the Al2O3-CaO-MgO-Cr2O3 system
    Wu, Yingjiang
    Song, Shengqiang
    Garbers-Craig, Andrie M.
    Xue, Zhengliang
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2018, 38 (06) : 2649 - 2661
  • [6] Effect of Cr2O3 addition on corrosion mechanism of refractory castables for waste melting furnaces and concurrent formation of hexavalent chromium
    Nath, Mithun
    Song, Shengqiang
    Li, Yawei
    Xu, Yibiao
    CERAMICS INTERNATIONAL, 2018, 44 (02) : 2383 - 2389
  • [7] Formation, leachability and encapsulation of hexavalent chromium in the Al2O3-CaO-Fe2O3-Cr2O3 system
    Song, Shengqiang
    Garbers-Craig, Andrie M.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2016, 36 (06) : 1479 - 1485
  • [8] Inhibited Cr(VI) formation in Cr2O3-containing refractory castable using reactive MgO as hydraulic binder
    Guo, Liu
    Song, Shengqiang
    Mu, Yuandong
    Ye, Guotian
    Chen, Liugang
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2022, 42 (16) : 7656 - 7666
  • [9] Phase evolution with temperature in chromium-containing refractory castables used for waste melting furnaces and Cr(VI) leachability
    Nath, Mithun
    Song, Shengqiang
    Garbers-Craig, Andrie M.
    Li, Yawei
    CERAMICS INTERNATIONAL, 2018, 44 (16) : 20391 - 20398
  • [10] ELECTRICAL-PROPERTIES OF CR2O3-CONTAINING GLASSES
    MOURE, C
    FERNANDEZARROYO, G
    JURADO, JR
    PASCUAL, C
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 1983, 56 (1-3) : 385 - 385