The processes of melting and solidification of the eutectic Sn–43 mol % Bi alloy are studied by cyclic thermal analysis. It is found that this alloy melts at a temperature TL = 412 K (which corresponds to the reference melting temperature of the eutectic) upon heating and solidifies isothermally at a temperature TS = 394 K upon cooling; that is, the temperature difference is ΔTLS −= 18 K. A comparison of temperatures TL and TS reveals a temperature hysteresis (TH). The activities and the activity coefficients of tin and bismuth in the eutectic are calculated at temperatures TL and TS. The enthalpies of melting at TL and solidification at TS are measured. The ways of changing the Gibbs energy during TH are determined. © 2017, Pleiades Publishing, Ltd.
引用
收藏
页码:612 / 616
页数:4
相关论文
共 50 条
  • [1] Solidification of the Eutectic Ga-Sn Alloy
    Aleksandrov, V. D.
    Frolova, S. A.
    Amerkhanova, Sh. K.
    RUSSIAN METALLURGY, 2016, (05): : 437 - 442
  • [2] Superconductivity of the Bi–Sn Eutectic Alloy
    M. V. Likholetova
    E. V. Charnaya
    E. V. Shevchenko
    Yu. A. Kumzerov
    Physics of the Solid State, 2021, 63 : 232 - 236
  • [3] Superconductivity of the Bi-Sn Eutectic Alloy
    Likholetova, M. V.
    Charnaya, E. V.
    Shevchenko, E. V.
    Kumzerov, Yu. A.
    PHYSICS OF THE SOLID STATE, 2021, 63 (02) : 232 - 236
  • [4] Structural changes in Bi-43 wt % Sn eutectic alloy under superplastic deformation
    V. F. Korshak
    Yu. A. Shapovalov
    O. Prymak
    A. P. Kryshtal
    R. L. Vasilenko
    The Physics of Metals and Metallography, 2015, 116 : 829 - 837
  • [5] Effect of liquid–liquid structure transition on solidification of Sn57Bi43 alloy
    Mingyang Li
    Yongxing Zhang
    Chen Wu
    Haoran Geng
    Applied Physics A, 2016, 122
  • [6] Structural changes in Bi-43 wt % Sn eutectic alloy under superplastic deformation
    Korshak, V. F.
    Shapovalov, Yu. A.
    Prymak, O.
    Kryshtal, A. P.
    Vasilenko, R. L.
    PHYSICS OF METALS AND METALLOGRAPHY, 2015, 116 (08): : 829 - 837
  • [7] Peculiarities of the volume ratio of α and β phases in the superplastic eutectic Bi-43 wt % Sn Alloy
    V. F. Korshak
    P. V. Mateychenko
    Yu. A. Shapovalov
    The Physics of Metals and Metallography, 2014, 115 : 1249 - 1258
  • [8] Peculiarities of the volume ratio of α and β phases in the superplastic eutectic Bi-43 wt % Sn Alloy
    Korshak, V. F.
    Mateychenko, P. V.
    Shapovalov, Yu. A.
    PHYSICS OF METALS AND METALLOGRAPHY, 2014, 115 (12): : 1249 - 1258
  • [9] Mechanism of anomalous eutectic formation in the solidification of undercooled Ni–Sn eutectic alloy
    J.F. Li
    X.L. Li
    L. Liu
    S.Y. Lu
    Journal of Materials Research, 2008, 23 : 2139 - 2148
  • [10] Directional solidification and characterization of the Cd-Sn eutectic alloy
    Cadirli, E.
    Kaya, H.
    Gunduz, M.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2007, 431 (1-2) : 171 - 179