The scientific pursuit of the determination of mechanisms of corrosion of metals and alloys operating at high temperatures in thermal power generating environments has resulted in volumes of reported data, yet little achievement has been made so far. In reviewing the literature, it has been attempted here to indicate the diversified nature of the problems and the characteristics of various parameters such as mineralogical constituents of the fuel, fuel ash and various products of combustion (e.g. sulphurous oxides, sulphates, pyrosulphates, sulphides, etc.) in monitoring the rate of reactions, and hence corrosion, of component materials. Rapid and intensive corrosion attack due to conjoint action of gaseous, chemical and liquid phases under normal boiler operating conditions have been expressed to offer a really challenging situation for further studies.
引用
收藏
页码:835 / 849
页数:14
相关论文
共 50 条
  • [1] Fuel ash corrosion of boiler and superheater tubes
    Srivastava, SC
    Godiwalla, KM
    Banerjee, MK
    JOURNAL OF MATERIALS SCIENCE, 1997, 32 (04) : 835 - 849
  • [2] Influence of ash composition on the corrosion rate of superheater tubes
    Nishio, T
    Shinohara, M
    Matsumoto, H
    Arakawa, Y
    2001 INTERNATIONAL CHEMICAL RECOVERY CONFERENCE: CHANGING RECOVERY TECHNOLOGY TO MEET THE CHALLENGES OF THE PULP AND PAPER INDUSTRY, 2001, : P39 - P42
  • [3] Recovery boiler superheater corrosion
    Crowe, DC
    Youngblood, WC
    9TH INTERNATIONAL SYMPOSIUM ON CORROSION IN THE PULP AND PAPER INDUSTRY, 1998, : 225 - 230
  • [4] Corrosion and life assessment of Intrex™ superheater tubes in a CFB oil shale boiler
    Dedov, Andrei
    Klevtsov, Ivan
    Lausmaa, Toomas
    Hlebnikov, Aleksandr
    Bojarinova, Tatjana
    APPLIED THERMAL ENGINEERING, 2016, 101 : 468 - 478
  • [5] Corrosion of high-alloy superheater tubes in a coastal biomass power boiler
    Kish, J. R.
    Reid, C.
    Singbeil, D. L.
    Seguin, R.
    CORROSION, 2008, 64 (04) : 356 - 366
  • [6] Retardation of High-Temperature Fuel Ash Corrosion of Fireside Boiler Tubes via Nanoparticles
    Anees A. Khadom
    Hongfang Liu
    Ahmed A. Fadhil
    Abdul Mun’em A. Karim
    Oxidation of Metals, 2016, 86 : 553 - 565
  • [7] Retardation of High-Temperature Fuel Ash Corrosion of Fireside Boiler Tubes via Nanoparticles
    Khadom, Anees A.
    Liu, Hongfang
    Fadhil, Ahmed A.
    Karim, Abdul Mun'em A.
    OXIDATION OF METALS, 2016, 86 (5-6): : 553 - 565
  • [8] IMPROVED MATERIALS FOR COAL FIRED BOILER SUPERHEATER AND REHEATER TUBES SUBJECTED TO FIRESIDE CORROSION
    REHN, IM
    JOURNAL OF METALS, 1984, 36 (07): : 21 - 21
  • [9] Effect of sulphur containing additive on initial corrosion of superheater tubes in waste fired boiler
    Viklund, P.
    Pettersson, R.
    Hjornhede, A.
    Henderson, P.
    Sjovall, P.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2009, 44 (03) : 234 - 240
  • [10] Laboratory-simulated fuel-ash corrosion of superheater tubes in coal-fired ultra-supevcritical-boilers
    Castello, P
    Guttmann, V
    Farr, N
    Smith, G
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2000, 51 (11): : 786 - 790