A study of Sn-Bi-Ag-(In) lead-free solders

被引:0
|
作者
Ren-Kae Shiue
Leu-Wen Tsay
Chun-Lun Lin
Jia-Lin Ou
机构
[1] National Dong Hwa University,Department of Materials Science and Engineering
[2] National Taiwan Ocean University,Institute of Materials Science and Engineering
来源
关键词
Thermal Expansion; Expansion Coefficient; Thermal Expansion Coefficient; Liquidus Temperature; Interfacial Reaction;
D O I
暂无
中图分类号
学科分类号
摘要
Sn-Bi-Ag-(In) solder alloys have been extensively studied in the study. The experimental results reveals that the liquidus temperatures of Sn-(1–5) Bi-(2–3.5)Ag-(0–10)In solders are between 201.7 and 225.3°C, which were higher than that of the most popular eutectic Pb-Sn solder (183°C). Additions of (5–10) wt% In into Sn-Bi-Ag solders can effectively decrease the melting point of the solder alloy. However, the gap between Ts and TL temperatures increases with the additions of Bi and In into Sn-Bi-Ag-(In) solders. Although there is no flux applied during soldering, most Sn-Bi-Ag-(In) solder alloys can well bond the Au/Ni metallized copper substrate. 94Sn-3Bi-3Ag solder demonstrates the lowest wetting angle of 45° among all test samples. Thermal expansion coefficients of both 94Sn-3Bi-3Ag and 90Sn-2Bi-3Ag-5In solders are slightly less than that of 63Sn-37Pb. Both 90Sn-2Bi-3Ag-5In/substrate and 94Sn-3Bi-3Ag/substrate interfaces demonstrate similar reaction kinetics in the experiment. The stability of the interface is greatly impaired during 90°C aging. Some locations of the electroless Ni layer break down, and new phases are formed nearby the interface during aging treatment. Initially, the growth of Ni-rich (Ni,Cu)3Sn4 phase dominates the interfacial reaction. However, the growth of Cu-rich (Cu,Ni)6Sn5 phase will dominate the reaction layer for specimens aged at 90°C for long time periods.
引用
收藏
页码:1269 / 1279
页数:10
相关论文
共 50 条
  • [1] A study of Sn-Bi-Ag-(In) lead-free solders
    Shiue, RK
    Tsay, LW
    Lin, CL
    Ou, JL
    JOURNAL OF MATERIALS SCIENCE, 2003, 38 (06) : 1269 - 1279
  • [2] Creep deformation of lead-free Sn-3.5Ag-Bi solders
    Shin, SW
    Yu, J
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 2003, 42 (03): : 1368 - 1374
  • [3] Tensile deformation behavior of Sn-Ag-Bi system lead-free solders
    Takemoto, Tadashi
    Takahashi, Masahiro
    Matsunawa, Akira
    Ninomiya, Ryuji
    Tai, Hideo
    Yosetsu Gakkai Ronbunshu/Quarterly Journal of the Japan Welding Society, 1998, 16 (01): : 87 - 92
  • [4] Creep deformation of lead-free Sn-3.5 Ag-Bi solders
    Shin, S.W., 1600, Japan Society of Applied Physics (42):
  • [5] Mechanical characterization of Sn-Ag-based lead-free solders
    Amagai, M
    Watanabe, M
    Omiya, M
    Kishimoto, K
    Shibuya, T
    MICROELECTRONICS RELIABILITY, 2002, 42 (06) : 951 - 966
  • [6] Properties and Microstructures of Sn-Bi-X Lead-Free Solders
    Yang, Fan
    Zhang, Liang
    Liu, Zhi-quan
    Zhong, Su-juan
    Ma, Jia
    Bao, Li
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2016, 2016
  • [7] Study on microstructure and properties of Sn-Ag-Cu-Mg lead-free solders
    Lu, Sheng
    Chen, Jing
    Luo, Fei
    Wang, Baohua
    ESTC 2008: 2ND ELECTRONICS SYSTEM-INTEGRATION TECHNOLOGY CONFERENCE, VOLS 1 AND 2, PROCEEDINGS, 2008, : 1193 - +
  • [8] Effect of Ag, Ni and Bi Additions on Solderability of Lead-Free Solders
    Nobari, Amir Hossein
    Maalekian, Mehran
    Seelig, Karl
    Pekguleryuz, Mihriban
    JOURNAL OF ELECTRONIC MATERIALS, 2017, 46 (07) : 4076 - 4084
  • [9] Effect of Ag, Ni and Bi Additions on Solderability of Lead-Free Solders
    Amir Hossein Nobari
    Mehran Maalekian
    Karl Seelig
    Mihriban Pekguleryuz
    Journal of Electronic Materials, 2017, 46 : 4076 - 4084
  • [10] Fatigue crack-growth behavior of Sn-Ag-Cu and Sn-Ag-Cu-Bi lead-free solders
    Zhao, J
    Mutoh, Y
    Miyashita, Y
    Mannan, SL
    JOURNAL OF ELECTRONIC MATERIALS, 2002, 31 (08) : 879 - 886