A Comparison of Creep Rupture Strength of Ferritic/Austenitic Dissimilar Weld Joints of Different Grades of Cr-Mo Ferritic Steels

被引:0
|
作者
K. Laha
K. S. Chandravathi
P. Parameswaran
Sunil Goyal
M. D. Mathew
机构
[1] Metallurgy and Materials Group,
[2] Indira Gandhi Centre for Atomic Research,undefined
关键词
Weld Metal; Weld Joint; PWHT; Ferritic Steel; Weld Interface;
D O I
暂无
中图分类号
学科分类号
摘要
Evaluations of creep rupture properties of dissimilar weld joints of 2.25Cr-1Mo, 9Cr-1Mo, and 9Cr-1MoVNb steels with Alloy 800 at 823 K were carried out. The joints were fabricated by a fusion welding process employing an INCONEL 182 weld electrode. All the joints displayed lower creep rupture strength than their respective ferritic steel base metals, and the strength reduction was greater in the 2.25Cr-1Mo steel joint and less in the 9Cr-1Mo steel joint. Failure location in the joints was found to shift from the ferritic steel base metal to the intercritical region of the heat-affected zone (HAZ) of the ferritic steel (type IV cracking) with the decrease in stress. At still lower stresses, the failure in the joints occurred at the ferritic/austenitic weld interface. The stress-life variation of the joints showed two-slope behavior and the slope change coincided with the occurrence of ferritic/austenitic weld interface cracking. Preferential creep cavitation in the soft intercritical HAZ induced type IV failure, whereas creep cavitation at the interfacial particles induced ferritic/austenitic weld interface cracking. Micromechanisms of the type IV failure and the ferritic/austenitic interface cracking in the dissimilar weld joint of the ferritic steels and relative cracking susceptibility of the joints are discussed based on microstructural investigation, mechanical testing, and finite element analysis (FEA) of the stress state across the joint.
引用
收藏
页码:1174 / 1186
页数:12
相关论文
共 50 条
  • [1] A Comparison of Creep Rupture Strength of Ferritic/Austenitic Dissimilar Weld Joints of Different Grades of Cr-Mo Ferritic Steels
    Laha, K.
    Chandravathi, K. S.
    Parameswaran, P.
    Goyal, Sunil
    Mathew, M. D.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2012, 43A (04): : 1174 - 1186
  • [2] Type IV Cracking Susceptibility in Weld Joints of Different Grades of Cr-Mo Ferritic Steel
    Laha, K.
    Chandravathi, K. S.
    Parameswaran, P.
    Rao, K. Bhanu Sankara
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2009, 40A (02): : 386 - 397
  • [3] Type IV Cracking Susceptibility in Weld Joints of Different Grades of Cr-Mo Ferritic Steel
    K. Laha
    K.S. Chandravathi
    P. Parameswaran
    K. Bhanu Sankara Rao
    Metallurgical and Materials Transactions A, 2009, 40 : 386 - 397
  • [4] Analysis of Creep Rupture Behavior of Cr-Mo Ferritic Steels in the Presence of Notch
    Goyal, Sunil
    Laha, K.
    Das, C. R.
    Mathew, M. D.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2015, 46A (01): : 205 - 217
  • [5] Analysis of Creep Rupture Behavior of Cr-Mo Ferritic Steels in the Presence of Notch
    Sunil Goyal
    K. Laha
    C. R. Das
    M. D. Mathew
    Metallurgical and Materials Transactions A, 2015, 46 : 205 - 217
  • [6] Mechanistic approach for prediction of creep deformation, damage and rupture life of different Cr-Mo ferritic steels
    Goyal, S.
    Laha, K.
    Selvi, S. Panneer
    Mathew, M. D.
    MATERIALS AT HIGH TEMPERATURES, 2014, 31 (03) : 211 - 220
  • [7] An evaluation of creep rupture strength of ferritic/austenitic dissimilar weld interfaces using cohesive zone modelling
    Hu, Jia-nan
    Fukahori, Takuya
    Igari, Toshihide
    Chuman, Yasuharu
    Cocks, Alan C. F.
    21ST EUROPEAN CONFERENCE ON FRACTURE, (ECF21), 2016, 2 : 934 - 941
  • [8] REDUCED-ACTIVATION FERRITIC STEELS - A COMPARISON WITH CR-MO STEELS
    KLUEH, RL
    MAZIASZ, PJ
    JOURNAL OF NUCLEAR MATERIALS, 1988, 155 : 602 - 607
  • [9] Modelling of creep rupture of ferritic/austenitic dissimilar weld interfaces under mode I fracture
    Hu, Jia-nan
    Fukahori, Takuya
    Igari, Toshihide
    Chuman, Yasuharu
    Cocks, Alan C. F.
    ENGINEERING FRACTURE MECHANICS, 2018, 191 : 344 - 364
  • [10] Decomposition modes of austenite in Cr-Mo ferritic steels
    Parameswaran, P
    Saroja, S
    Vijayalakshmi, M
    Raghunathan, VS
    JOURNAL OF NUCLEAR MATERIALS, 1996, 232 (2-3) : 226 - 232