Hydriding/dehydriding properties of MgH2/5 wt.% Ni coated CNFs composite

被引:35
|
作者
Wu, C. Z. [1 ]
Yao, X. D. [2 ,3 ]
Zhang, H. [4 ]
机构
[1] Chinese Acad Sci, Dalian Inst Chem Phys, Dalian 116023, Peoples R China
[2] Univ Queensland, Sch Engn, ARC Ctr Excellence Funct Nanomat, St Lucia, Qld 4072, Australia
[3] Griffith Univ, Queensland Micro & Nanotechnol Ctr, Nathan, Qld 4072, Australia
[4] Shenyang Inst Chem Technol, Sch Mat Sci & Engn, Shenyang 110142, Peoples R China
关键词
Hydrogen storage materials; Magnesium hydride; Ni coated CNFs; Composites; Ball milling; HYDROGEN STORAGE PROPERTIES; CARBON NANOTUBES; MAGNESIUM; SORPTION; KINETICS; NB2O5; MG; NANOCOMPOSITES; IMPROVEMENT; GRAPHITE;
D O I
10.1016/j.ijhydene.2009.10.079
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this paper, we reported that the prepared nickel coated carbon nanofibers (NiCNFs) by electroless plating method exhibited superior catalytic effect on hydrogen absorption/desorption of magnesium (Mg). It is demonstrated that the nanocomposites of MgH2/5 wt.% NiCNFs prepared by ball milling could absorb hydrogen very fast at low temperatures, e.g. absorb similar to 6.0 wt.% hydrogen in 5 min at 473 K and similar to 5.0 wt.% hydrogen in 10 min even at a temperature as low as 423 K. More importantly, the desorption of hydrogen was also significantly improved with additives of NiCNFs. Diffraction scanning calorimetry (DSC) measurement indicated that the peak desorption temperature decreased 50 K and the onset temperature for desorption decreased 123 K. The composites also desorbed hydrogen fast, e.g. desorb 5.5 wt.% hydrogen within 20 min at 573 K. It is suggested that the new phase of Mg2Ni, and the nano-sized dispersed distribution of Ni and carbon contributed to this significant improvement. Johnson-Mehl-Avrami (JMA) analysis illustrated that hydrogen diffusion is the rate-limiting step for hydrogen absorption/desorption. (C) 2009 Professor T. Nejat Veziroglu. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:247 / 252
页数:6
相关论文
共 50 条
  • [1] THE EFFECT OF SURFACE NICKEL ON THE HYDRIDING-DEHYDRIDING KINETICS OF MGH2
    EISENBERG, FG
    ZAGNOLI, DA
    SHERIDAN, JJ
    JOURNAL OF THE LESS-COMMON METALS, 1980, 74 (02): : 323 - 331
  • [2] Hydriding and dehydriding properties of Mg2Ni/Ni and Mg2 Ni/Ni+5 wt.% Cu prepared by mechanical alloying
    Palacios-Lazcano, A. F.
    Cabanas-Moreno, J. G.
    Bonifacio-Martinez, J.
    Iturbe-Garcia, J. L.
    Cruz-Gandarilla, F.
    Calderon, H. A.
    REVISTA MEXICANA DE FISICA, 2009, 55 (05) : 367 - 372
  • [3] Effects of Indium on the Dehydriding Properties of MgH2
    Zhong Haichang
    Wang Hui
    RARE METAL MATERIALS AND ENGINEERING, 2014, 43 (11) : 2806 - 2809
  • [4] Hydriding/dehydriding behaviors of La2Mg17-10 wt.%Ni composite prepared by mechanical milling
    Liu Jing
    Li Qian
    JOURNAL OF RARE EARTHS, 2013, 31 (01) : 73 - 78
  • [5] Hydriding/dehydriding behaviors of La2Mg17-10 wt.%Ni composite prepared by mechanical milling
    刘静
    李谦
    Journal of Rare Earths, 2013, 31 (01) : 73 - 78
  • [6] Effects of indium on the dehydriding properties of MgH2
    Zhong, Haichang, 1600, Science Press (43):
  • [7] Differences in the heterogeneous nature of hydriding/dehydriding kinetics of MgH2 - TiH2 nanocomposites
    Biasetti Andres, T.
    Zelis Luis, Mendoza
    Marcos, Meyer
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2020, 45 (51) : 27421 - 27433
  • [8] Hydriding/Dehydriding Properties of an MgH2+20%(w) MgTiO3 Composite
    Wang Jia-Sheng
    Han Shu-Min
    Li Yuan
    Shen Na
    Zhang Wei
    ACTA PHYSICO-CHIMICA SINICA, 2014, 30 (12) : 2323 - 2327
  • [9] Preparation of a sample with a single MgH2 phase by horizontal ball milling and the first hydriding reaction of 90 wt% Mg-10 wt% MgH2
    Seong-Hyeon Hong
    Myoung Youp Song
    Metals and Materials International, 2015, 21 : 422 - 428
  • [10] Catalytic effect of ZrCrNi alloy on hydriding properties of MgH2
    Agarwal, Shivani
    Aurora, Annalisa
    Jain, Ankur
    Jain, I. P.
    Montone, Amelia
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2009, 34 (22) : 9157 - 9162