Effect of cooling condition on the intergranular corrosion resistance of UNS S32506 duplex stainless steel

被引:18
|
作者
Takei, Takayuki [1 ]
Yabe, Murotsune [1 ]
Wei, Fu-Gao [1 ]
机构
[1] Nippon Yakin Kogyo Co Ltd, Tech Res Ctr, Kawasaki Ku, 4-2 Kojima Cho, Kawasaki, Kanagawa 2108558, Japan
关键词
Duplex stainless steel; Intergranular corrosion; Cooling condition; Cr depletion; alpha/gamma Interface; SECONDARY AUSTENITE; PITTING CORROSION; HEAT-TREATMENT; NITRIC-ACID; SIGMA-PHASE; MICROSTRUCTURE; PRECIPITATION; BEHAVIOR; SUSCEPTIBILITY; PHOSPHORUS;
D O I
10.1016/j.corsci.2017.03.018
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of cooling condition on the intergranular corrosion resistance of UNS S32506 duplex stainless steel was investigated by means of Huey test and microstructural observation. It was found that quenching at a temperature below 800 degrees C after air cooling at a fixed rate from solutionization temperature enhances the intergranular corrosion rate. No precipitation has been found at all cooling conditions. Formation of Cr-depletion zone on the gamma phase side of the alpha/gamma interface due to local chemical change accompanying alpha-gamma phase transformation during air cooling is responsible for the intergranular corrosion degradation of the UNS S32506 duplex stainless steel.
引用
收藏
页码:80 / 89
页数:10
相关论文
共 50 条
  • [1] Effect of Boron Distribution on the Intergranular Corrosion Resistance of UNS S32506 Duplex Stainless Steels
    Takei, Takayuki
    Yabe, Murotsune
    Ooi, Azusa
    Tada, Eiji
    Nishikata, Atsushi
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2019, 166 (13) : C375 - C381
  • [2] Evaluation of the intergranular corrosion susceptibility of UNS S31803 duplex stainless steel with thermoelectric power measurements
    Ortiz, N.
    Curiel, F. F.
    Lopez, V. H.
    Ruiz, A.
    CORROSION SCIENCE, 2013, 69 : 236 - 244
  • [3] Effect of annealing temperature on the pitting corrosion resistance of super duplex stainless steel UNS S32750
    Tan, Hua
    Jiang, Yiming
    Deng, Bo
    Sun, Tao
    Xu, Juliang
    Li, Jin
    MATERIALS CHARACTERIZATION, 2009, 60 (09) : 1049 - 1054
  • [4] Effect of cooling rate after heat treatment on pitting corrosion of super duplex stainless steel UNS S 32750
    Shin, Byung-Hyun
    Park, Junghyun
    Jeon, Jongbae
    Heo, Sung-bo
    Chung, Wonsub
    ANTI-CORROSION METHODS AND MATERIALS, 2018, 65 (05) : 492 - 498
  • [5] Effect of cooling intensity on impact toughness and corrosion resistance of duplex stainless steel
    Wang R.
    Honda M.
    Miyauchi K.
    Mori T.
    Fukuhara H.
    Zairyo/Journal of the Society of Materials Science, Japan, 2020, 69 (06) : 471 - 478
  • [6] Determination of Susceptibility to Intergranular Corrosion of UNS 31803 Type Duplex Stainless Steel by Electrochemical Reactivation Method
    Arikan, Mehmet Emin
    Arikan, Rafet
    Doruk, Mustafa
    INTERNATIONAL JOURNAL OF CORROSION, 2012, 2012 (2012)
  • [7] Determination of susceptibility to intergranular corrosion of UNS 31803 type duplex stainless steel by electrochemical reactivation method
    Metallurgical and Materials Engineering Department, Middle East Technical University, Ankara, Turkey
    Turk. J. Eng. Environ. Sci., 2008, 6 (323-335): : 323 - 335
  • [8] The effect of cooling rate on the mechanical and corrosion properties of SAF 2205 (UNS 31803) duplex stainless steel welds
    Kordatos, JD
    Fourlaris, G
    Papadimitriou, G
    SCRIPTA MATERIALIA, 2001, 44 (03) : 401 - 408
  • [9] Comparative analysis of the corrosion resistance of UNS S31200 duplex stainless steel and its analogue
    Lapechenkov, Andrey
    Fedorov, Aleksandr
    Galata, Lyudmila
    Piskarev, Aleksey
    MATERIALS TODAY-PROCEEDINGS, 2020, 30 : 361 - 364
  • [10] Microstructure and intergranular corrosion resistance of UNS S17400 (17-4PH) stainless steel
    Tavares, S. S. M.
    da Silva, F. J.
    Scandian, C.
    da Silva, G. F.
    de Abreu, H. F. G.
    CORROSION SCIENCE, 2010, 52 (11) : 3835 - 3839