Analysis of Adhesion and Fracture Energy of Nano-Particle Silver in Electronics Packaging Applications

被引:12
|
作者
Joo, Sung Chul [1 ]
Baldwin, Daniel F. [1 ]
机构
[1] Georgia Inst Technol, George W Woodruff Sch Mech Engn, Packaging Res Ctr, Atlanta, GA 30332 USA
来源
关键词
Adhesion; button shear; die shear; electronics packaging; interfacial bond strength; interfacial fracture; interfacial fracture energy; nano-particle silver; FAILURE;
D O I
10.1109/TADVP.2009.2033809
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Nano-particle silver (NPS) conductors are increasingly being investigated for package level electronics applications. Unlike traditional thick film materials and conductive inks, nano-particle conductors often do not incorporate compounds to promote interfacial adhesion such as binders used in thick films and polymer adhesives used in conductive inks as these adhesion promoters can degrade the electrical performance. The NPS is concerned with low adhesion to most of processed polymer surface such as liquid crystal polymer (LCP), polyimide, and benzocyclobutene (BCB). Moreover, the adhesion mechanism of NPS has not been identified yet. Thus, as a first step to identify NPS adhesion mechanism and thus, to improve NPS adhesion, quantitative measurement of the adhesion strength of NPS is necessary. Since conventional adhesion test methods are not directly applicable to thin (similar to 2 mu m) NPS film adhesion test, a new adhesion test method is developed in this paper to estimate the adhesion strength of NPS films. The newly developed adhesion test method is called modified button shear test (MBST) because it modifies the conventional button shear test and integrates the generally known die shear test. The MBST is used for measuring not only interfacial bond strength, but also interfacial fracture energy. The interfacial bond strength in tension and the interfacial fracture energy of NPS with LCP substrate measured by MBST are 24.4 MPa and 17.2 J/m(2), respectively. The MBST is generic in nature and can be extended to other thin films adhesion test for measuring interfacial bond strength and interfacial fracture energy.
引用
收藏
页码:48 / 57
页数:10
相关论文
共 50 条
  • [1] Interfacial adhesion of nano-particle silver interconnects for electronics packaging application
    Joo, Sungchul
    Baldwin, Daniel F.
    58TH ELECTRONIC COMPONENTS & TECHNOLOGY CONFERENCE, PROCEEDINGS, 2008, : 1417 - 1423
  • [2] Characterization of Silver Nano-particle CoatedEichhornia crassipesFiber for Antibacterial Applications
    Palai, Basantakumar
    Sarangi, Saroj Kumar
    Mohapatra, Siba Shankar
    JOURNAL OF NATURAL FIBERS, 2022, 19 (05) : 1828 - 1836
  • [3] Reliability testing of nano-particle system packaging
    James E. Morris
    Microsystem Technologies, 2009, 15 : 139 - 143
  • [4] Reliability testing of nano-particle system packaging
    Morris, James E.
    MICROSYSTEM TECHNOLOGIES-MICRO-AND NANOSYSTEMS-INFORMATION STORAGE AND PROCESSING SYSTEMS, 2009, 15 (01): : 139 - 143
  • [5] Micro/nano-particle manipulation and adhesion studies
    Ding, Weiqiang
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2008, 22 (5-6) : 457 - 480
  • [6] Micro/nano-particle manipulation and adhesion studies
    Ding, Weiqiang
    Journal of Adhesion Science and Technology, 2008, 22 (5-6): : 457 - 480
  • [7] On fracture toughness of nano-particle modified epoxy
    Liu, Hong-Yuan
    Wang, Gong-Tao
    Mai, Yiu-Wing
    Zeng, Ying
    COMPOSITES PART B-ENGINEERING, 2011, 42 (08) : 2170 - 2175
  • [8] Development of high adhesion nano-thermal interface materials for electronics packaging applications
    Aronsson, Tomas
    Wang, Wen Xuan
    Olorunyomi, Michael Olugbenga
    Lu, Xiuzhen
    Shangguan, Dongkai
    Liu, Johan
    2006 INTERNATIONAL CONFERENCE ON ELECTRONIC MATERIALS AND PACKAGING, VOLS 1-3, 2006, : 277 - +
  • [9] New nano-particle material (NPM) for micro- and opto-electronic packaging applications
    Suhir, E
    2005 10th International Symposium on Advanced Packaging Materials: Processes, Properties and Interfaces, 2005, : 255 - 258
  • [10] Nano-particle Sensor for Biomedical Applications: Bioimaging
    Singh, Aditi
    Rao, Krishna M.
    Singh, Satya Pal
    3RD INTERNATIONAL CONFERENCE ON CONDENSED MATTER & APPLIED PHYSICS (ICC-2019), 2020, 2220