Effect of rapid thermal annealing on the mechanical stress and physico-chemical properties in plasma enhanced atomic layer deposited silicon nitride thin films

被引:0
|
作者
Peter, Antony Premkumar [1 ]
Marquez, Alfonso Sepulveda [1 ]
Meersschaut, Johan [1 ]
Dara, Praveen [1 ]
Blanquart, Timothee [2 ]
Tomomi, Takayama [3 ]
Taishi, Ebisudani [3 ]
Elichiro, Shiba [3 ]
Kimura, Yosuke [1 ]
van Gompel, Sander [1 ]
Morin, Pierre [1 ]
机构
[1] Interuniv Microelect Ctr Imec, Kapeldreef 75, B-3001 Leuven, Belgium
[2] ASM Belgium, Kapeldreef 75, B-3001 Leuven, Belgium
[3] ASM Japan, KK 6-23-1, Tama, Tokyo 2060025, Japan
来源
关键词
LPCVD; TECHNOLOGY; CHALLENGES; DENSITY; SPACER;
D O I
10.1116/6.0001922
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
The present study reports the impact of process conditions and post annealing treatment on the stress and physico-chemical properties in different types of plasma enhanced atomic layer deposited (PEALD) SiNx films. More specifically, the SiNx films deposited at 500 ? were annealed subsequently at 1000 ? in N-2 ambient for different times ranging between 30 and 6750 s and were subjected to thickness, mass, refractive index, chemical bonds and structure, H content, N/Si stoichiometry, morphology, roughness, and uniformity monitoring. Depending on the deposition process conditions, we confirm the possibility to form, at 500 ? with PEALD, some very compressive SiN films with reduced hydrogen content by controlling the plasma conditions along the deposition process. More interestingly, these compressive films with low hydrogen concentration exhibit high thermo-mechanical stability compared to hydrogenated PEALD and plasma enhanced chemical vapor deposition silicon nitride from this study or reported in the literature, films which typically tend to become tensile with a similar annealing sequence. These results confirm the importance of the plasma power to engineer the as-deposited silicon nitride stress but also highlight the role of hydrogen in the thermal instability of these layers, a low H concentration being needed for a better mechanical stability. Published under an exclusive license by AIP Publishing.
引用
收藏
页数:11
相关论文
共 50 条
  • [1] Thermal annealing of superconducting niobium titanium nitride thin films deposited by plasma-enhanced atomic layer deposition
    Gonzalez Diaz-Palacio, Isabel
    Wenskat, Marc
    Deyu, Getnet Kacha
    Hillert, Wolfgang
    Blick, Robert H.
    Zierold, Robert
    JOURNAL OF APPLIED PHYSICS, 2023, 134 (03)
  • [2] THE EFFECT OF DILUENT GAS AND RAPID THERMAL ANNEALING ON THE PROPERTIES OF PLASMA-DEPOSITED SILICON-NITRIDE FILMS
    NAM, CW
    WOO, SI
    KIM, YT
    MIN, SK
    THIN SOLID FILMS, 1992, 209 (02) : 215 - 222
  • [3] Aluminum nitride thin films deposited by hydrogen plasma enhanced and thermal atomic layer deposition
    Tian, L.
    Ponton, S.
    Benz, M.
    Crisci, A.
    Reboud, R.
    Giusti, G.
    Volpi, F.
    Rapenne, L.
    Vallee, C.
    Pons, M.
    Mantoux, A.
    Jimenez, C.
    Blanquet, E.
    SURFACE & COATINGS TECHNOLOGY, 2018, 347 : 181 - 190
  • [4] Effect of rapid thermal annealing on the properties of μPCVD and PECVD silicon nitride thin films
    Bakardjieva, V
    Beshkov, G
    Vitanov, P
    Alexieva, Z
    JOURNAL OF OPTOELECTRONICS AND ADVANCED MATERIALS, 2005, 7 (01): : 377 - 380
  • [5] Material Structure and Mechanical Properties of Silicon Nitride and Silicon Oxynitride Thin Films Deposited by Plasma Enhanced Chemical Vapor Deposition
    Gan, Zhenghao
    Wang, Changzheng
    Chen, Zhong
    SURFACES, 2018, 1 (01): : 59 - 72
  • [6] Nanostructural Characteristics and Mechanical Properties of Low Temperature Plasma Enhanced Chemical Vapor Deposited Silicon Nitride Thin Films
    Huang, H.
    Dell, J. M.
    Liu, S.
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2009, 9 (06) : 3734 - 3741
  • [7] Mechanical property characterization of sputtered and plasma enhanced chemical deposition (PECVD) silicon nitride films after rapid thermal annealing
    Wu, P. -H.
    Lin, I-K
    Yan, H. -Y.
    Ou, K. -S.
    Chen, K. -S.
    Zhang, X.
    SENSORS AND ACTUATORS A-PHYSICAL, 2011, 168 (01) : 117 - 126
  • [8] Stress in low-temperature plasma enhanced chemical vapour deposited silicon nitride thin films
    Martyniuk, M
    Antoszewski, J
    Musca, CA
    Dell, JM
    Faraone, L
    SMART MATERIALS AND STRUCTURES, 2006, 15 (01) : S29 - S38
  • [9] The effect of rapid thermal annealing on properties of plasma enhanced CVD silicon oxide films
    Domínguez, C
    Rodríguez, JA
    Muñoz, FJ
    Zine, N
    THIN SOLID FILMS, 1999, 346 (1-2) : 202 - 206
  • [10] Effect of rapid thermal annealing on properties of plasma enhanced CVD silicon oxide films
    Centre Nacional de Microelectronica, 08193 Bellatera, Barcelona, Spain
    不详
    Thin Solid Films, 1 (202-206):