Ultrahigh-temperature microwave annealing of Al+- and P+-implanted 4H-SiC

被引:39
|
作者
Sundaresan, Siddarth G.
Rao, Mulpuri V.
Tian, Yong-lai
Ridgway, Mark C.
Schreifels, John A.
Kopanski, Joseph J.
机构
[1] George Mason Univ, Dept Elect & Comp Engn, Fairfax, VA 22030 USA
[2] LT Technol, Fairfax, VA 22033 USA
[3] Australian Natl Univ, Dept Elect Mat Engn, Canberra, ACT 0200, Australia
[4] George Mason Univ, Dept Chem & Biochem, Fairfax, VA 22030 USA
[5] Natl Inst Stand & Technol, Semicond Elect Div, Gaithersburg, MD 20899 USA
关键词
D O I
10.1063/1.2717016
中图分类号
O59 [应用物理学];
学科分类号
摘要
In this work, an ultrafast solid-state microwave annealing has been performed, in the temperature range of 1700-2120 degrees C on Al+- and P+-implanted 4H-SiC. The solid-state microwave system used in this study is capable of raising the SiC sample temperatures to extremely high values, at heating rates of similar to 600 degrees C/s. The samples were annealed for 5-60 s in a pure nitrogen ambient. Atomic force microscopy performed on the annealed samples indicated a smooth surface with a rms roughness of 1.4 nm for 5x5 mu m(2) scans even for microwave annealing at 2050 degrees C for 30 s. Auger sputter profiling revealed a < 7 nm thick surface layer composed primarily of silicon, oxygen, and nitrogen for the samples annealed in N-2, at annealing temperatures up to 2100 degrees C. X-ray photoelectron spectroscopy revealed that this surface layer is mainly composed of silicon oxide and silicon nitride. Secondary ion mass spectrometry depth profiling confirmed almost no dopant in diffusion after microwave annealing at 2100 degrees C for 15 s. However, a sublimation of similar to 100 nm of the surface SiC layer was observed for 15 s annealing at 2100 degrees C. Rutherford backscattering spectra revealed a lattice damage-free SiC material after microwave annealing at 2050 degrees C for 15 s, with scattering yields near the virgin SiC material. Van der Pauw-Hall measurements have revealed sheet resistance values as low as 2.4 k Omega/square for Al+-implanted material annealed at 2100 degrees C for 15 s and 14 Omega/square for the P+-implanted material annealed at 1950 degrees C for 30 s. The highest electron and hole mobilities measured in this work were 100 and 6.8 cm(2)/V s, respectively, for the P+- and Al+-implanted materials. (c) 2007 American Institute of Physics.
引用
收藏
页数:7
相关论文
共 50 条
  • [1] Microwave Annealing of Ion Implanted 4H-SiC
    Rao, Mulpuri V.
    Nath, A.
    Qadri, S. B.
    Tian, Y-L.
    Nipoti, R.
    ION IMPLANTATION TECHNOLOGY 2010, 2010, 1321 : 241 - +
  • [2] Laser Annealing of P and Al Implanted 4H-SiC Epitaxial Layers
    Calabretta, Cristiano
    Agati, Marta
    Zimbone, Massimo
    Boninelli, Simona
    Castiello, Andrea
    Pecora, Alessandro
    Fortunato, Guglielmo
    Calcagno, Lucia
    Torrisi, Lorenzo
    La Via, Francesco
    MATERIALS, 2019, 12 (20)
  • [3] Microwave annealing of Al+ implanted 4H-SiC: towards device fabrication
    Nath, A.
    Parisini, A.
    Tian, Y-L
    Rao, M. V.
    Nipoti, R.
    SILICON CARBIDE AND RELATED MATERIALS 2013, PTS 1 AND 2, 2014, 778-780 : 653 - +
  • [4] Shuttle activation annealing of implanted al in 4H-SiC
    Watanabe, Tomokatsu
    Hattori, Ryo
    Imaizumi, Masayuki
    Oomori, Tatsuo
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2008, 47 (04) : 2841 - 2844
  • [5] Shuttle activation annealing of implanted Al in 4H-SiC
    Watanabe, Tomokatsu
    Hattori, Ryo
    Imaizumi, Masayuki
    Oomori, Tatsuo
    Japanese Journal of Applied Physics, 2008, 47 (4 PART 2): : 2841 - 2844
  • [6] Defect formation in (0001)- and (1120)-oriented 4H-SiC crystals P+-Implanted at room temperature
    Okada, T
    Negoro, Y
    Kimoto, T
    Okamoto, K
    Kujime, N
    Tanaka, N
    Matsunami, H
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 2004, 43 (10): : 6884 - 6889
  • [7] Microwave Annealing of High Dose Al+-implanted 4H-SiC: Towards Device Fabrication
    Nath, A.
    Rao, Mulpuri V.
    Tian, Y. -L.
    Parisini, A.
    Nipoti, R.
    JOURNAL OF ELECTRONIC MATERIALS, 2014, 43 (04) : 843 - 849
  • [8] Microwave Annealing of High Dose Al+-implanted 4H-SiC: Towards Device Fabrication
    A. Nath
    Mulpuri V. Rao
    Y. -L. Tian
    A. Parisini
    R. Nipoti
    Journal of Electronic Materials, 2014, 43 : 843 - 849
  • [9] Impact of rapid cooling process in ultrahigh-temperature oxidation of 4H-SiC(0001)
    Sometani, Mitsuru
    Nagai, Daisuke
    Katsu, Yoshihito
    Hosoi, Takuji
    Shimura, Takayoshi
    Takei, Manabu
    Yonezawa, Yoshiyuki
    Watanabe, Heiji
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2017, 56 (04)
  • [10] Crystalline Recovery after Activation Annealing of Al Implanted 4H-SiC
    Hattori, R.
    Watanabe, T.
    Mitani, T.
    Sumitani, H.
    Oomori, T.
    SILICON CARBIDE AND RELATED MATERIALS 2007, PTS 1 AND 2, 2009, 600-603 : 585 - +