SURFACE DAMAGE OF SLAG-CEMENT CONCRETE STRUCTURE EXPOSED TO DEICING-FROST CONDITIONS

被引:0
|
作者
Zhang, Yun-Qing [1 ]
Yu, Hong-Fa [1 ]
Wang, Jia-Chun [1 ]
机构
[1] Nanjing Univ Aeronaut & Astronaut, Dept Civil Engn, Nanjing 210016, Peoples R China
关键词
high performance concrete; air-entrained Portland cement concrete; deicing-frost resistance; freezing and thawing cycles; subsurface damaged thickness; REINFORCED-CONCRETE; CORROSION;
D O I
暂无
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The deicing-frost experimentation with test beams made of ordinary Portland cement concrete (OPC), air-entrained Portland cement concrete (APC) and high performance concrete (HPC) subjected to the action of 3.5% (mass fraction) sodium chloride (NaCl) solution was studied by the accelerated freezing method. Adopting to ultrasonic testing method, the surface damaged thickness of concrete structure was detected, and a new evaluation index was put forward, the deicing-frost damaged degree. The results show that the deicing-frost damaged degree of OPC increases sharply and linearly with increase of freeze-thawing cycle. But the addition of air-entrained admixture can efficiently not only decrease deicing-frost damaged degree of the concrete but also enhance its deicing-frost resistance. The deicer-frosting-resistance of air-entrained HPC is prodigiously influenced by the amount of mineral admixtures. Air-entrained HPC with 50%SG (50% of binder mass) has strongest deicing-frost resistance, and its typical characteristic is that the deicing-frost damaged degree decreases and in the later period it increases very slowly. Finally, Minimum cover depth of concrete structure exposed to deicing-frost conditions was discussed, and some regulation required by Code for Design of Highway Reinforced Concrete and Prestressed Concrete Bridge and Culverts (JTG D62-2004) was insecure by considered.
引用
收藏
页码:1100 / 1105
页数:6
相关论文
共 50 条
  • [1] Strength of slag-cement concrete cured in place and in other conditions
    Sanjayan, JG
    Sioulas, B
    ACI MATERIALS JOURNAL, 2000, 97 (05) : 603 - 611
  • [2] The Evaluation of Damage Effects on MgO Added Concrete with Slag Cement Exposed to Calcium Chloride Deicing Salt
    Jang, Jae-Kyeong
    Kim, Hong-Gi
    Kim, Jun-Hyeong
    Ryou, Jae-Suk
    MATERIALS, 2018, 11 (05)
  • [3] Optimizing the use of recycled concrete fines in slag-cement
    Janssen, Donald J.
    Vandenbossche, Julie M.
    Koubaa, Amir
    ZKG INTERNATIONAL, 2007, 60 (04): : 88 - 95
  • [4] Carbonation Curing of Slag-Cement Concrete for Binding CO2 and Improving Performance
    Monkman, Sean
    Shao, Yixin
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2010, 22 (04) : 296 - 304
  • [5] INFLUENCE OF SLAG CEMENT ON THE FROST RESISTANCE OF CONCRETE - A THEORETICAL ANALYSIS.
    Fagerlund, Goran
    CBI Forskning (Cement-och Betonginstitutet), 1980, (01):
  • [6] HARDENED SLAG-CEMENT PASTES OF VARIOUS POROSITIES .3. SURFACE-AREA IN RELATION TO PORE STRUCTURE
    MIKHAIL, RS
    ABOELENEIN, SA
    ABDELKHALIK, M
    JOURNAL OF APPLIED CHEMISTRY AND BIOTECHNOLOGY, 1975, 25 (11): : 849 - 857
  • [7] Behaviour of slag cement concrete under restraint conditions
    Darquennes, Aveline
    Staquet, Stephanie
    Espion, Bernard
    EUROPEAN JOURNAL OF ENVIRONMENTAL AND CIVIL ENGINEERING, 2011, 15 (05) : 787 - 798
  • [8] Scaling resistance of concrete paving block surface exposed to deicing chemicals
    Ghafoori, N
    Mathis, RP
    ACI MATERIALS JOURNAL, 1997, 94 (01) : 32 - 38
  • [9] HYDRAULIC PROPERTIES AND PASTE STRUCTURE OF BASIC OXYGEN FURNACE STEEL SLAG-CEMENT BLENDED MATERIALS
    Du, Jun
    Liu, Jiaxiang
    FRESENIUS ENVIRONMENTAL BULLETIN, 2013, 22 (11A): : 3279 - 3286
  • [10] Study on Preparation and Interfacial Transition Zone Microstructure of Red Mud-Yellow Phosphorus Slag-Cement Concrete
    Su, Zhennan
    Li, Xianhai
    MATERIALS, 2021, 14 (11)