Effect of various phase fractions of bainite, retained austenite, intercritical ferrite and pearlite on the wear behaviour of multiphase steels

被引:13
|
作者
Neetu [1 ]
Sangal, S. [1 ]
Mondal, K. [1 ]
机构
[1] Indian Inst Technol Kanpur, Dept Mat Sci & Engn, Kanpur 208016, Uttar Pradesh, India
关键词
Multiphase steel (MPS); Sliding wear; Abrasion; Optical profilometry; Coefficient of friction (COF); Wear volume loss; WORK-HARDENING BEHAVIOR; NANOSTRUCTURED BAINITE; MECHANICAL-PROPERTIES; ROLLING/SLIDING WEAR; SUPER STRONG; SILICON; MICROSTRUCTURE; RESISTANCE; CORROSION; RAIL;
D O I
10.1016/j.wear.2022.204355
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In this study, the dry sliding wear behaviour of multiphase steels (MPS) was investigated with the help of a pin/ ball-on-disc wear setup. The newly developed high strength and highly ductile MPS specimens consisting of various fractions of bainite, retained austenite, intercritical ferrite and pearlite, were obtained by a combination of continuous cooling for different times (0 s, 10 s, 20 s and 40 s) after austenitization followed by isothermal heat treatment at various temperatures (300 C, 350 C and 400 C) for 10 min from a moderately high C (~0.67 wt%) high Si (~1.71 wt%) steel. The worn-out surfaces and wear debris revealed that the primary material removal mechanism was of abrasive types. Wear scars were seen like a ploughed field-like structure. The depth of wear scars and amount of material collected at the periphery were affected by various phases and their fractions in the MPS specimens. The wear behaviour of the multiphase steels was affected by the distribution of plastic deformation due to continuous sliding of wear ball and application of loads on the surface of MPS specimens which was analysed by hardness variation of the sub-surfaces beneath the wear scars. At a particular austempering temperature, the wear volume loss and specific wear rate of the MPS specimens increased with the increase of continuous cooling time irrespective of the applied wear loads, and it was attributed to the formation of softer intercritical ferrite as well as pearlite formed due to longer continuous cooling. However, the bainitic structure formed by austempering without continuous cooling led to the highest wear resistance irrespective of the isothermal temperatures.
引用
收藏
页数:18
相关论文
共 50 条
  • [1] Effect of various phase fraction of bainite, intercritical ferrite, retained austenite and pearlite on the corrosion behavior of multiphase steels
    Neetu
    Katiyar, Prvan Kumar
    Sangal, S.
    Mondal, K.
    CORROSION SCIENCE, 2021, 178 (178)
  • [2] Super strong and highly ductile low alloy multiphase steels consisting of bainite, ferrite and retained austenite
    Varshney, A.
    Sangal, S.
    Kundu, S.
    Mondal, K.
    MATERIALS & DESIGN, 2016, 95 : 75 - 88
  • [3] Stability of retained austenite under strain conditions on multiphase steels with nanostructured bainite
    Loaiza Uribe, Tania
    Perez Espitia, Paula Andrea
    Serna Giraldo, Claudia Patricia
    Aristizabal Sierra, Ricardo Emilio
    MATERIA-RIO DE JANEIRO, 2018, 23 (02):
  • [4] Comparison of the fatigue performance of ferrite–pearlite and ferrite–bainite dual-phase steels
    Jeong Yeol Park
    Dong Jin Oh
    Myung Hyun Kim
    Journal of Marine Science and Technology, 2021, 26 : 344 - 356
  • [5] Effect of retained austenite on wear resistance of nanostructured dual phase steels
    Hu, F.
    Wu, K. M.
    Hodgson, P. D.
    MATERIALS SCIENCE AND TECHNOLOGY, 2016, 32 (01) : 40 - 48
  • [6] Comparison of the fatigue performance of ferrite-pearlite and ferrite-bainite dual-phase steels
    Park, Jeong Yeol
    Oh, Dong Jin
    Kim, Myung Hyun
    JOURNAL OF MARINE SCIENCE AND TECHNOLOGY, 2021, 26 (02) : 344 - 356
  • [7] Abrasive wear behaviour of ADI material with various retained austenite content
    Balos, S.
    Rajnovic, D.
    Dramicanin, M.
    Labus, D.
    Eric-Cekic, O.
    Grbovic-Novakovic, J.
    Sidjanin, L.
    INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 2016, 29 (04) : 187 - 193
  • [8] Influence of Multiphase High Silicon Steel (Retained Austenite-RA, Ferrite-F, Bainite-B and Pearlite-P) and Carbon Content of RA-Cγ on Rolling/Sliding Wear
    Rajan Kumar
    Ravi Kumar Dwivedi
    Siraj Ahmed
    Silicon, 2021, 13 : 3307 - 3320
  • [9] Influence of Multiphase High Silicon Steel (Retained Austenite-RA, Ferrite-F, Bainite-B and Pearlite-P) and Carbon Content of RA-Cγon Rolling/Sliding Wear
    Kumar, Rajan
    Dwivedi, Ravi Kumar
    Ahmed, Siraj
    SILICON, 2021, 13 (10) : 3307 - 3320
  • [10] Influence of Toughness and Retained Austenite on Wear Behaviour of Carbide-Free Bainite in High Silicon Steel
    Rajan Kumar
    R. K. Dwivedi
    Virendra Pratap Singh
    Basil Kuriachen
    N. Anand Krishnan
    Transactions of the Indian Institute of Metals, 2023, 76 : 2425 - 2434