Influence of neutron irradiation on Al-6061 alloy produced via ultrasonic additive manufacturing

被引:17
|
作者
Gussev, M. N. [1 ]
Sridharan, N. [1 ]
Babu, S. S. [1 ]
Terrani, K. A. [1 ]
机构
[1] Oak Ridge Natl Lab, POB 2008, Oak Ridge, TN 37831 USA
关键词
Ultrasonic additive manufacturing; HFIR; neutron irradiation; tensile tests; DIC; post-weld heat treatment; hot isostatic pressing; MICROSTRUCTURE; CONSOLIDATION; PERFORMANCE; PARAMETERS; INTERFACES; STABILITY; OXIDATION; BEHAVIOR;
D O I
10.1016/j.jnucmat.2021.152939
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Samples of aluminum alloy 6061 produced via ultrasonic additive manufacturing (UAM) were irradiated in the High Flux Isotope Reactor (HFIR) up to 17.3 dpa at similar to 70 degrees C while in contact with water using perforated rabbit capsules. The irradiation campaign included as-received (AR) material, specimens subjected to various post-weld heat treatments (PWHTs, including hot isostatic pressing [HIP]), and reference (wrought) alloy samples. Mechanical tensile tests, accompanied by digital image correlation (DIC) analysis, fractography, and metallography, were performed as a part of the post-irradiation evaluation. The X- and Y-specimens (i.e., oriented in the sonotrode moving and vibration directions, respectively) showed pronounced radiation hardening and ductility decrease. Specific serration flow behavior and propagation of deformation bands were observed under various material conditions up to 3.5 dpa but disappeared at 17.3 dpa. In all cases, the fracture mechanism of X- and Y-specimens was ductile; ductile dimples dominated the fracture surface. Irradiated X- and Y-specimens showed good performance, regardless of material conditions (AR or PWHT). The performance of Z-specimens oriented in the build direction was strongly dependent on the PWHT. The AR and aged specimens showed fracture stress decrease with dose, and they experienced fracture under irradiation after 3.5 dpa; specimen cross section analysis revealed specific interface degradation that was likely related to corrosion. Recrystallization significantly improved in-reactor performance. HIP suppressed interface degradation due to recrystallization and pore removal, which led to good in-reactor performance for Z-specimens. (C) 2021 Elsevier B.V. All rights reserved.
引用
收藏
页数:13
相关论文
共 50 条
  • [1] Rationalization of anisotropic mechanical properties of Al-6061 fabricated using ultrasonic additive manufacturing
    Sridharan, Niyanth
    Gussev, Maxim
    Seibert, Rachel
    Parish, Chad
    Norfolk, Mark
    Terrani, Kurt
    Babu, Sudarsanam Suresh
    ACTA MATERIALIA, 2016, 117 : 228 - 237
  • [2] Evaluation of microstructure stability at the interfaces of Al-6061 welds fabricated using ultrasonic additive manufacturing
    Sridharan, Niyanth
    Gussev, Maxim N.
    Parish, Chad M.
    Isheim, Dieter
    Seidman, David N.
    Terrani, Kurt A.
    Babu, Sudarsanam S.
    MATERIALS CHARACTERIZATION, 2018, 139 : 249 - 258
  • [3] Effect of post weld heat treatment on the 6061 aluminum alloy produced by ultrasonic additive manufacturing
    Gussev, M. N.
    Sridharan, N.
    Norfolk, M.
    Terrani, K. A.
    Babu, S. S.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 684 : 606 - 616
  • [4] Growth of AlN coating on Al-6061 alloy surface
    Soni, Rohan
    Sarin, Vinod K.
    Rao, Pratima
    Srinivasan, Easwar
    Basu, Soumendra N.
    SURFACE & COATINGS TECHNOLOGY, 2024, 476
  • [5] Ultrasonic powder consolidation of metallic glass/Al-6061 composites
    Wang, Jiahao
    Liu, Senji
    Huang, Pengyu
    Liu, Junsheng
    Zhang, Yu
    Liang, Xiong
    Sohrabi, Sajad
    Ma, Jiang
    INTERMETALLICS, 2024, 174
  • [6] Mechanism of weld formation during very-high-power ultrasonic additive manufacturing of Al alloy 6061
    Shimizu, S.
    Fujii, H. T.
    Sato, Y. S.
    Kokawa, H.
    Sriraman, M. R.
    Babu, S. S.
    ACTA MATERIALIA, 2014, 74 : 234 - 243
  • [7] Investigation on Mechanical properties of Al-6061 Alloy based MMC
    Senapati, Ajit Kumar
    Abhishek-Kumar
    Anurag-Kumar
    1ST INTERNATIONAL CONFERENCE ON ADVANCED ENGINEERING FUNCTIONAL MATERIALS (ICAEFM), 2018, 410
  • [8] Influence of gaseous dielectrics on the wettability of Al-6061 alloy using dry μ-electrical discharge milling
    Kumar, Harish
    Roy, Tribeni
    Jha, Sunil
    APPLIED SURFACE SCIENCE, 2025, 685
  • [9] Sintering behaviour of Al-6061 powder produced by rapid solidification process
    Arockiasamy, A.
    German, Randall M.
    Wang, P. T.
    Horstemeyer, M. F.
    Morgan, W.
    Park, S. J.
    Otsuka, Isamu
    POWDER METALLURGY, 2011, 54 (03) : 354 - 359
  • [10] Effects of Process Parameters on Cold Spray Deposition of Al-6061 Alloy
    Ahmad Nourian
    Tricia Schwartz
    Samuel Boese
    Sinan Müftü
    Journal of Thermal Spray Technology, 2022, 31 : 2517 - 2536