Micromechanical modeling of hardening mechanisms in commercially pure α-titanium in tensile condition

被引:83
|
作者
Amouzou, K. E. K. [1 ]
Richeton, T. [1 ]
Roth, A. [2 ]
Lebyodkin, M. A. [1 ]
Lebedkina, T. A. [1 ]
机构
[1] Univ Lorraine, CNRS, UMR 7239, LEM3, F-57045 Metz, France
[2] Asco Ind CREAS, Ave France, F-57300 Hagondange, France
关键词
Microstructures; Anisotropic material; Crystal plasticity; Polycrystalline material; Mechanical testing; SLIP SYSTEMS INTERACTIONS; DEFORMATION MECHANISMS; GRAIN-SIZE; CRYSTAL-PLASTICITY; TEXTURE EVOLUTION; BEHAVIOR; STRESS; DISLOCATIONS; ALLOYS; DISTRIBUTIONS;
D O I
10.1016/j.ijplas.2015.09.008
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Tensile tests on commercially pure alpha-titanium show a three-stage behavior giving rise to a well on the strain dependence of the work hardening. An opposite strain rate effect on the well depth is found whether specimens are elongated along the rolling or the transverse direction. Slip lines analysis reveals an initial predominance of prismatic slip, particularly pronounced in specimens strained along the rolling direction. The relative activity of prismatic slip is then observed to decrease with the samples deformation. These results provide grounds for elaboration of an elasto-viscoplastic self-consistent model based on the translated field method and an affine linearization of the viscoplastic flow rule, and capable of explaining such peculiar work hardening behavior. The model considers crystal plasticity and deals separately with mobile dislocation density and dislocation velocity. It assumes lower strain rate sensitivity as well as higher dislocation multiplication rate for prismatic systems. Based on these assumptions, the model reproduces correctly the stress strain curves and gives sound estimates of Lankford coefficients, prismatic slip activity and textures evolution. Most importantly, the opposite effect of strain rate on the well depth with regard to the orientation of the tensile axis is qualitatively retrieved, which allows putting forward an explanation of the observed phenomena. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:222 / 240
页数:19
相关论文
共 50 条
  • [1] Work-hardening stages and deformation mechanism maps during tensile deformation of commercially pure titanium
    Becker, Hanka
    Pantleon, Wolfgang
    COMPUTATIONAL MATERIALS SCIENCE, 2013, 76 : 52 - 59
  • [2] Effect of twinning deformation on work hardening in commercially pure titanium
    Tsukamoto, Genki
    Kunieda, Tomonori
    Mitsuhara, Masatoshi
    Nakashima, Hideharu
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 840
  • [3] Tensile strain-hardening behavior and related deformation mechanisms of pure titanium at cryogenic temperature
    Won, Jong Woo
    Suh, Byeong-Chan
    Jeong, Jae Suk
    Hyun, Yong-Taek
    Lee, Min -Su
    Jun, Tea-Sung
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 26 : 1669 - 1676
  • [4] Effect of initial orientation on the tensile properties of commercially pure titanium
    Sinha, Subhasis
    Ghosh, Atasi
    Gurao, N. P.
    PHILOSOPHICAL MAGAZINE, 2016, 96 (15) : 1485 - 1508
  • [5] Mechanical properties and deformation mechanisms of a commercially pure titanium
    Nemat-Nasser, S
    Guo, WG
    Cheng, JY
    ACTA MATERIALIA, 1999, 47 (13) : 3705 - 3720
  • [6] Modeling the ductile damage process in commercially pure titanium
    Zhai, Jinyuan
    Luo, Tuo
    Gao, Xiaosheng
    Graham, Stephen M.
    Baral, Madhav
    Korkolis, Yannis P.
    Knudsen, Erik
    INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 2016, 91 : 26 - 45
  • [7] Enhanced tensile strength and high ductility in cryomilled commercially pure titanium
    Ertorer, Osman
    Topping, Troy
    Li, Ying
    Moss, Wes
    Lavernia, Enrique J.
    SCRIPTA MATERIALIA, 2009, 60 (07) : 586 - 589
  • [8] SURFACE HARDENING OF BN COATED COMMERCIALLY PURE TITANIUM DUE TO LASER IRRADIATION
    YANO, T
    YONEDA, M
    UTSUMI, A
    MATSUDA, J
    KATSUMURA, M
    SATOU, M
    NISHIDA, N
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1991, 55 (08) : 881 - 886
  • [9] Surface hardening of commercially pure titanium by laser nitriding: Response surface analysis
    Hamad, A. R.
    Abboud, J. H.
    Shuaeib, F. M.
    Benyounis, K. Y.
    ADVANCES IN ENGINEERING SOFTWARE, 2010, 41 (04) : 674 - 679
  • [10] Plastic deformation of commercially-pure titanium: experiments and modeling
    Baral, Madhav
    Hama, Takayuki
    Knudsen, Erik
    Korkolis, Yannis P.
    INTERNATIONAL JOURNAL OF PLASTICITY, 2018, 105 : 164 - 194