AGING EFFECTS OF TRITIUM ON Pd POWDERS AND Pd91.31Y8.50Ru0.19 ALLOY FILM

被引:0
|
作者
Chen Miao [1 ]
Lu Guangda [2 ]
Zhang Guikai [1 ]
Zhang Yanzhi [1 ]
Wang Xiaoying [1 ]
Ren Dapeng [2 ]
机构
[1] Natl Key Lab Surface Phys & Chem, Mianyang 621907, Peoples R China
[2] China Acad Engn Phys, Mianyang 621900, Peoples R China
关键词
Pd; Pd91.31Y8.50Ru0.19; tritium aging; He-3; He bubble; PALLADIUM TRITIDE; SEPARATION; MEMBRANES; STORAGE; TEM;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
During tritium (T) treatment, Pd and its alloys will be aged due to solution of He-3, a product of T decay, in lattices, which changes the microstructure and properties of the materials. The existing and distributing states of He-3 in Pd and Pd91.31Y8.50Ru0.19 alloy during T aging were studied by XRD and TEM. XRD results for Pd powders aged up to 1.6 and 3.5 a show that the peaks widen, intensities of peaks reduce and lattice constants increase by 0.095% and 0.11%, respectively. TEM. observations show that, about 1 nm sized He bubbles appear in Pd91.31Y8.50Ru0.19 alloy aged for 41 d, and more dislocations and dislocation loops are observed; after 295 d aging, the He bubbles grow slightly and reach 1.2-1.4 nm in diameter, but the amounts of dislocations and dislocation loops decrease.
引用
收藏
页码:1277 / 1280
页数:4
相关论文
共 15 条
  • [1] HELIUM RELEASE FROM AGED PALLADIUM TRITIDE
    ABELL, GC
    MATSON, LK
    STEINMEYER, RH
    BOWMAN, RC
    OLIVER, BM
    [J]. PHYSICAL REVIEW B, 1990, 41 (02): : 1220 - 1223
  • [2] A PROPOSED METHOD OF HYDROGEN ISOTOPE-SEPARATION USING PALLADIUM ALLOY MEMBRANES
    EVANS, J
    HARRIS, IR
    ROSS, DK
    [J]. JOURNAL OF THE LESS-COMMON METALS, 1983, 89 (02): : 407 - 414
  • [3] On the correlation between mechanical and TEM studies of the aging of palladium during tritium storage
    Fabre, A
    Decamps, B
    Finot, E
    Penisson, JM
    Demoment, J
    Thiebaut, S
    Contreras, S
    Percheron-Guegan, A
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2005, 342 (1-3) : 101 - 107
  • [4] HU ZL, 2002, HYDROGEN STORAGE MAT, P32
  • [5] The impact of tritium on the structure and properties of Pd-membranes
    Klevtsov, VG
    Boitsov, IE
    Vedeneev, AI
    Glagolev, MV
    Lobanov, VN
    Malkov, IL
    Pimanikhin, SA
    Stengach, AV
    [J]. FUSION ENGINEERING AND DESIGN, 2000, 49-50 : 873 - 877
  • [6] LASSER R, 1989, TRITIUM HELIUM 3 MET, P34
  • [7] Hydrogen isotope separation factors on palladium alloy membranes
    Luo, DL
    Shen, CS
    Meng, DQ
    [J]. FUSION SCIENCE AND TECHNOLOGY, 2002, 41 (03) : 1142 - 1145
  • [8] SEPARATION AND CONCENTRATION OF HYDROGEN ISOTOPES BY A PALLADIUM ALLOY MEMBRANE
    SUZUKI, Y
    KIMURA, S
    [J]. NUCLEAR TECHNOLOGY, 1993, 103 (01) : 93 - 100
  • [9] Evolution of a defect structure of Pd-Ag alloys during tritium exposure
    Tebus, V
    Rivkis, L
    Dmitrievskaia, E
    Arutunova, G
    Golikov, I
    Ryazantseva, N
    Filin, V
    Kapychev, V
    Bulkin, V
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2002, 307 (2 SUPPL.) : 966 - 970
  • [10] Structural changes in Pd (Rh, Pt) solid solutions due to 3He formation during tritium storage
    Thiebaut, S
    Paul-Boncour, V
    Percheron-Guegan, A
    Limacher, B
    Blaschko, O
    Maier, C
    Tailland, C
    Leroy, D
    [J]. PHYSICAL REVIEW B, 1998, 57 (17): : 10379 - 10387