Process characteristics and film properties upon growth of TiOx films by high power pulsed magnetron sputtering

被引:120
|
作者
Sarakinos, K. [1 ]
Alami, J. [1 ]
Wuttig, M. [1 ]
机构
[1] RWTH Aachen Univ Technol, Inst Phys IA, D-52056 Aachen, Germany
关键词
D O I
10.1088/0022-3727/40/7/037
中图分类号
O59 [应用物理学];
学科分类号
摘要
In this work TiOx (x > 1.8) films are grown reactively from a ceramic TiO1.8 target employing high power pulsed magnetron sputtering (HPPMS) at a constant average target current. The effect of the pulse on/off time configuration on the target and the discharge characteristics as well as on the film properties is investigated. The target voltage (V-T) increases from 480 to 650V and the peak target current (I-Tp) increases from 2 to 40A when the pulse off-time is increased from 200 to 2450 mu s, while the on-time is kept constant at 50 mu s. This is accompanied by an increase in the number of Ti atoms sputtered from the target, as manifested by time-resolved optical emission spectroscopy (OES) measurements. OES also manifests an increase in the ionization of the sputtered Ti atoms with increasing I-Tp. The above changes in the target and discharge characteristics affect the deposition rate so that the latter increases with increasing I-Tp up to a value of 14 A, above which the deposition rate drops. In all the cases the deposition rates are up to similar to 40% higher compared to the rates achieved for films grown by dc magnetron sputtering (dcMS) which are also studied for reference. The increase in I-Tp from 2 to 40A also affects the films' properties. It is shown that a drop in the surface roughness from 1.1 to 0.5 nm takes place. These values are lower than the surface roughness of films grown by dcMS (1.35 nm). Moreover, films grown by HPPMS are found to have higher densities (up to 3.83 g cm(-3)) and higher refractive indices (up to 2.48) in comparison to the films grown by dcMS (3.71 g cm(-3) and 2.38, respectively).
引用
收藏
页码:2108 / 2114
页数:7
相关论文
共 50 条
  • [1] Formation of TiOx films produced by high-power pulsed magnetron sputtering
    Stranak, Vitezslav
    Quaas, Marion
    Wulff, Harm
    Hubicka, Zdenek
    Wrehde, Stefan
    Tichy, Milan
    Hippler, Rainer
    JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2008, 41 (05)
  • [2] Growth of tiox films magnetron sputtering by high power pulsed from a compound tio1.8 target
    Sarakinos, K.
    Alami, J.
    Klever, C.
    Wuttig, M.
    REVIEWS ON ADVANCED MATERIALS SCIENCE, 2007, 15 (01) : 44 - 48
  • [3] Plasma characteristics and properties of Cu films prepared by high power pulsed magnetron sputtering
    Wu, B. H.
    Wu, J.
    Jiang, F.
    Ma, D. L.
    Chen, C. Z.
    Sun, H.
    Leng, Y. X.
    Huang, N.
    VACUUM, 2017, 135 : 93 - 100
  • [4] Tailoring of titanium thin film properties in high power pulsed magnetron sputtering
    Wu, Baohua
    Yu, Yan
    Wu, Jian
    Shchelkanov, Ivan
    Ruzic, David N.
    Huang, Nan
    Leng, Y. X.
    VACUUM, 2018, 150 : 144 - 154
  • [5] Fabrication and surface properties of ZrN films by high power pulsed magnetron sputtering
    Wu, Zhongzhen
    Tian, Xiubo
    Duan, Weizan
    Gong, Chunzhi
    Yang, Shiqin
    Cailiao Yanjiu Xuebao/Chinese Journal of Materials Research, 2010, 24 (06): : 561 - 566
  • [7] Deposition and Properties of CrNx films by High Power Pulsed Unbalanced Magnetron Sputtering
    Mu Xiaodong
    Mu Zongxin
    Wang Chun
    Jia Li
    Zang Hirong
    Liu Bingbing
    Dong Chuang
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 : 160 - 163
  • [9] The Deposition and Properties of Titanium Films Prepared by High Power Pulsed Magnetron Sputtering
    Jiang, Quanxin
    Ma, Donglin
    Li, Yantao
    Chen, Changzi
    MATERIALS, 2023, 16 (23)
  • [10] Chromium films deposition by hot target high power pulsed magnetron sputtering: Deposition conditions and film properties
    Grudinin, Vladislav A.
    Bleykher, Galina A.
    Sidelev, Dmitrii, V
    Krivobokov, Valery P.
    Bestetti, Massimiliano
    Vicenzo, Antonello
    Franz, Silvia
    SURFACE & COATINGS TECHNOLOGY, 2019, 375 : 352 - 362