Corrosion studies in Pb-Bi liquid alloy

被引:0
|
作者
Deloffre, P [1 ]
Barbier, F [1 ]
机构
[1] CEA Saclay, CEREM, SCECF, F-91191 Gif Sur Yvette, France
来源
CORROSION AND OXYGEN CONTROL: MINUTES OF THE WORKSHOP ON HEAVY LIQUID METAL TECHNOLOGY | 1999年 / 6389卷
关键词
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Corrosion studies in Pb-Bi liquid alloy are necessary for materials selection. At first, we present the R&D programme which has been proposed. The aims of this programme are : 1) basic corrosion studies in static Pb-Bi, 2) corrosion studies in dynamic Pb-Bi, 3) compatibility studies in Pb-Bi containing additional impurities (spallation products), 4) structure protection studies. To carry out the corrosion studies in static Pb-Bi liquid alloy, three experimental devices have been developed. They are : 1) COLIMET (COrrosion LIquid MEtal), to perform experiments with small quantities of eutectic Pb-Bi alloy in reductive atmosphere Ar + H-2, 2) COLIMESTA (COrrosion LIquid MEtal STAtic), for experiments with larger quantities of static eutectic Pb-Bi and in a wide range of oxygen contents measured by oxygen sensor, 3) DECO (DEposition and COrrosion), for experiments in a sealed container with a thermal. gradient under inert atmosphere Ar. The various devices and the experiments planned to be performed are described.
引用
收藏
页码:197 / +
页数:4
相关论文
共 50 条
  • [1] Corrosion studies of steels in the presence of flowing liquid Pb-Bi
    Balbaud, F
    Barbier, F
    CORROSION AND OXYGEN CONTROL: MINUTES OF THE WORKSHOP ON HEAVY LIQUID METAL TECHNOLOGY, 1999, 6389 : 209 - +
  • [2] High-temperature corrosion of steels in liquid Pb-Bi alloy
    Balbaud-Célérier, F
    Martinelli, L
    Terlain, A
    Ngomsik, A
    Sanchez, S
    Picard, G
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS, 2004, 461-464 : 1091 - 1098
  • [3] The electrical resistivity of liquid Pb-Bi alloy
    Li, Q
    Zu, FQ
    Li, XF
    Xi, YU
    MODERN PHYSICS LETTERS B, 2006, 20 (04): : 151 - 158
  • [4] Corrosion studies in liquid Pb-Bi alloy at JAERI: R&D program and first experimental results
    Kurata, Y
    Futakawa, A
    Kikuchi, K
    Saito, S
    Osugi, T
    JOURNAL OF NUCLEAR MATERIALS, 2002, 301 (01) : 28 - 34
  • [5] Structural changes of liquid Pb-Bi eutectic alloy
    Deodati, Paolo
    Gauzzi, Franco
    Montanari, Roberto
    Varone, Alessandra
    THERMEC 2011, PTS 1-4, 2012, 706-709 : 878 - 883
  • [6] Behaviour of different steels in liquid Pb and Pb-Bi eutectic alloy
    Benamati, G
    Buttol, P
    Fazio, C
    Imbeni, V
    Martini, C
    Palombarini, G
    Rusanov, A
    CORROSION AND OXYGEN CONTROL: MINUTES OF THE WORKSHOP ON HEAVY LIQUID METAL TECHNOLOGY, 1999, 6389 : 91 - +
  • [7] Corrosion of CrN-coated steels in liquid Pb-Bi
    Kurata, Yuji
    Futakawa, Masatoshi
    MATERIALS TRANSACTIONS, 2007, 48 (03) : 519 - 525
  • [8] Experimental studies on steel corrosion in Pb-Bi with steam injection
    Hata, K
    Hara, K
    Takahashi, M
    PROGRESS IN NUCLEAR ENERGY, 2005, 47 (1-4) : 596 - 603
  • [9] Corrosion behaviour of aluminized martensitic and austenitic steels in liquid Pb-Bi
    Deloffre, P
    Balbaud-Célérier, F
    Terlain, A
    JOURNAL OF NUCLEAR MATERIALS, 2004, 335 (02) : 180 - 184
  • [10] Flowing Liquid Metal Corrosion of Structural Steels in the Pb-Bi Eutectic
    Wang, Z. H.
    Chen, H.
    FRONTIERS OF MATERIALS, CHEMICAL AND METALLURGICAL TECHNOLOGIES, PTS 1 AND 2, 2012, 581-582 : 1040 - 1043