Influence of zincate treatment on adhesion strength of electroless nickel-phosphorus plated film for commercial pure aluminum

被引:2
|
作者
Murakami, Koji [1 ]
Hino, Makoto
Hiramatsu, Minoru
Osamura, Kozo
Kanadani, Teruto
机构
[1] Ind Technol Res Inst, Okayama 7011296, Japan
[2] Kyoto Univ, Dept Mat Sci & Engn, Sakyo Ku, Kyoto 6068501, Japan
[3] Okayama Univ Sci, Fac Engn, Okayama 7000005, Japan
关键词
commercial pure aluminum; zincate; electroless plating; nickel; phosphorus; adhesion;
D O I
10.4028/www.scientific.net/MSF.519-521.759
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Characterizations of zincate films were conducted formed as a pretreatment for electroless nickel-phosphorus platings on commercial pure aluminum substrate (JIS A1050P-H24, 99.5 mass%Al). By using a basic solution which consists of sodium hydroxide and zinc oxide, a zincate film formed by the single zincate treatment showed coarse zinc grains of 1-2 mu m in size. The double zincate treatment by using the basic solution reduced coarse zinc grains, and the thickness of the uniform zincate film was 20-30 nm. Iron-added zincate solutions decreased the number and the size of coarse grains in the single zincate treatments compared with the case of the basic zincate solution, and the double zincate treatments brought about further thin zincate films of similar to 10 nm in thickness. The single zincate treatment by using the basic zincate solution resulted in poor adhesion strength of the electroless nickel-phosphorus plated film which peeled spontaneously off the substrate due to its residual stress. Quantification of adhesion strength by 90 degrees peeling test showed the double zincate treatment by the basic solution increased the adhesion strength of the plated film up to 30 N/m. In the cases of the double zincate treatments by the iron-added zincate solutions, the adhesion strengths of the plated nickel-phosphorus films showed such remarkable increase that those could not be quantified by the peeling test due to the rupture of the plated nickel-phosphorus films. From the observation by transmission electron microscopy of the interfaces between the nickel-phosphorus plated films and the substrates, thickness of a zincate film ought to be similar to 10 nm for eliminating gaps between the plated film and the substrate.
引用
收藏
页码:759 / 764
页数:6
相关论文
共 49 条
  • [1] Effect of zincate treatment on adhesion of electroless nickel-phosphorus coating for commercial pure aluminum
    Murakami, Koji
    Hino, Makoto
    Hiramatsu, Minoru
    Osamura, Kozo
    Kanadani, Teruto
    MATERIALS TRANSACTIONS, 2006, 47 (10) : 2518 - 2523
  • [2] Effect of zincate treatment on adhesion of electroless nickel-phosphorus coating for commercial pure aluminum
    Industrial Technology Research Institute of Okayama Prefectural Government, 5301, Haga, Okayama-shi, Okayama 701-1296
    不详
    不详
    不详
    Keikinzoku J Jpn Inst Light Met, 2007, 3 (125-130):
  • [3] Formation of Zincate Films on Binary Aluminum Alloys and Adhesion of Electroless Nickel-Phosphorus Plated Films
    Murakami, Koji
    Hino, Makoto
    Ushio, Masashi
    Yokomizo, Daichi
    Kanadani, Teruto
    MATERIALS TRANSACTIONS, 2013, 54 (02) : 199 - 206
  • [4] Effect of zincate immersion pretreatment on corrosion resistance of electroless plated nickel-phosphorus film for advanced packaging
    Gan, Weixing
    Li, Ming
    Hang, Tao
    2018 19TH INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY (ICEPT), 2018, : 804 - 807
  • [5] Effects of Alloying Elements in Aluminum Alloys and Activations on Zincate Treatment and Electroless Nickel-Phosphorus Plating
    Murakami, Koji
    Hino, Makoto
    Furukawa, Ryosuke
    Kanadani, Teruto
    MATERIALS TRANSACTIONS, 2010, 51 (01) : 78 - 84
  • [6] FATIGUE-STRENGTH OF ELECTROLESS NICKEL-PHOSPHORUS PLATED STEEL AND MICROSTRUCTURE OF PLATED LAYER
    IZUMI, H
    SUNADA, H
    KONDO, Y
    YAMASAKI, T
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1980, 44 (07) : 829 - 835
  • [7] Effect of zincate treatment on adhesion of electroless Ni-P plated film for 2017 aluminum alloy
    Hino, M
    Murakami, K
    Hiramatsu, M
    Chen, KK
    Saijo, A
    Kanadani, T
    MATERIALS TRANSACTIONS, 2005, 46 (10) : 2169 - 2175
  • [8] Effect of Alloying Elements and Generation of Hydrogen Gas on Zincate Treatment and Electroless Nickel-Phosphorus Plating of Aluminum Alloys
    Murakami, Koji
    Hino, Makoto
    Nagata, Norihito
    Kanadani, Teruto
    MATERIALS TRANSACTIONS, 2015, 56 (05) : 691 - 695
  • [9] Effect of Alloying Elements and Generation of Hydrogen Gas on Zincate Treatment and Electroless Nickel-Phosphorus Plating for Aluminum Alloys
    Murakami, Koji
    Hino, Makoto
    Nagata, Norihito
    Kanadani, Teruto
    JOURNAL OF THE JAPAN INSTITUTE OF METALS AND MATERIALS, 2013, 77 (12) : 599 - 603
  • [10] THE RELATIONSHIP BETWEEN STRESS AND ADHESION OF ELECTROLESS NICKEL-PHOSPHORUS DEPOSITS ON ZINCATED ALUMINUM
    MALLORY, GO
    PLATING AND SURFACE FINISHING, 1985, 72 (06): : 86 - 95