Intermetallic growth study at Sn-3.0Ag-0.5Cu/Cu solder joint interface during different thermal conditions

被引:19
|
作者
Li, Shuai [1 ]
Yan, Yan-fu [2 ]
机构
[1] Dalian Univ Technol, Sch Mat Sci & Engn, Dalian 116024, Peoples R China
[2] Henan Univ Sci & Technol, Sch Mat Sci & Engn, Luoyang 471003, Peoples R China
基金
中国国家自然科学基金;
关键词
LEAD-FREE; IMC GROWTH; ORIENTATION;
D O I
10.1007/s10854-015-3406-4
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
The morphology and growth behaviors of intermetallic compounds (IMCs) of Sn-3.0Ag-0.5Cu/Cu solder joints were investigated during isothermal aging, thermal cycling and thermal shock. The Sn-3.0Ag-0.5Cu/Cu solder joints were isothermal aged at 150 A degrees C, while the non-isothermal aging was performed within the temperature range from -40 to +150 A degrees C. It was observed that the Cu6Sn5 layer initially formed between the copper substrate and solder, followed by the creation of a Cu3Sn layer for aging times greater than 200 h or 200 thermal cycles. However, the Cu3Sn could not be found in solder joints until thermal shock 800 cycles. The results showed that the initial scallop-like IMCs layer changed into a level duplex structure with the aging time (cycling numbers) increasing. The growth rate of Cu6Sn5 was lower than that of Cu3Sn during isothermal aging. While for thermal cycling, it was Cu6Sn5 contributed more to the growth of IMCs than the Cu3Sn. The value of the time exponent n under isothermal aging, thermal cycling and thermal shock were about 0.58, 0.64, 0.66 respectively.
引用
收藏
页码:9470 / 9477
页数:8
相关论文
共 50 条
  • [1] Intermetallic growth study at Sn–3.0Ag–0.5Cu/Cu solder joint interface during different thermal conditions
    Shuai Li
    Yan-fu Yan
    Journal of Materials Science: Materials in Electronics, 2015, 26 : 9470 - 9477
  • [2] Growth behavior of intermetallic compounds on Sn-3.0Ag-0.5Cu/Cu interface
    Li, Shuai
    Yan, Yan-Fu
    Zhao, Yong-Meng
    Xu, Yuan-Yuan
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2014, 35 (05): : 24 - 28
  • [3] Effect of Coloured Pigment on Intermetallic Compound Growth of Sn-3.0Ag-0.5Cu Solder Joint
    Jalar, Azman
    Abu Bakar, Maria
    Ismail, Roslina
    Ibrahim, Najib Saedi
    Ambak, Mohd Ariffin
    SAINS MALAYSIANA, 2018, 47 (05): : 1005 - 1010
  • [4] Undercooling Behavior and Intermetallic Compound Coalescence in Microscale Sn-3.0Ag-0.5Cu Solder Balls and Sn-3.0Ag-0.5Cu/Cu Joints
    M. B. Zhou
    X. Ma
    X. P. Zhang
    Journal of Electronic Materials, 2012, 41 : 3169 - 3178
  • [5] Undercooling Behavior and Intermetallic Compound Coalescence in Microscale Sn-3.0Ag-0.5Cu Solder Balls and Sn-3.0Ag-0.5Cu/Cu Joints
    Zhou, M. B.
    Ma, X.
    Zhang, X. P.
    JOURNAL OF ELECTRONIC MATERIALS, 2012, 41 (11) : 3169 - 3178
  • [6] Effect of current on the growth of intermetallic compounds in Sn-3.0Ag-0.5Cu solder joints
    Li, Bofeng
    Wang, Jundong
    Yao, Yao
    2023 24TH INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY, ICEPT, 2023,
  • [7] Mechanical properties of intermetallic compounds at the Sn-3.0Ag-0.5Cu/Cu joint interface using nanoindentation
    Xiao, Gesheng
    Yang, Xuexia
    Yuan, Guozheng
    Li, Zhigang
    Shu, Xuefeng
    MATERIALS & DESIGN, 2015, 88 : 520 - 527
  • [8] The effects of laser reflow conditions on the formation of intermetallic compounds at Sn3.0Ag0.5Cu solder/Cu joint interface
    Liu, W
    Wang, CQ
    Li, MY
    Tian, YH
    Guan, JW
    PROCEEDINGS OF THE SIXTH IEEE CPMT CONFERENCE ON HIGH DENSITY MICROSYSTEM DESIGN AND PACKAGING AND COMPONENT FAILURE ANALYSIS (HDP'04), 2004, : 70 - 73
  • [9] Microstructural evolutions of Sn-3.0Ag-0.5Cu solder joints during thermal cycling
    Libot, J. B.
    Alexis, J.
    Dalverny, O.
    Arnaud, L.
    Milesi, P.
    Dulondel, F.
    MICROELECTRONICS RELIABILITY, 2018, 83 : 64 - 76
  • [10] Kinetics of Intermetallic Compound Formation at the Interface Between Sn-3.0Ag-0.5Cu Solder and Cu-Zn Alloy Substrates
    Young Min Kim
    Hee-Ra Roh
    Sungtae Kim
    Young-Ho Kim
    Journal of Electronic Materials, 2010, 39 : 2504 - 2512