Modification of isotropic coal-tar pitch by acid treatments for carbon fiber melt-spinning

被引:19
|
作者
Yoo, Mi Jung [1 ]
Ko, Hyo Jun [2 ]
Lim, Yun-Soo [2 ]
Kim, Myung-Soo [1 ]
机构
[1] Myongji Univ, Dept Chem Engn, Yongin 449728, South Korea
[2] Myongji Univ, Dept Mat Sci & Engn, Yongin 449728, South Korea
关键词
coal tar pitch; acid treatment; carbon fiber; melt-spinning; QUINOLINE-INSOLUBLES; CARBONIZATION; BEHAVIOR; QI;
D O I
10.5714/CL.2014.15.4.247
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
In this work, thermal treatment accompanied with different acid treatments was applied to a commercial coal tar pitch (CTP) to obtain a spinnable precursor pitch for carbon fiber. In the case of thermal treatment only, a relatively high reaction temperature of between 380 degrees C and 400 degrees C was required to obtain a softening point (SP) range of 220 degrees C-260 degrees C and many meso-phase particles were created during the application of high reaction temperature. When nitric acid or sulfuric acid treatment was conducted before the thermal treatment, the precursor pitch with a proper SP range could be obtained at reaction temperatures of 280 degrees C-300 degrees C, which were about 100 degrees C lower than those for the case of thermal treatment only. With the acid treatments, the yield and SP of the precursor pitch increased dramatically and the formation of meso-phase was suppressed due to the lower reaction temperatures. Since the precursor pitches with acid and thermal treatment were not spinnable due to the inhomogeneity of properties such as molecular weight distribution and viscosity, the CTP was mixed with ethanol before the consecutive nitric acid and thermal treatments. The precursor pitches with ethanol, nitric acid, and thermal treatments were easily spinnable, and their spinning and carbon fiber properties were compared to those of air blowing and thermal treated CTP.
引用
收藏
页码:247 / 254
页数:8
相关论文
共 50 条
  • [1] Modification of coal-tar pitch with polyamide waste
    Makomaski, Grzegorz
    PRZEMYSL CHEMICZNY, 2019, 98 (04): : 591 - 593
  • [2] Comparative studies of the modification of coal-tar pitch
    Oh, SM
    Park, YD
    FUEL, 1999, 78 (15) : 1859 - 1865
  • [3] Isotropic carbon and graphite fibers from chemically modified coal-tar pitch
    Kap Seung Yang
    Dong Joon Lee
    Seung Kon Ryu
    Yozo Korai
    Yong Joong Kim
    Isao Mochida
    Korean Journal of Chemical Engineering, 1999, 16 : 518 - 524
  • [4] Isotropic carbon and graphite fibers from chemically modified coal-tar pitch
    Yang, KS
    Lee, DJ
    Ryu, SK
    Korai, Y
    Kim, YJ
    Mochida, I
    KOREAN JOURNAL OF CHEMICAL ENGINEERING, 1999, 16 (04) : 518 - 524
  • [5] MODIFICATION OF PRECURSOR COAL-TAR PITCH WITH ALCOHOLS FOR MESOPHASE PITCH
    MATSUMOTO, M
    HIGUCHI, M
    TOMIOKA, T
    SUNAGO, H
    FUEL, 1994, 73 (02) : 237 - 242
  • [6] CARBON FROM PURIFIED COAL-TAR PITCH
    ROMEY, I
    CARBON, 1975, 13 (06) : 556 - 556
  • [7] USE OF COAL-TAR PITCH IN CARBON CARBON COMPOSITES
    MARKOVIC, V
    FUEL, 1987, 66 (11) : 1512 - 1515
  • [8] Properties of Coal-Tar Pitch Based Carbon Fiber with Different Stabilization Conditions
    Kim, Jung-dam
    Kim, Myung-Soo
    POLYMER-KOREA, 2018, 42 (01) : 59 - 66
  • [9] Optimisation of the melt-spinning of anthracene oil-based pitch for isotropic carbon fibre preparation
    Diez, Noel
    Alvarez, Patricia
    Santamaria, Ricardo
    Blanco, Clara
    Menendez, Rosa
    Granda, Marcos
    FUEL PROCESSING TECHNOLOGY, 2012, 93 (01) : 99 - 104
  • [10] TRANSVERSE STRUCTURE OF PITCH FIBER FROM COAL-TAR MESOPHASE PITCH
    HAMADA, T
    NISHIDA, T
    FURUYAMA, M
    TOMIOKA, T
    CARBON, 1988, 26 (06) : 837 - 841